SYNTHESIS OF LITHIUM- IRON- PHOSPHATES UNDER HYDROTHERMAL CONDITIONS
    1.
    发明申请
    SYNTHESIS OF LITHIUM- IRON- PHOSPHATES UNDER HYDROTHERMAL CONDITIONS 审中-公开
    锂热磷酸盐在氢热条件下的合成

    公开(公告)号:WO2010106035A3

    公开(公告)日:2011-01-06

    申请号:PCT/EP2010053326

    申请日:2010-03-16

    CPC classification number: C01B25/45 H01M4/5825

    Abstract: The present invention relates to a process for the preparation of compounds of general formula (I) Lia-bM1 bFe1-cM2 cPd-eM3 eOx, wherein Fe has the oxidation state +2 and M1, M2, M3, a, b, c, d, e and x are: M1 : Na, K, Rb and/or Cs, M2: Mn, Mg, Al, Ca, Ti, Co, Ni, Cr, V, M3: Si, S, F a: 0.8 - 1.9, b: 0 - 0.3, c: 0 - 0.9, d: 0.8 - 1.9, e: 0 - 0.5, x: 1.0 - 8, depending on the amount and oxidation state of Li, M1, M2, P, M3, wherein compounds of general formula (I) are neutrally charged, comprising the following steps (A) providing a mixture comprising at least one lithium-comprising compound, at least one iron-comprising compound, in which iron has the oxidation state 0, and at least one M1-comprising compound, if present, and/or at least one M2-comprising compound, if present, and/or least one M3-comprising compound, if present, and at least one compound comprising at least one phosphorous atom in oxidation state +5, and (B) heating the mixture obtained in step (A) at a temperature of 100 to 500 °C and at an autogeneous pressure to obtain a compound of general formula (I).

    Abstract translation: 本发明涉及制备通式(I)Lia-bM1 bFe1-cM2 cPd-eM3 eOx的化合物的方法,其中Fe具有氧化态+2和M1,M2,M3,a,b,c, d,e和x是:M1:Na,K,Rb和/或Cs,M2:Mn,Mg,Al,Ca,Ti,Co,Ni,Cr,V,M3:Si,S,F a: 1.9,b:0-0.3,c:0-0.9,d:0.8-1.9,e:0-0.5,x:1.0-8,这取决于Li,M1,M2,P,M3的量和氧化态, 其中通式(I)的化合物是中性带电的,包括以下步骤(A),提供包含至少一种含锂化合物,至少一种含铁化合物的混合物,其中铁具有氧化态为0,并且在 至少一种含M1化合物(如果存在)和/或至少一种含M2化合物(如果存在)和/或至少一种含M3化合物(如果存在)和至少一种包含至少一个磷原子的化合物 状态+5,和(B)在步骤(A)中获得的混合物的温度下加热 100〜500℃,自动压力,得到通式(I)的化合物。

    SYNTHESIS OF LITHIUM-METAL-PHOSPHATES UNDER HYDROTHERMAL CONDITIONS
    2.
    发明申请
    SYNTHESIS OF LITHIUM-METAL-PHOSPHATES UNDER HYDROTHERMAL CONDITIONS 审中-公开
    在氢热条件下合成硫酸金属磷酸盐

    公开(公告)号:WO2010076265A2

    公开(公告)日:2010-07-08

    申请号:PCT/EP2009067742

    申请日:2009-12-22

    CPC classification number: C01B25/45 H01M4/5825 H01M4/625 H01M10/0525

    Abstract: The present invention relates to a process for the preparation of compounds of general formula (I) Lia-bM1 bQ1-cM2 cPd-eM3 eOx (l), wherein Q has the oxidation state +2 and M1, M2, M3, a, b, c, d, e and x are: Q: Fe, Mn, Co, Ni, M1 : Na, K, Rb and/or Cs, M2: Mg, Al, Ca, Ti, Co, Ni, Cr, V, Fe, Mn, wherein Q and M2 are different from each other, M3: Si, S, F a: 0.8 - 1.9, b: 0 - 0.3, c: 0 - 0.9, d: 0.8 - 1.9, e: 0 - 0.5, x: 1.0 - 8, depending on the amount and oxidation state of Li, M1, M2, P, M3, wherein compounds of general formula (I) are neutrally charged, comprising the following steps (A) providing a mixture comprising at least one lithium-comprising compound, at least one Q-comprising compound, in which Q has at least partially an oxidation state higher than +2, and at least one M1-comprising compound, if present, and/or at least one M2-comprising compound, if present, and/or least one M3-comprising compound, if present, and at least one reducing agent which is oxidized to at least one compound comprising at least one phosphorous atom in oxidation state +5, and (B) heating the mixture obtained in step (A) at a temperature of 100 to 500 °C and at an autogeneous pressure to reduce Q to oxidation state +2 and to obtain a compound of general formula (I).

    Abstract translation: 本发明涉及制备通式(Ⅰ)Lia-bM1bQ1-cM2cPd-eM3eOx(1)的化合物的方法,其中Q具有氧化态+2和M1,M2,M3,a,b ,c,d,e和x分别为:Q:Fe,Mn,Co,Ni,M1:Na,K,Rb和/或Cs,M2:Mg,Al,Ca,Ti,Co,Ni,Cr, Fe,Mn,其中Q和M2彼此不同,M3:Si,S,F a:0.8-1.9,b:0-0.3,c:0-0.9,d:0.8-1.9,e:0-0.5 ,x:1.0-8,其取决于Li,M1,M2,P,M3的量和氧化态,其中通式(I)的化合物是中性带电的,包括以下步骤(A),提供至少包含 一种含锂化合物,至少一种含Q的化合物,其中Q至少部分具有高于+2的氧化态,以及至少一种含M1化合物(如果存在)和/或至少一种含M2的化合物 化合物(如果存在)和/或至少一种含M3化合物(如果存在)和至少一种被还原的还原剂 一种化合物,其包含至少一种氧化态+5的磷原子,和(B)在100-500℃的温度和自发压力下加热步骤(A)中获得的混合物以将Q降低至氧化态+2 并得到通式(I)的化合物。

    PRODUCING OXIDIC COMPOUNDS
    4.
    发明专利

    公开(公告)号:CA2787373A1

    公开(公告)日:2011-08-04

    申请号:CA2787373

    申请日:2011-01-28

    Applicant: BASF SE

    Abstract: A process for producing oxidic compounds of the general formula (?) LizMxOy (?) wherein M is one or more elements from groups 2 to 12 of the periodic table, more particularly selected from Co, Mn, Ni, Fe, Al, Mg, x is 1 to 2, y is 2 to 4, and z is 0.5 to 1.5, comprises heating mixtures selected from oxides, hydroxides, carbonates and nitrates of Li and of M together to temperatures in the range from 600 to 1200? in a reaction vessel performing incomplete rotary motions about one axis.

    PROCESS FOR THE PREPARATION OF CRYSTALLINE LITHIUM-, IRON- AND PHOSPHATE-COMPRISING MATERIALS

    公开(公告)号:CA2721204A1

    公开(公告)日:2009-10-22

    申请号:CA2721204

    申请日:2009-04-16

    Applicant: BASF SE

    Abstract: The present invention relates to a Process for the preparation of compounds of general formula (I), Lia-bM1bFe1-cM2 cPd-eM3 eOx, wherein M1, M2, M3, a, b, c, d and e: M1: Na, K, Rb and/or Cs, M2: Mn, Mg, Ca, Ti, Co, Ni, Cr, V, M3: Si, S, a: 0.8 - 1.9, b: 0 - 0.3, c: 0 - 0.9, d: 0.8 - 1.9, e: 0 - 0.5, x: 1.0 - 8, depending on the amount and oxidation state of Li, M1, Fe, M2, P, M3, wherein compounds of general formula (I) are neutrally charged, comprising the following steps (A) providing a mixture comprising at least one lithium-comprising compound, at least one iron-comprising compound, in which iron has the oxidation state +3, and at least one M1-comprising compound, if present, and/or at least one M2-comprising compound, if present, and/or least one M3-comprising compound, if present, and at least one reducing agent which is oxidized to at least one compound comprising at least one phosphorous atom in oxidation state +5, (B) optionally drying the mixture provided in step (A), in order to obtain a solid compound and (C) calcining the solid compound obtained from step (A) or (B) at a temperature of 300 to 1000° C.

    7.
    发明专利
    未知

    公开(公告)号:ES3010294T3

    公开(公告)日:2025-04-02

    申请号:ES11797720

    申请日:2011-06-24

    Applicant: BASF SE

    Abstract: La invención se refiere a un método para producir óxidos metálicos mixtos de litio que contienen esencialmente litio, manganeso, cobalto y níquel como átomos metálicos y tienen una relación estequiométrica de litio con respecto a la colectividad de los metales de transición mayor que 1, que comprende a) la producción de una mezcla denominada producto intermedio (B), que comprende esencialmente hidróxidos metálicos mixtos que contienen litio e hidróxidos de óxidos metálicos mixtos que contienen litio, en la que el manganeso, el cobalto y el níquel están contenidos en la relación (1-ab):a:b y en la que el número de oxidación, promediado sobre todos los iones de manganeso, cobalto y níquel, es al menos 4-1,75a-1,75b, donde 0

    SYNTHESIS OF LITHIUM-IRON-PHOSPHATES

    公开(公告)号:CA2755522A1

    公开(公告)日:2010-09-23

    申请号:CA2755522

    申请日:2010-03-16

    Applicant: BASF SE

    Abstract: The present invention relates to a process for the preparation of compounds of general formula (I) Lia-bM1 bFe1-cM2 cPd-eM3 eOx, wherein Fe has the oxidation state +2 and M1, M2, M3, a, b, c, d, e and x are: M1 : Na, K, Rb and/or Cs, M2: Mn, Mg, Al, Ca, Ti, Co, Ni, Cr, V, M3: Si, S, F a: 0.8 - 1.9, b: 0 - 0.3, c: 0 - 0.9, d: 0.8 - 1.9, e: 0 - 0.5, x: 1.0 - 8, depending on the amount and oxidation state of Li, M1, M2, P, M3, wherein compounds of general formula (I) are neutrally charged, comprising the following steps (A) providing a mixture comprising at least one lithium-comprising compound, at least one iron-comprising compound, in which iron has the oxidation state 0, and at least one M1-comprising compound, if present, and/or at least one M2-comprising compound, if present, and/or least one M3-comprising compound, if present, and at least one compound comprising at least one phosphorous atom in oxidation state +5, and (B) heating the mixture obtained in step (A) at a temperature of 100 to 500 °C and at an autogeneous pressure to obtain a compound of general formula (I).

    SYNTHESIS OF LITHIUM-METAL-PHOSPHATES UNDER HYDROTHERMAL CONDITIONS

    公开(公告)号:CA2746965A1

    公开(公告)日:2010-07-08

    申请号:CA2746965

    申请日:2009-12-22

    Applicant: BASF SE

    Abstract: The present invention relates to a process for the preparation of compounds of general formula (I) Lia-bM1 bQ1-cM2 cPd-eM3 eOx (l), wherein Q has the oxidation state +2 and M1, M2, M3, a, b, c, d, e and x are: Q: Fe, Mn, Co, Ni, M1 : Na, K, Rb and/or Cs, M2: Mg, Al, Ca, Ti, Co, Ni, Cr, V, Fe, Mn, wherein Q and M2 are different from each other, M3: Si, S, F a: 0.8 - 1.9, b: 0 - 0.3, c: 0 - 0.9, d: 0.8 - 1.9, e: 0 - 0.5, x: 1.0 - 8, depending on the amount and oxidation state of Li, M1, M2, P, M3, wherein compounds of general formula (I) are neutrally charged, comprising the following steps (A) providing a mixture comprising at least one lithium-comprising compound, at least one Q-comprising compound, in which Q has at least partially an oxidation state higher than +2, and at least one M1-comprising compound, if present, and/or at least one M2-comprising compound, if present, and/or least one M3-comprising compound, if present, and at least one reducing agent which is oxidized to at least one compound comprising at least one phosphorous atom in oxidation state +5, and (B) heating the mixture obtained in step (A) at a temperature of 100 to 500 °C and at an autogeneous pressure to reduce Q to oxidation state +2 and to obtain a compound of general formula (I).

    PRODUCING OXIDIC COMPOUNDS
    10.
    发明专利

    公开(公告)号:CA2787373C

    公开(公告)日:2018-03-06

    申请号:CA2787373

    申请日:2011-01-28

    Applicant: BASF SE

    Abstract: A process for producing oxidic compounds of the general formula (?) LizMxOy (?) wherein M is one or more elements from groups 2 to 12 of the periodic table, more particularly selected from Co, Mn, Ni, Fe, Al, Mg, x is 1 to 2, y is 2 to 4, and z is 0.5 to 1.5, comprises heating mixtures selected from oxides, hydroxides, carbonates and nitrates of Li and of M together to temperatures in the range from 600 to 1200? in a reaction vessel performing incomplete rotary motions about one axis.