3.
    发明专利
    未知

    公开(公告)号:DE4120723A1

    公开(公告)日:1992-12-24

    申请号:DE4120723

    申请日:1991-06-22

    Applicant: BASF AG

    Abstract: Described is a method of treating the surface of moulded polyamide articles by treating with aqueous acids, the method being characterized in that mixtures of aqueous hydrochloric acid (strength at least 20 % by wt.) with mono- or diethers of an aliphatic polyhydroxy compound are used, the components of the mixture being in the ratio 90:10 to 10:90 % by vol.

    9.
    发明专利
    未知

    公开(公告)号:DE19503326A1

    公开(公告)日:1996-08-08

    申请号:DE19503326

    申请日:1995-02-02

    Applicant: BASF AG

    Abstract: The invention concerns a foil, in particular for food packaging, said foil consisting of a polymer P1 or a mixture containing: P1: 0.1 to 100 wt %. of a rubber-elastic block copolymer P1 comprising at least one block S, which comprises vinylaromatic monomer units, incorporated by polymerization, and which forms a hard phase, and at least one elastomer block B/S, which comprises units, incorporated by polymerization, both of a vinylaromatic monomer (S) and of (B), and which forms a soft phase, the glass transition temperature Tg of the block S being more than 25 DEG C and that of the block B/S being less than 25 DEG C, and the phase-volume ratio of block S to block B/S being such that the hard phase portion in the total block copolymer is 1 to 40 vol % and the portion of the diene is less than 50 wt %; P2: 0 to 99.9 wt % of a thermoplastically formable and/or duroplastic polymer P2; P3: 0 to 70 wt % of further additives and forming auxiliary agents, the total of the weight percentages of constituents P1 to P3 being 100 %.

    10.
    发明专利
    未知

    公开(公告)号:DE59106535D1

    公开(公告)日:1995-10-26

    申请号:DE59106535

    申请日:1991-11-26

    Applicant: BASF AG

    Abstract: Thermoplastic molding compositions are obtainable by mixing A) from 0.5 to 5% by weight of a thermoplastic polyester elastomer and B) from 0 to 50% by weight of fibrous or particulate fillers or mixtures thereof into a melt of C) from 40 to 99.5% by weight of a polyamide prepolymer having a viscosity number of from 40 to 80 ml/g and subsequent postcondensation in solid phase.