토양 및 지하수 복원을 위한 친환경 Р―nZVI 및 그 제조방법
    1.
    发明授权
    토양 및 지하수 복원을 위한 친환경 Р―nZVI 및 그 제조방법 有权
    用于复原土壤和地下水的聚苯酚涂层的纳米级零价铁及其制备方法

    公开(公告)号:KR101027139B1

    公开(公告)日:2011-04-05

    申请号:KR1020090103591

    申请日:2009-10-29

    Abstract: PURPOSE: A polyphenol-coated nano-scale zero valent iron(P-nZVI) for restoring soil and underground water and a method for preparing the same are provided to expand the effective radius of the P-nZVI by including the superior dispersibility and the mobility. CONSTITUTION: A method for preparing P-nZVI includes the following: polyphenol is added to an iron-contained solution to obtain a polyphenol-Fe solution. A reducing agent is added to the polyphenol-Fe solution. A reaction is implemented to synthesize the P-nZVI. The adding amount of the polyphenol is 10 to 50 parts by weight with respect to 100 parts by weight of iron.

    Abstract translation: 目的:提供一种用于恢复土壤和地下水的多酚包覆纳米级零价铁(P-nZVI)及其制备方法,以扩大P-nZVI的有效半径,包括优异的分散性和流动性 。 构成:制备P-nZVI的方法包括:将多酚加入含铁溶液中以得到多酚-Fe溶液。 将还原剂加入到多酚-Fe溶液中。 进行反应以合成P-nZVI。 相对于100重量份的铁,多酚的添加量为10〜50重量份。