公开(公告)号:DE2714897A1
公开(公告)日:1978-10-05
申请号:DE2714897
申请日:1977-04-02
Applicant: BASF AG
Inventor: SCHENK WOLFGANG DIPL CHEM DR , STEDEFEDER JOACHIM DIPL CHEM D , LEITNER HEINZ , SCHENCK HANS-UWE DIPL CHEM DR
IPC: C08F220/00 , C08F220/04 , C08F220/06 , C08F220/42 , D06M15/263 , D06M15/285 , D06M15/38
Abstract: A process for sizing staple fiber yarns by applying an aqueous sizing liquor which contains an alkaline earth metal salt of a copolymer containing from 90 to 30% by weight of acrylic acid and/or methacrylic acid and from 10 to 70% by weight of acrylonitrile and/or methacrylonitrile, which copolymer has a viscosity of from 50 to 1,000 cp in 15% strength aqueous solution at 85 DEG C., and drying the treated yarns. The sized films obtained are moisture-insensitive and have good heat stability.
-
2.
公开(公告)号:DE19533218A1
公开(公告)日:1997-03-13
申请号:DE19533218
申请日:1995-09-08
Applicant: BASF AG
Inventor: HAEBERLE KARL DR , FUCHS HORST , REICHERT JUERGEN DR , SENDHOFF NORBERT DR , LEITNER HEINZ
IPC: C08G18/08 , C08G18/80 , D06M15/263 , D06M15/333 , D06M15/507 , D06M15/564 , D06M15/568 , D06P1/00 , D06P1/22 , D06P1/52 , D06P1/54 , D06P3/60 , D06P3/85
Abstract: The claims concern the use of hydrophilic modified polyisocyanates (I) in combination with (a) sizes (II) cured with (I) for producing permanently sized yarns and (b) (II) and indigo for 1-stage sizing and dyeing of yarns or dyeing and printing of fabrics.
-
公开(公告)号:FI891274A0
公开(公告)日:1989-03-17
申请号:FI891274
申请日:1989-03-17
Applicant: BASF AG
Inventor: BRUECKMANN RALF , LEITNER HEINZ , SCHOEPKE HOLGER
IPC: C08L67/02 , C08G63/12 , C08G63/20 , C08L67/00 , D06M13/02 , D06M13/325 , D06M15/507 , D06M101/00 , D06M101/16 , D06M101/30 , D06M101/32 , C08G
Abstract: The process involves… a) condensing aromatic dicarboxylic acids or esters thereof with at least one diol to give prepolymers having an acid number of from 2 to 8,… b) reacting the prepolymers with at least one molecular-weight-increasing compound, for example trimellitic anhydride, to give polyesters having acid numbers of from 40 to 60, and… c) dispersing the polyesters by adding aqueous mixtures of ammonia and amines in a molar ratio of from 10:1 to 1:10 to give a polyester melt which has a temperature in the range from 150 to 210 DEG C. … The polyester dispersions are used as sizes or sizing filament warp thread.
-
公开(公告)号:DK128189D0
公开(公告)日:1989-03-16
申请号:DK128189
申请日:1989-03-16
Applicant: BASF AG
Inventor: BRUECKMANN RALF , LEITNER HEINZ , SCHOEPKE HOLGER
IPC: C08L67/02 , C08G63/12 , C08G63/20 , C08L67/00 , D06M13/02 , D06M13/325 , D06M15/507 , D06M101/00 , D06M101/16 , D06M101/30 , D06M101/32 , C08J3/06
Abstract: The process involves… a) condensing aromatic dicarboxylic acids or esters thereof with at least one diol to give prepolymers having an acid number of from 2 to 8,… b) reacting the prepolymers with at least one molecular-weight-increasing compound, for example trimellitic anhydride, to give polyesters having acid numbers of from 40 to 60, and… c) dispersing the polyesters by adding aqueous mixtures of ammonia and amines in a molar ratio of from 10:1 to 1:10 to give a polyester melt which has a temperature in the range from 150 to 210 DEG C. … The polyester dispersions are used as sizes or sizing filament warp thread.
-
公开(公告)号:CH623973B5
公开(公告)日:1982-01-15
申请号:CH350678
申请日:1978-03-31
Applicant: BASF AG
Inventor: SCHENK WOLFGANG DR , STEDEFEDER JOACHIM DR , LEITNER HEINZ , SCHENCK HANS-UWE DR
IPC: C08F220/00 , C08F220/04 , C08F220/06 , C08F220/42 , D06M15/263 , D06M15/285 , D06M15/14
-
公开(公告)号:ES2047049T3
公开(公告)日:1994-02-16
申请号:ES89103945
申请日:1989-03-07
Applicant: BASF AG
Inventor: BRUECKMANN RALF DR , LEITNER HEINZ , SCHOEPKE HOLGER DR
IPC: C08L67/02 , C08G63/12 , C08G63/20 , C08L67/00 , D06M13/02 , D06M13/325 , D06M15/507 , D06M101/00 , D06M101/16 , D06M101/30 , D06M101/32
Abstract: The process involves… a) condensing aromatic dicarboxylic acids or esters thereof with at least one diol to give prepolymers having an acid number of from 2 to 8,… b) reacting the prepolymers with at least one molecular-weight-increasing compound, for example trimellitic anhydride, to give polyesters having acid numbers of from 40 to 60, and… c) dispersing the polyesters by adding aqueous mixtures of ammonia and amines in a molar ratio of from 10:1 to 1:10 to give a polyester melt which has a temperature in the range from 150 to 210 DEG C. … The polyester dispersions are used as sizes or sizing filament warp thread.
-
公开(公告)号:DE58906468D1
公开(公告)日:1994-02-03
申请号:DE58906468
申请日:1989-03-07
Applicant: BASF AG
Inventor: BRUECKMANN RALF DR , LEITNER HEINZ , SCHOEPKE HOLGER DR
IPC: C08L67/02 , C08G63/12 , C08G63/20 , C08L67/00 , D06M13/02 , D06M13/325 , D06M15/507 , D06M101/00 , D06M101/16 , D06M101/30 , D06M101/32
Abstract: The process involves… a) condensing aromatic dicarboxylic acids or esters thereof with at least one diol to give prepolymers having an acid number of from 2 to 8,… b) reacting the prepolymers with at least one molecular-weight-increasing compound, for example trimellitic anhydride, to give polyesters having acid numbers of from 40 to 60, and… c) dispersing the polyesters by adding aqueous mixtures of ammonia and amines in a molar ratio of from 10:1 to 1:10 to give a polyester melt which has a temperature in the range from 150 to 210 DEG C. … The polyester dispersions are used as sizes or sizing filament warp thread.
-
公开(公告)号:AT98976T
公开(公告)日:1994-01-15
申请号:AT89103945
申请日:1989-03-07
Applicant: BASF AG
Inventor: BRUECKMANN RALF DR , LEITNER HEINZ , SCHOEPKE HOLGER DR
IPC: C08L67/02 , C08G63/12 , C08G63/20 , C08L67/00 , D06M13/02 , D06M13/325 , D06M15/507 , D06M101/00 , D06M101/16 , D06M101/30 , D06M101/32
-
公开(公告)号:DE3808882A1
公开(公告)日:1989-09-28
申请号:DE3808882
申请日:1988-03-17
Applicant: BASF AG
Inventor: BRUECKMANN RALF DR , LEITNER HEINZ , SCHOEPKE HOLGER DR
IPC: C08L67/02 , C08G63/12 , C08G63/20 , C08L67/00 , D06M13/02 , D06M13/325 , D06M15/507 , D06M101/00 , D06M101/16 , D06M101/30 , D06M101/32
Abstract: The process involves… a) condensing aromatic dicarboxylic acids or esters thereof with at least one diol to give prepolymers having an acid number of from 2 to 8,… b) reacting the prepolymers with at least one molecular-weight-increasing compound, for example trimellitic anhydride, to give polyesters having acid numbers of from 40 to 60, and… c) dispersing the polyesters by adding aqueous mixtures of ammonia and amines in a molar ratio of from 10:1 to 1:10 to give a polyester melt which has a temperature in the range from 150 to 210 DEG C. … The polyester dispersions are used as sizes or sizing filament warp thread.
-
公开(公告)号:FI891274A
公开(公告)日:1989-09-18
申请号:FI891274
申请日:1989-03-17
Applicant: BASF AG
Inventor: BRUECKMANN RALF , LEITNER HEINZ , SCHOEPKE HOLGER
IPC: C08L67/02 , C08G63/12 , C08G63/20 , C08L67/00 , D06M13/02 , D06M13/325 , D06M15/507 , D06M101/00 , D06M101/16 , D06M101/30 , D06M101/32 , C08G
Abstract: The process involves… a) condensing aromatic dicarboxylic acids or esters thereof with at least one diol to give prepolymers having an acid number of from 2 to 8,… b) reacting the prepolymers with at least one molecular-weight-increasing compound, for example trimellitic anhydride, to give polyesters having acid numbers of from 40 to 60, and… c) dispersing the polyesters by adding aqueous mixtures of ammonia and amines in a molar ratio of from 10:1 to 1:10 to give a polyester melt which has a temperature in the range from 150 to 210 DEG C. … The polyester dispersions are used as sizes or sizing filament warp thread.
-
-
-
-
-
-
-
-
-