탄화공정이도입된활성탄소섬유의제조방법
    1.
    发明公开
    탄화공정이도입된활성탄소섬유의제조방법 失效
    生产活性碳纤维的方法,介绍碳化工艺

    公开(公告)号:KR1020000028505A

    公开(公告)日:2000-05-25

    申请号:KR1019980046740

    申请日:1998-10-29

    Abstract: PURPOSE: A method for producing an activated carbon fiber is provided to improve the absorbing property for various absorbing materials, and to continuously show the absorbing characteristic by a surface functional group formed on the surface of the activated carbon fiber. CONSTITUTION: An activated carbon fiber is produced by carbonizing under a nitrogen atmosphere at 900, 1000, 1100, 1200, and 1300°C for 30-150minutes used to a general production of carbon fiber. The content of carbon is increased by removing non-carbon components, and the spot-like pored structure on the surface of the carbon fiber is developed with the discharge of non-carbon components by introducing the carbonizing process before an oxy PAN (Poly Acrylo Nitrile) fiber and/of its carbon fiber of high intensity are activated. And the absorbing property is improved by showing the uniform structure and the distribution of pore formed micro pores under 20Angstroms.

    Abstract translation: 目的:提供活性碳纤维的制造方法,以提高各种吸收材料的吸收性,并且通过在活性炭纤维的表面上形成的表面官能团来连续显示吸收特性。 构成:活性碳纤维通过在900,1000,1100,1200和1300℃的氮气氛下碳化用于一般生产碳纤维的30-150分钟来生产。 通过除去非碳成分来增加碳含量,通过在碳PAN(聚丙烯腈(Poly Acrylo Nitrile))之前引入碳化工艺,在碳纤维的表面上形成点状的孔结构, )纤维和/或其高强度碳纤维被激活。 通过显示均匀的结构和形成微孔的分布在20Ang以下,吸收性能得到改善。

    탄화공정이도입된활성탄소섬유의제조방법
    2.
    发明授权
    탄화공정이도입된활성탄소섬유의제조방법 失效
    用消泡法生产活性碳纤维的方法

    公开(公告)号:KR100291886B1

    公开(公告)日:2001-11-14

    申请号:KR1019980046740

    申请日:1998-10-29

    Abstract: 본 발명은 고분자 복합재료의 강화재료로 주로 사용되는 탄소섬유를 고온에서의 탄화 공정을 거친 후 활성화 기체를 유입시키면서 다양한 온도와 시간으로 활성화시켜 기상 및 액상 오염원에 대해 향상된 흡착 성능을 갖는 활성 탄소섬유를 제조하는 방법과 그에 의해 제조된 활성 탄소섬유에 관한 것이다.