公开(公告)号:WO03000786A8
公开(公告)日:2003-02-06
申请号:PCT/EP0206546
申请日:2002-06-14
Applicant: BASF AG , EMRI IGOR , VON BERNSTORFF BERND-STEFFEN , RAUSCHENBERGER VOLKER , HORN HANS CHRISTOPH
-
公开(公告)号:PL367818A1
公开(公告)日:2005-03-07
申请号:PL36781802
申请日:2002-06-14
Applicant: BASF AG
IPC: C08L67/00 , C08L67/02 , C08L77/00 , C08L77/02 , C08L77/06 , C08L77/12 , C08L101/02 , C08L101/12
Abstract: The invention relates to a thermoplastic polymer mixture containing m, m representing a natural number higher than 1, polymers Pn wherein n represents a natural number between 1 and m, and at least one recurring functional group contained in the Pn polymer chain, said group(s) having the structure -(R )x-C(O)-(R )y- wherein x and y independently represent 0 or 1, and x+y=1, and R , R independently represent oxygen or nitrogen linked into the main polymer chain. The polymers Pn differ in terms of at least one characteristic related to molecular weight. The polymer mixture has a number average molecular weight Mn(P)1, a weight average molecular weight Mw(P)1, a Z average molecular weight Mz(P)1, a heterogeneity index Mw(P)1/Mn(P)1, and a molecular weight Mp(P)1 defined according to DIN 55672-2 in hexafluoroisopropanol as an elution agent. After maintaining the polymer mixture at the melting point of the same, defined according to ISO 11357-1 and 11357-3, for five minutes, the polymer mixture has a number average molecular weight Mn(P)2, a weight average molecular weight Mw(P)2, a Z average molecular weight Mz(P)2, a heterogeneity index Mw(P)2/Mn(P)2, and a molecular weight Mp(P)2 defined according to DIN 55672-2 in hexafluoroisopropanol as an elution agent. The values Mn(P)2, Mw(P)2, Mz(P)2, Mw(P)2/Mn(P)2 and Mp(P)2 lie within the triple replication standard deviation sigma (r) in relation to Mn(P)1, Mw(P)1, Mz(P)1, Mw(P)1/Mn(P)1 and Mp(P
-
公开(公告)号:HU0401480A2
公开(公告)日:2004-10-28
申请号:HU0401480
申请日:2002-06-14
Applicant: BASF AG
Abstract: The invention relates to a thermoplastic polymer mixture containing m, m representing a natural number higher than 1, polymers Pn wherein n represents a natural number between 1 and m, and at least one recurring functional group contained in the Pn polymer chain, said group(s) having the structure -(R )x-C(O)-(R )y- wherein x and y independently represent 0 or 1, and x+y=1, and R , R independently represent oxygen or nitrogen linked into the main polymer chain. The polymers Pn differ in terms of at least one characteristic related to molecular weight. The polymer mixture has a number average molecular weight Mn(P)1, a weight average molecular weight Mw(P)1, a Z average molecular weight Mz(P)1, a heterogeneity index Mw(P)1/Mn(P)1, and a molecular weight Mp(P)1 defined according to DIN 55672-2 in hexafluoroisopropanol as an elution agent. After maintaining the polymer mixture at the melting point of the same, defined according to ISO 11357-1 and 11357-3, for five minutes, the polymer mixture has a number average molecular weight Mn(P)2, a weight average molecular weight Mw(P)2, a Z average molecular weight Mz(P)2, a heterogeneity index Mw(P)2/Mn(P)2, and a molecular weight Mp(P)2 defined according to DIN 55672-2 in hexafluoroisopropanol as an elution agent. The values Mn(P)2, Mw(P)2, Mz(P)2, Mw(P)2/Mn(P)2 and Mp(P)2 lie within the triple replication standard deviation sigma (r) in relation to Mn(P)1, Mw(P)1, Mz(P)1, Mw(P)1/Mn(P)1 and Mp(P
-
公开(公告)号:CA2449895A1
公开(公告)日:2003-01-03
申请号:CA2449895
申请日:2002-06-14
Applicant: BASF AG
IPC: C08L67/00 , C08L67/02 , C08L77/00 , C08L77/02 , C08L77/06 , C08L77/12 , C08L101/02 , C08L101/12
Abstract: The invention relates to a thermoplastic polymer mixture containing m, m representing a natural number higher than 1, polymers Pn wherein n represent s a natural number between 1 and m, and at least one recurring functional grou p contained in the Pn polymer chain, said group(s) having the structure -(R1)x - C(O)-(R2)y- wherein x and y independently represent 0 or 1, and x + y = 1, a nd R1, R2 independently represent oxygen or nitrogen linked into the main polym er chain. The polymers Pn differ in terms of at least one characteristic relate d to molecular weight. The polymer mixture has a number average molecular weig ht Mn(P)1, a weight average molecular weight Mw(P)1, a Z average molecular weig ht Mz(P)1, a heterogeneity index Mw(P)1/Mn(P)1 and a molecular weight Mp(P)1 defined according to DIN 55672-2 in hexafluoroisopropanol as an elution agen t. After maintaining the polymer mixture at the melting point of the same, defined according to ISO 11357-1 and 11357-3, for five minutes, the polymer mixture has a number average molecular weight Mn(P)2, a weight average molecular weight Mw(P)2, a Z average molecular weight Mz(P)2, a heterogeneit y index Mw(P)2/Mn(P)2, and a molecular weight Mp(P)2 defined according to DIN 55672-2 in hexafluoroisopropanol as an elution agent. The values Mn(P)2, Mw(P)2, Mz(P)2, Mw(P)2/Mn(P)2 and Mp(P)2 lie within the triple replication standard deviation sigma (r) in relation to Mn(P)1, Mw(P)1, Mz(P)1, Mw(P)1/Mn(P)1 and Mp(P)1 according to DIN 55672-2 in hexafluoroisopropanol a s an elution agent.
-
公开(公告)号:HU0600301A2
公开(公告)日:2006-07-28
申请号:HU0600301
申请日:2002-06-13
Applicant: BASF AG
Abstract: A thermoplastic polymer mixture comprising m polymers Pn, where m is a natural number greater than 1 and n is a natural number from 1 to m, where n is a natural number from 1 to m, where each of the polymers has one or more functional groups of the structure -(R )x-C(O)-(R )y- present as repeat units in the main chain of polymer Pn where x and y, independently of one another, are 0 or 1, and x+y=1 R and R , independently of one another, are oxygen or nitrogen bonded into the main polymer chain, where in the differential distribution curve W(M) determined to DIN 55672-2 in hexafluoroisopropanol as eluent the polymer mixture has at least two maxima of the relative frequency W, and after aging of the polymer mixture at the melting point of the polymer mixture determined to ISO 11357-1 and 11357-3 for 5 minutes, the polymer mixture has in the differential distribution curve W(M) determined to DIN 55672-2 in hexafluoroisopropanol as eluent at least 2 maxima of the relative frequency W, and the position of the maxima here after aging of the polymer mixture at the melting point of the polymer mixture is within three times the recurrent standard deviation sigma(r) of MP in percentage of the value measured to DIN 55672-2, based on the position of the maxima prior to aging of the polymer mixture at the melting point of the polymer mixture.
-
公开(公告)号:BG108521A
公开(公告)日:2004-12-30
申请号:BG10852104
申请日:2004-01-12
Applicant: BASF AG
Inventor: EMRI IGOR , VON BERNSTORFF BERND-STEFFEN , RAUSCHENBERGER VOLKER , HORN HANS
Abstract: The invention relates to thermoplastic polymer mixture containing m polymers Pn, wherein m is a natural number from 1 to m and where each of the polymers has one or more functional groups with structure -(R1)x-C(O)-(R2)y- found as recurring unit of polymer Pn, wherein x and y independently are 0 or 1 and x+ y = 1; R1 and R2, independently, are oxygen or nitrogen, bound to the main polymer chain, wherein the differential curve of distribution W(M) of the polymer mixture there are at least two maximums at relative occurrence W, and after ageing of the polymer mixture at the melting point, at least two maximums at relative occurrence W. The position of the maximums ageing of the polymer mixture at its melting point is within the triple recurrent standard deviation sigma (r) of Mp in percentages from the value, related to the position of the maximums before ageing of the polymer mixture at its melting point.
-
公开(公告)号:DE10129522A1
公开(公告)日:2003-01-09
申请号:DE10129522
申请日:2001-06-21
Applicant: BASF AG
IPC: C08L67/00 , C08L67/02 , C08L77/00 , C08L77/02 , C08L77/06 , C08L77/12 , C08L101/02 , C08L77/10 , C08G69/26 , C08J3/11 , C08J5/02 , D01F6/80
Abstract: The invention relates to a thermoplastic polymer mixture containing m, m representing a natural number higher than 1, polymers Pn wherein n represents a natural number between 1 and m, and at least one recurring functional group contained in the Pn polymer chain, said group(s) having the structure -(R )x-C(O)-(R )y- wherein x and y independently represent 0 or 1, and x + y = 1, and R , R independently represent oxygen or nitrogen linked into the main polymer chain. The polymers Pn differ in terms of at least one characteristic related to molecular weight. The polymer mixture has a number average molecular weight Mn(P)1, a weight average molecular weight Mw(P)1, a Z average molecular weight Mz(P)1, a heterogeneity index Mw(P)1/Mn(P)1 and a molecular weight Mp(P)1 defined according to DIN 55672-2 in hexafluoroisopropanol as an elution agent. After maintaining the polymer mixture at the melting point of the same, defined according to ISO 11357-1 and 11357-3, for five minutes, the polymer mixture has a number average molecular weight Mn(P)2, a weight average molecular weight Mw(P)2, a Z average molecular weight Mz(P)2, a heterogeneity index Mw(P)2/Mn(P)2, and a molecular weight Mp(P)2 defined according to DIN 55672-2 in hexafluoroisopropanol as an elution agent. The values Mn(P)2, Mw(P)2, Mz(P)2, Mw(P)2/Mn(P)2 and Mp(P)2 lie within the triple replication standard deviation sigma (r) in relation to Mn(P)1, Mw(P)1, Mz(P)1, Mw(P)1/Mn(P)1 and Mp(P)1 according to DIN 55672-2 in hexafluoroisopropanol as an elution agent.
-
公开(公告)号:BR0210573A
公开(公告)日:2004-08-03
申请号:BR0210573
申请日:2002-06-13
Applicant: BASF AG
Abstract: A thermoplastic polymer mixture comprising m polymers Pn, where m is a natural number greater than 1 and n is a natural number from 1 to m, where n is a natural number from 1 to m, where each of the polymers has one or more functional groups of the structure -(R )x-C(O)-(R )y- present as repeat units in the main chain of polymer Pn where x and y, independently of one another, are 0 or 1, and x+y=1 R and R , independently of one another, are oxygen or nitrogen bonded into the main polymer chain, where in the differential distribution curve W(M) determined to DIN 55672-2 in hexafluoroisopropanol as eluent the polymer mixture has at least two maxima of the relative frequency W, and after aging of the polymer mixture at the melting point of the polymer mixture determined to ISO 11357-1 and 11357-3 for 5 minutes, the polymer mixture has in the differential distribution curve W(M) determined to DIN 55672-2 in hexafluoroisopropanol as eluent at least 2 maxima of the relative frequency W, and the position of the maxima here after aging of the polymer mixture at the melting point of the polymer mixture is within three times the recurrent standard deviation sigma(r) of MP in percentage of the value measured to DIN 55672-2, based on the position of the maxima prior to aging of the polymer mixture at the melting point of the polymer mixture.
-
公开(公告)号:CZ20033514A3
公开(公告)日:2004-05-12
申请号:CZ20033514
申请日:2002-06-14
Applicant: BASF AG
IPC: C08L67/00 , C08L67/02 , C08L77/00 , C08L77/02 , C08L77/06 , C08L77/12 , C08L101/02 , C08L101/12
Abstract: The invention relates to a thermoplastic polymer mixture containing m, m representing a natural number higher than 1, polymers Pn wherein n represents a natural number between 1 and m, and at least one recurring functional group contained in the Pn polymer chain, said group(s) having the structure -(R )x-C(O)-(R )y- wherein x and y independently represent 0 or 1, and x+y=1, and R , R independently represent oxygen or nitrogen linked into the main polymer chain. The polymers Pn differ in terms of at least one characteristic related to molecular weight. The polymer mixture has a number average molecular weight Mn(P)1, a weight average molecular weight Mw(P)1, a Z average molecular weight Mz(P)1, a heterogeneity index Mw(P)1/Mn(P)1, and a molecular weight Mp(P)1 defined according to DIN 55672-2 in hexafluoroisopropanol as an elution agent. After maintaining the polymer mixture at the melting point of the same, defined according to ISO 11357-1 and 11357-3, for five minutes, the polymer mixture has a number average molecular weight Mn(P)2, a weight average molecular weight Mw(P)2, a Z average molecular weight Mz(P)2, a heterogeneity index Mw(P)2/Mn(P)2, and a molecular weight Mp(P)2 defined according to DIN 55672-2 in hexafluoroisopropanol as an elution agent. The values Mn(P)2, Mw(P)2, Mz(P)2, Mw(P)2/Mn(P)2 and Mp(P)2 lie within the triple replication standard deviation sigma (r) in relation to Mn(P)1, Mw(P)1, Mz(P)1, Mw(P)1/Mn(P)1 and Mp(P
-
-
-
-
-
-
-
-
-