1.
公开(公告)号:JPH10101954A
公开(公告)日:1998-04-21
申请号:JP24899697
申请日:1997-09-12
Applicant: BASF AG
Inventor: AUWETER HELMUT , BOHN HERIBERT , HABERKORN HERBERT , HORN DIETER , LUEDDECKE ERIK , RAUSCHENBERGER VOLKER
IPC: A23K1/16 , A23L1/275 , A23L5/44 , A61K9/16 , C07C403/24 , C09B61/00 , C09B67/06 , C09B67/10 , C09B67/46 , A23L1/272
Abstract: PROBLEM TO BE SOLVED: To provide a finely powdered carotenoid preparation controllable to have intended coloration effects and having a high bioavailability. SOLUTION: The production process comprises forming a molecular dispersion of carotenoid at an elevated temperature in a water-miscible volatile organic solvent optionally together with an emulsifier and/or an edible oil and adding a protective colloid to the solution. In this process, the hydrophilic solvent component is transferred to the water phase to form a hydrophobic phase of carotenoid as a nano-disperse phase and the obtained hydrosol is heat-treated at 40-90 deg.C. Then the solvent and water are removed from the heat-treated hydrosol to convert it into a water-dispersible dry powder.
-
公开(公告)号:WO03000786A8
公开(公告)日:2003-02-06
申请号:PCT/EP0206546
申请日:2002-06-14
Applicant: BASF AG , EMRI IGOR , VON BERNSTORFF BERND-STEFFEN , RAUSCHENBERGER VOLKER , HORN HANS CHRISTOPH
-
公开(公告)号:BR0210573A
公开(公告)日:2004-08-03
申请号:BR0210573
申请日:2002-06-13
Applicant: BASF AG
Abstract: A thermoplastic polymer mixture comprising m polymers Pn, where m is a natural number greater than 1 and n is a natural number from 1 to m, where n is a natural number from 1 to m, where each of the polymers has one or more functional groups of the structure -(R )x-C(O)-(R )y- present as repeat units in the main chain of polymer Pn where x and y, independently of one another, are 0 or 1, and x+y=1 R and R , independently of one another, are oxygen or nitrogen bonded into the main polymer chain, where in the differential distribution curve W(M) determined to DIN 55672-2 in hexafluoroisopropanol as eluent the polymer mixture has at least two maxima of the relative frequency W, and after aging of the polymer mixture at the melting point of the polymer mixture determined to ISO 11357-1 and 11357-3 for 5 minutes, the polymer mixture has in the differential distribution curve W(M) determined to DIN 55672-2 in hexafluoroisopropanol as eluent at least 2 maxima of the relative frequency W, and the position of the maxima here after aging of the polymer mixture at the melting point of the polymer mixture is within three times the recurrent standard deviation sigma(r) of MP in percentage of the value measured to DIN 55672-2, based on the position of the maxima prior to aging of the polymer mixture at the melting point of the polymer mixture.
-
公开(公告)号:CZ20033514A3
公开(公告)日:2004-05-12
申请号:CZ20033514
申请日:2002-06-14
Applicant: BASF AG
IPC: C08L67/00 , C08L67/02 , C08L77/00 , C08L77/02 , C08L77/06 , C08L77/12 , C08L101/02 , C08L101/12
Abstract: The invention relates to a thermoplastic polymer mixture containing m, m representing a natural number higher than 1, polymers Pn wherein n represents a natural number between 1 and m, and at least one recurring functional group contained in the Pn polymer chain, said group(s) having the structure -(R )x-C(O)-(R )y- wherein x and y independently represent 0 or 1, and x+y=1, and R , R independently represent oxygen or nitrogen linked into the main polymer chain. The polymers Pn differ in terms of at least one characteristic related to molecular weight. The polymer mixture has a number average molecular weight Mn(P)1, a weight average molecular weight Mw(P)1, a Z average molecular weight Mz(P)1, a heterogeneity index Mw(P)1/Mn(P)1, and a molecular weight Mp(P)1 defined according to DIN 55672-2 in hexafluoroisopropanol as an elution agent. After maintaining the polymer mixture at the melting point of the same, defined according to ISO 11357-1 and 11357-3, for five minutes, the polymer mixture has a number average molecular weight Mn(P)2, a weight average molecular weight Mw(P)2, a Z average molecular weight Mz(P)2, a heterogeneity index Mw(P)2/Mn(P)2, and a molecular weight Mp(P)2 defined according to DIN 55672-2 in hexafluoroisopropanol as an elution agent. The values Mn(P)2, Mw(P)2, Mz(P)2, Mw(P)2/Mn(P)2 and Mp(P)2 lie within the triple replication standard deviation sigma (r) in relation to Mn(P)1, Mw(P)1, Mz(P)1, Mw(P)1/Mn(P)1 and Mp(P
-
公开(公告)号:DE10156293A1
公开(公告)日:2003-05-28
申请号:DE10156293
申请日:2001-11-19
Applicant: BASF AG
Inventor: RAUSCHENBERGER VOLKER , LAUN HANS-MARTIN , KISSEL JUTTA , HECKMANN WALTER , BERNSTORFF BERND-STEFFEN VON , HORN HANS CHRISTOPH
Abstract: A thermoplastic polymer mixture (I) containing a polyamide (II) and a polymer (III), where the melt viscosity, as measured at 280 deg C is 100-20,000 s-1 is at most 75% of the melt viscosity measured in accordance with ISO 1443 of polyamide (II) at 280 deg C, and the boundary surface tension between a melt of polyamide (II) and a melt of polyamide (III) at 280 deg C, measured in accordance with US patent 5,50,607 by the Spinning-Drop-Method is in the region of 0-10 mN/m. A thermoplastic polymer mixture (I) containing (wt.%): (a) a polyamide (II)(50-99.9), (b) a polymer (III)( 0.1-50), where the melt viscosity, as measured in accordance with ISO 1443 of polyamide (II) at 280 deg C over the whole Scherraten (sic) region is 100-20,000 s-1 is at most 75% of the melt viscosity measured in accordance with ISO 1443 of polyamide (II) at 280 deg C, and the boundary surface tension between a melt of polyamide (II) and a melt of polyamide (III) at 280 deg C, measured in accordance with US patent 5,50,607 by the Spinning-Drop-Method is in the region of 0-10 mN/m. Independent claims are included for: (1) a process for preparation of a fiber by spinning a melt of a thermoplastic polymer, using the above polymer mixture (I) as the thermoplastic polymer; (2) a fiber obtained by the above process; (3) a carpet containing the above fiber; and (4) flat structure textiles containing the above fiber.
-
-
公开(公告)号:PL367818A1
公开(公告)日:2005-03-07
申请号:PL36781802
申请日:2002-06-14
Applicant: BASF AG
IPC: C08L67/00 , C08L67/02 , C08L77/00 , C08L77/02 , C08L77/06 , C08L77/12 , C08L101/02 , C08L101/12
Abstract: The invention relates to a thermoplastic polymer mixture containing m, m representing a natural number higher than 1, polymers Pn wherein n represents a natural number between 1 and m, and at least one recurring functional group contained in the Pn polymer chain, said group(s) having the structure -(R )x-C(O)-(R )y- wherein x and y independently represent 0 or 1, and x+y=1, and R , R independently represent oxygen or nitrogen linked into the main polymer chain. The polymers Pn differ in terms of at least one characteristic related to molecular weight. The polymer mixture has a number average molecular weight Mn(P)1, a weight average molecular weight Mw(P)1, a Z average molecular weight Mz(P)1, a heterogeneity index Mw(P)1/Mn(P)1, and a molecular weight Mp(P)1 defined according to DIN 55672-2 in hexafluoroisopropanol as an elution agent. After maintaining the polymer mixture at the melting point of the same, defined according to ISO 11357-1 and 11357-3, for five minutes, the polymer mixture has a number average molecular weight Mn(P)2, a weight average molecular weight Mw(P)2, a Z average molecular weight Mz(P)2, a heterogeneity index Mw(P)2/Mn(P)2, and a molecular weight Mp(P)2 defined according to DIN 55672-2 in hexafluoroisopropanol as an elution agent. The values Mn(P)2, Mw(P)2, Mz(P)2, Mw(P)2/Mn(P)2 and Mp(P)2 lie within the triple replication standard deviation sigma (r) in relation to Mn(P)1, Mw(P)1, Mz(P)1, Mw(P)1/Mn(P)1 and Mp(P
-
公开(公告)号:HU0401480A2
公开(公告)日:2004-10-28
申请号:HU0401480
申请日:2002-06-14
Applicant: BASF AG
Abstract: The invention relates to a thermoplastic polymer mixture containing m, m representing a natural number higher than 1, polymers Pn wherein n represents a natural number between 1 and m, and at least one recurring functional group contained in the Pn polymer chain, said group(s) having the structure -(R )x-C(O)-(R )y- wherein x and y independently represent 0 or 1, and x+y=1, and R , R independently represent oxygen or nitrogen linked into the main polymer chain. The polymers Pn differ in terms of at least one characteristic related to molecular weight. The polymer mixture has a number average molecular weight Mn(P)1, a weight average molecular weight Mw(P)1, a Z average molecular weight Mz(P)1, a heterogeneity index Mw(P)1/Mn(P)1, and a molecular weight Mp(P)1 defined according to DIN 55672-2 in hexafluoroisopropanol as an elution agent. After maintaining the polymer mixture at the melting point of the same, defined according to ISO 11357-1 and 11357-3, for five minutes, the polymer mixture has a number average molecular weight Mn(P)2, a weight average molecular weight Mw(P)2, a Z average molecular weight Mz(P)2, a heterogeneity index Mw(P)2/Mn(P)2, and a molecular weight Mp(P)2 defined according to DIN 55672-2 in hexafluoroisopropanol as an elution agent. The values Mn(P)2, Mw(P)2, Mz(P)2, Mw(P)2/Mn(P)2 and Mp(P)2 lie within the triple replication standard deviation sigma (r) in relation to Mn(P)1, Mw(P)1, Mz(P)1, Mw(P)1/Mn(P)1 and Mp(P
-
公开(公告)号:ES2212023T3
公开(公告)日:2004-07-16
申请号:ES97115588
申请日:1997-09-09
Applicant: BASF AG
Inventor: AUWETER HELMUT , BOHN HERIBERT , HABERKORN HERBERT , HORN DIETER , LUEDDECKE ERIK , RAUSCHENBERGER VOLKER
-
公开(公告)号:DE59711046D1
公开(公告)日:2004-01-08
申请号:DE59711046
申请日:1997-09-09
Applicant: BASF AG
Inventor: AUWETER HELMUT , BOHN HERIBERT , HABERKORN HERBERT , HORN DIETER , LUEDDECKE ERIK , RAUSCHENBERGER VOLKER
-
-
-
-
-
-
-
-
-