Abstract:
A polymer filament comprising a polyolefin composition which comprises at least 10% by weight of one or more copolymer(s) (I) of propylene with one or more comonomers selected from ethylene, C 4 -C 10 α-olefins and their combinations, said copolymer or copolymers (I) having MFR from 0.5 to 10 g/10 min. and containing units deriving from the said comonomers in a total amount of from 0.5 to 25% by weight with respect to the total amount of all momoner units in the copolymer, provided that, in the absence of comonomer units deriving from C 6 -C 10 α-olefins, the amount of comonomer units deriving from ethylene or C 4 -C 5 α-olefins or their combinations is at least 2.5% by weight.
Abstract:
A polyolefϊn composition comprising, in percentage by weight based on the weight sum of the components (al), (a2) and (b): al) 16-78 % of a propylene homopolymer or copolymer containing at most 15% of ethylene and/or C4-C10 α-olefm(s), having an isotactic index over 80%; and a2) 6-44% of a copolymer of ethylene with one or more C 4 -C 10 α-olefm(s) containing from 10 to 40%, preferably from 15 to 35%,of said C 4 -C 10 α-olefm(s); b) 3-70% of a butene-1 (co)polymer having: - a content of butene-1 derived units of 80% wt or more, - flexural modulus (MEF) of 60 MPa or less. The polyolefϊn composition exhibits good impact resistance, excellent whitening resistance and relatively low stiffness combined with good optical properties suitable for injection and blow molding, thermoforming and film application.
Abstract:
A skin-core fiber wherein the skin comprises a propylene ethylene copolymer having: : i) xylene soluble fraction from 14 wt% to 27 wt% ii) intrinsic viscosity of the fraction soluble in xylene at 25°C from 1.0 to 2.4 dl/g; iii) melt flow rate, MFR, from 1.0 g/10 min to 50.0 g/10 min; iv) an ethylene content from 5.0 wt% to 12.0 wt% v) the ethylene content on the fraction insoluble in xylene from 2.5 wt% to 6.0 wt%; vi) the ethylene content on the fraction soluble in xylene ranging from 15.2. wt% to 30.2 wt% vii) the C 13 NMR sequences PEP on the fraction insoluble in xylene from 3.5mol% to 5.5mol% and the sequences PEP on the fraction soluble in xylene from 11.0 mol% to 14.2 mol%; the core of the fiber comprises a polyethylene having a density between 0.940 g/cm 3 to 0.975 g/cm 3 .
Abstract:
A polyolefin composition comprising: T1) 70-95wt%, a polyolefin component containing: a1) from 30 wt% to 70 wt% of a propylene based polymer; and a2) from 30 wt% to 70 wt% of an ethylene based polymer; the sum of a1) and a2), being referred to the total weight of a1) and a2), being 100; T2) 5-30 wt% of a propylene ethylene copolymer containing from 2.0 wt% to 10.0 wt%; of ethylene derived units and having the melt flow rate (230°C/2.16 kg) ranging from 0.5 to 20.0 g/10 min, and having a fraction soluble in xylene at 25°C lower than 20 wt%. the sum of the amount of T1) and T2), being referred to the total weight of T1) and T2), being 100;
Abstract:
A plate for use in an extrusion-based additive manufacturing system comprising as a top layer a sheet or film comprising 1-butene based copolymer containing from 0 to 50 wt% of ethylene, propylene or alpha olefins of formula CH 2 =CHR, wherein R is a C 3 -C 10 alkyl radical.
Abstract:
A consumable filament for use in an extrusion-based additive manufacturing system comprising a propylene terpolymer containing ethylene and 1-butene or 1-hexene as comonomers having: -MFR L (Melt Flow Rate according to ISO 1133, condition L, i.e. 230°C and 2.16 kg load) ranging from 1 to 20 g/10 min; - xylene solubles measured at 25°C comprised between 3 wt% and 30 wt%.
Abstract:
A fiber comprising a propylene ethylene copolymer, said propylene ethylene copolymer having: i) xylene soluble fraction at 25°C ranging from 14 wt% to 27 wt% ii) intrinsic viscosity of the fraction soluble in xylene at 25°C ranging from 1.0 to 2.4 dl/g; 111) melt flow rate, MFR, ranging from 1.0 g/10 min to 50.0 g/10 min; iv) an ethylene derived units content ranging from 5.0 wt% to 12.0 wt% v) the ethylene derived units content on the fraction insoluble in xylene at 25°C ranging from 2.5 wt% to 6.0 wt%; Vl) the ethylene derived units content on the fraction soluble in xylene at 25 °C ranging from 15.2. wt% to 30.2 wt% vii) the C 13 NMR sequences PEP measured on the fraction insoluble in xylene at 25°C ranging from 3.5mol% to 5.5mol% and the C 13 NMR sequences PEP measured on the fraction soluble in xylene at 25 °C ranging from 11.0 mol% to 14.2 mol%.
Abstract:
The use of a propylene homopolymer for producing fibers; wherein the propylene homopolymer is characterized in that: - the melting point ranges from 150°C to 164°C; - the fraction soluble in xylene at 25°C is comprised between 6.0 wt% and 2.0 wt%; - the fraction soluble in acetone 25°C is comprised between 0.5 wt% and 2.0 wt%; - the ratio fraction soluble in xylene at 25°C/ fraction soluble in acetone 25°C is comprised between 30 wt% and 60 wt%; - the polydispersity index ranges from 2.8 to 4.5 the melt flow rate (ISO 1133, 230 °C/2.16 kg) is comprised between 2 to 40 g/10min.
Abstract:
A polyolefin composition for preparing fibres, comprising: A) 60-95% by weight of a propylene homo- or copolymer, or mixture of said homo- or copolymer; B) 5-40% by weight of a copolymer of butene-1 or a butene-1 polymer composition having: - a Melt Flow Rate value of from 20 to 100 g/10 min., measured according to ISO 1133 at 190°C with a load of 2.16 kg; - a copolymerized comonomer content from 4% to 15% by mole, referred to the total weight of B); - a Mw/Mn value equal to or lower than 4; - flexural modulus of 80 MPa or higher.
Abstract:
Pipe systems having at least one layer comprising a semi-crystalline random polymer of propylene and 0.2 to 5 wt% 1-hexen and optionally a recurring unit selected from ethylene and a C 4 -C 10 α-olefin in an amount from more than 0 to 9 % by moles. The polymer exhibits broad molecular weight distribution, in terms of the ratio of weight average molecular weight to numeric average molecular weight formula (I), ranging from 5 to 11, molecular weight distribution of monomodal type and hexen-1 content in the fraction with an intrinsic viscosity of equal to or higher than 3.3 dl/g lower than the hexen-1 content in the fraction with an intrinsic viscosity of less than 3.3 dl/g.