METHOD FOR PRODUCING GLUED WOOD IN SHORT PHASES
    1.
    发明申请
    METHOD FOR PRODUCING GLUED WOOD IN SHORT PHASES 审中-公开
    在短切过程中生产润滑木材的方法

    公开(公告)号:WO2004033577A3

    公开(公告)日:2004-07-01

    申请号:PCT/EP0311078

    申请日:2003-10-07

    CPC classification number: C09J5/04 B27G11/00 B27M3/0053 B27M3/0086 C09J5/06

    Abstract: The invention relates to a method for gluing wood parts/components (10) by means of thermoplastic or duroplastic glue resins or glue resin systems. Before the wood parts/components (10) are glued, the entire cross-section (8) of the wood parts/components (10) is heated through evenly in an electromagnetic radiation field (9). The heated wood parts or wood components (10) are glued by the separate application of glue resin and hardener (binder) or of a mixed glue system consisting of glue resin and hardener.

    Abstract translation: 木材部件/木质部件的本发明涉及一种通过热塑性粘合木材部件/木质部件(10)或热固性其中在所述木材部件/木质部件的胶合(10)的整个横截面的均匀加热粘合剂树脂或Leimharzsysteme(8)(10 )发生在电磁辐射场(9)中。 加热的木质部件或木质部件(10)的胶合通过胶粘树脂和硬化剂(粘合剂)的单独施加或胶合树脂和硬化剂胶水系统的混合来进行。

    5.
    发明专利
    未知

    公开(公告)号:NO20033056L

    公开(公告)日:2003-09-03

    申请号:NO20033056

    申请日:2003-07-03

    Applicant: BASF AG

    Abstract: Woodbase materials comprise wood pieces glued using an adhesive composition comprising an isocyanato-bearing prepolymer (prepolymer P) derived from A) a component A comprising A1) from 25 to 100% by weight of a triglyceride having two or more reactive groups which may react with isocyanate groups in an addition reaction (triglycerides A1), and A2) from 0 to 75% by weight of another compound having one or more reactive groups which may react with isocyanate groups in an addition reaction (component A2), and B) a component B comprising a polyisocyanate if desired, customary auxiliaries and additives if desired, an activator, and if desired, a filler, and adhesive compositions.

Patent Agency Ranking