公开(公告)号:DE2302370A1
公开(公告)日:1974-07-25
申请号:DE2302370
申请日:1973-01-18
Applicant: BASF AG
Inventor: MUELLER-TAMM HEINZ DR , BUECHNER OSKAR DR , GIERTH VOLKER DR , WENDLER KLAUS
Abstract: The powder is heated to 15-20 degrees C below its melting range, fed into an agglomerating device and raised by mechanical friction to 2-13 degrees C below melting range, held there 2-10 mins passed at >=30 degrees C below melting range through a crusher/sieve to separate particles >3.5 mm dia diameter. The agglomerating device is a cylinder with rotating hammer, baffles and several anvils of specified sizes, the hammer rotates at a specified speed relative to the baffle periphery. The result is a fine powder with very low content of particles 200 mu m dia.
-
公开(公告)号:DE2147262A1
公开(公告)日:1973-03-29
申请号:DE2147262
申请日:1971-09-22
Applicant: BASF AG
Inventor: STEIGERWALD KLAUS DR , GIERTH VOLKER DR , ZIZLSPERGER JOHANN DR , WENDLER KLAUS
Abstract: Polyisobutylene is heated to 120 - 200 degrees C before mixing with polyolefin at 120 - 200 degrees C with shearing at a rate of 700 - 1200 cm-1. Homogeneous mixts. are obtd. in a single stage and are used for impact and tear resistant mouldings, foams, cable insulation and packaging.
-
公开(公告)号:DE2302329A1
公开(公告)日:1974-07-25
申请号:DE2302329
申请日:1973-01-18
Applicant: BASF AG
Inventor: MUELLER-TAMM HEINZ DR , BUECHNER OSKAR DR , GIERTH VOLKER DR , WENDLER KLAUS
Abstract: Reducing the proportion of particles with dia. below 200 m mu in finely divided polyolefins e.g. polyethylene, comprising particles with dia below 3.5 mm, comprises (1) suspending 1 pbe of the polyolefin, in 2-6 pbw of a water-sol, inert, liq. e.g. ethylene glycol; heating the resulting suspension to 2-6.5 degrees C below the melting range of the polymer, maintaining the suspension at that temp. for 5-30, the processing time being of a duration inversely proportional to the working temp; then (2) separating the so-treated polyolefin from the suspension medium; washing with water; and drying. Step (1) is effected under continuous stirring. The resulting dust-free prod. has improved flow characteristics and is free of voids giving mouldings free of cavities.
-
公开(公告)号:DE2203553A1
公开(公告)日:1973-08-02
申请号:DE2203553
申请日:1972-01-26
Applicant: BASF AG
Inventor: TRIESCHMANN HANS-GEORG PROF DR , URBAN FRIEDRICH DR , GIERTH VOLKER DR , WENDLER KLAUS , ZIZLSPERGER JOHANN DR , BRUENEMANN HILMAR DIPL-ING
Abstract: The plastics are mixed at high temps. in a shearing gradient, in which the inhomogeneous plastic fusion is fed into the centre of a mixing zone between two parallel circular surfaces equipped with toothed comminuting elements and with >=1 of the circular surfaces rotated to homogenise the fusion at temps. between the m.pt. of >=1 of the plastic components and 350 degrees C.
-
-
-