LOW TEMPERATURE CHEMICAL STRENGTHENING PROCESS FOR GLASS
    2.
    发明申请
    LOW TEMPERATURE CHEMICAL STRENGTHENING PROCESS FOR GLASS 审中-公开
    玻璃纤维低温化学强化工艺

    公开(公告)号:WO2016137916A2

    公开(公告)日:2016-09-01

    申请号:PCT/US2016019017

    申请日:2016-02-23

    Applicant: CORNING INC

    CPC classification number: C03C21/002 C03C21/001 C03C21/005

    Abstract: A method of chemically strengthening a glass. The method includes heating an ion exchange solution to a temperature less than about 360 C, and contacting the glass and the strengthening solution at the temperature for a duration from about 0.5 hours to about 24 hours. The ion exchange solution includes a primary nitrate and at least one monovalent or divalent cation nitrate component in an amount from about 1 wt.% to about 10 wt.%.

    Abstract translation: 化学强化玻璃的方法。 该方法包括将离子交换溶液加热至低于约360℃的温度,并使玻璃和强化溶液在该温度下接触约0.5小时至约24小时。 离子交换溶液包含约1重量%至约10重量%的伯硝酸盐和至少一种一价或二价阳离子硝酸盐组分。

    CROSSLINKED STARCHES FOR PORE FORMING IN CERAMICS
    3.
    发明申请
    CROSSLINKED STARCHES FOR PORE FORMING IN CERAMICS 审中-公开
    在陶瓷中形成孔的交联淀粉

    公开(公告)号:WO2015057805A3

    公开(公告)日:2015-07-30

    申请号:PCT/US2014060641

    申请日:2014-10-15

    Applicant: CORNING INC

    Abstract: Disclosed herein are green bodies comprising at least one ceramic-forming powder; at least one binder; and at least one cross-linked starch present in an amount of at least about 20% by weight as a super addition. Further disclosed herein is a method of making a porous ceramic body comprising mixing at least one ceramic-forming powder, at least one solvent such as water, at least one binder, and at least one cross-linked starch present in an amount of about 20% by weight as a super addition to form a batch composition; extruding the batch composition to form a green body; drying the green body; and firing the green body to form a porous ceramic body. Also disclosed herein are methods of screening a green body for making a porous ceramic body.

    Abstract translation: 本文公开了包含至少一种陶瓷形成粉末的生坯; 至少一个粘合剂; 和至少一种交联淀粉以至少约20重量%的量作为超添加剂存在。 本文进一步公开的是制备多孔陶瓷体的方法,该方法包括将至少一种陶瓷形成粉末,至少一种溶剂如水,至少一种粘合剂和至少一种交联淀粉混合,所述交联淀粉的存在量为约20 重量%作为超级添加以形成批料组合物; 挤出批料组合物以形成生坯; 干燥绿色的身体; 并焙烧生坯以形成多孔陶瓷体。 本文还公开了筛选生坯以制造多孔陶瓷体的方法。