Abstract:
The present invention is directed towards a process for making a lithiated transition metal oxide, said process comprising the following steps: (a) providing a precursor selected from mixed oxides, hydroxides, oxyhydroxides, and carbonates of nickel and at least one transition metal selected from manganese and cobalt, wherein at least 45 mole-% of the cations of the precursor are Ni cations, (b) mixing said precursor with at least one lithium salt selected from LiOH, Li2O, Li2CO3, and LiNO3, thereby obtaining a mixture, (c) adding at least one phosphorus compound of general formula (I) XyH3-yPO4 (I) wherein X is selected from NH4 and Li, y is 1 or 2, to the mixture obtained in step (b), wherein steps (b) and (c) may be performed consecutively or simultaneously, treating the mixture so obtained at a temperature in the range of from 650 to 950°C.
Abstract translation:本发明涉及一种制备锂化过渡金属氧化物的方法,所述方法包括以下步骤:(a)提供一种选自镍的混合氧化物,氢氧化物,羟基氧化物和碳酸盐的前体和至少一种选自以下的过渡金属: 锰和钴,其中前体的至少45摩尔%的阳离子是Ni阳离子,(b)将所述前体与至少一种选自LiOH,Li 2 O,Li 2 CO 3和LiNO 3的锂盐混合,从而得到混合物( c)向步骤(b)中获得的混合物中加入至少一种其中X选自NH 4和Li,y为1或2的通式(I)XyH 3-y PO 4(I)的磷化合物,其中步骤(b) 和(c)可以连续或同时进行,在650-950℃的温度范围内处理如此获得的混合物。
Abstract:
La invención se refiere a un método para producir óxidos metálicos mixtos de litio que contienen esencialmente litio, manganeso, cobalto y níquel como átomos metálicos y tienen una relación estequiométrica de litio con respecto a la colectividad de los metales de transición mayor que 1, que comprende a) la producción de una mezcla denominada producto intermedio (B), que comprende esencialmente hidróxidos metálicos mixtos que contienen litio e hidróxidos de óxidos metálicos mixtos que contienen litio, en la que el manganeso, el cobalto y el níquel están contenidos en la relación (1-ab):a:b y en la que el número de oxidación, promediado sobre todos los iones de manganeso, cobalto y níquel, es al menos 4-1,75a-1,75b, donde 0