Powdered resin coating compsn. contg. masked acyl isocyanate - for metals, concretes, ceramics, glass, plastics, wood etc.

    公开(公告)号:DE2633385A1

    公开(公告)日:1978-01-26

    申请号:DE2633385

    申请日:1976-07-24

    Applicant: BASF AG

    Abstract: Powdered coating agents contains, as binder forming components, a mixture of (A) >=1 OH-gp. contg. resin, with an OH value of 30-200, pref. 60-120, a glass temp. of 35-95 degrees C, pref. 45-70 degrees C and an average mol. wt. of 1000-10,000, pref. 2000-70000, and (B) >=1 di- or polyacyl isocyanate masked by an aliphatic monoalcohol opt. contg. ether gp(s). The compsn. can be stoved at 150-200 degrees C. pref. 160-175 degrees C, for 5-40, pref. 10-30 mins, to give cross-linked elastic, solvent-stable and corrosion-protecting coatings having good flow properties and high polish on metals, glass, ceramics, concrete, plastics, wood, etc. The decompsn. products produced are relatively free from environmental problems.

    Heat-hardenable coating compsn - contg styrene-acrylic copolymer and epoxy deriv of acetylene di-urea, as powder or solvent lacquer

    公开(公告)号:DE2406998A1

    公开(公告)日:1975-08-28

    申请号:DE2406998

    申请日:1974-02-14

    Applicant: BASF AG

    Abstract: A heat-hardenable coating compsn. contains as binder a mixt. of (A) 94-60 (90-70) pts. wt. of a copolymer of (a) 25-70 (45-65) wt. % is not 1 vinyl-aromatic and/or methyl methacrylate and/or (meth)acrylonitrile, (b) 20-60 (30-55) wt. % is not 1 ester of a 3-5C olefinically unsatd. carboxylic acid with 1-18C alkanol, and (c) 3-25 (5-15) wt. % of an alpha, beta-ethylenically unsatd. nomo- or di-carboxylic acid, with melt viscosity fo 500-10,000 Pas at 120 degrees C and (B) 6-40 pts. wt. of a cpd. with 2 epoxy gps. of formula:- where R is -CH2- , H, (cyclo)alkyl, aryl, acyl or a residue of formula:- and n = 1-10. The compsn. may be used as a powder coating or a solvent lacquer. It can be applied to substrate, e.g. metals by electrostatic deposition and baked at 130-220 degrees (140-180 degrees C). The coating is hard, elastic, glossy, fast to light and to weather; it does not become yellow. The compsn. is brittle and easily ground at room temp. The raw materials are cheap and easily available. The powder compsn. evolves little volatile matter on baking.