A glass article having a glass bump formed integrally thereon by laser-irradiation methods. The glass bump includes a lower region connected to an upper region by an inflection region. The lower region projects from a surface of the glass article and is defined by concavely rounded sides with a radius of curvature R1. The upper region includes a transition portion and a top portion. The transition portion is defined by convexly rounded sides with a radius of curvature R2. The transition portion connects to the lower portion via the inflection region. The upper portion connects to the transition portion and is defined by a convexly rounded top surface with a radius of curvature R3, which is greater than radius of curvature R2.
Abstract:
Se provee un procedimiento para convertir datos del color en una o más notas musicales; el procedimiento implica leer, usando un dispositivo de lectura del color, los colores respectivos aplicados a un lienzo por una pluralidad de instrumentos de dibujo como datos del color, en donde cada uno de la pluralidad de instrumentos de dibujo está configurado para introducir los colores respectivos de una paleta de colores, y en donde los colores respectivos de la paleta de colores corresponden respectivamente a una serie de notas musicales; el procedimiento implica también procesar, usando un módulo de procesamiento del color, los datos del color para generar una composición de las una o más notas musicales de los datos del color con base en una serie de notas musicales que corresponden a los colores respectivos en los datos del color.
Abstract:
A method of forming a strengthened glass article is provided. The method includes providing a strengthened glass article. The strengthened glass article is in the form of a container including a sidewall having an exterior surface and an interior surface that encloses an interior volume. The sidewall has an exterior strengthened surface layer that includes the exterior surface, an interior strengthened surface layer that includes the interior surface and a central layer between the exterior strengthened surface layer and the interior strengthened surface layer that is under a tensile stress. A laser-induced intended line of separation is formed in the central layer at a predetermined depth between the exterior strengthened surface layer and the interior strengthened surface layer by irradiating the sidewall with a laser without separating the glass article.
Abstract:
A glass container including a body having a delamination factor less than or equal to 10 and at least one marking is described. The body has an inner surface, an outer surface, and a wall thickness extending between the outer surface and the inner surface. The marking is located within the wall thickness. In particular, the marking is a portion of the body having a refractive index that differs from a refractive index of an unmarked portion of the body. Methods of forming the marking within the body are also described.
Abstract:
Methods of forming a glass article are disclosed. In one embodiment, a method of forming a glass article includes translating a pulsed laser beam on a glass substrate sheet to form a laser damage region between a first surface and a second surface of the glass substrate sheet. The method further includes applying an etchant solution to the glass substrate sheet to remove a portion of the glass substrate sheet about the laser damage region. The method may further include strengthening the glass substrate sheet by an ion-exchange strengthening process, and coating the glass substrate sheet with an acid-resistant coating. Also disclosed are methods where the laser damage region has an initial geometry that changes to a desired geometry following the reforming of the glass substrate sheet such that the initial geometry of the laser damage region compensates for the bending of the glass substrate sheet.
Abstract:
A method of fabricating a high-density array of holes in glass is provided, comprising providing a glass piece having a front surface, then irradiating the front surface of the glass piece with a UV laser beam focused to a focal point within +/- 100 µm of the front surface of the glass piece most desirably within +/- 50 µm of the front surface. The lens focusing the laser has a numerical aperture desirably in the range of from 0.1 to 0.4, more desirably in the range of from 0.1 to 0.15 for glass thickness between 0.3 mm and 0.63 mm, even more desirably in the range of from 0.12 to 0.13, so as to produce open holes extending into the glass piece 100 from the front surface 102 of the glass piece, the holes having an diameter the in range of from 5 to 15 µm, and an aspect ratio of at least 20:1. For thinner glass, in the range of from 0.1 - 0.3 mm, the numerical aperture is desirably from 0.25 to 0.4, more desirably from 0.25 to 0.3, and the beam is preferably focused to within +/- 30 µm of the front surface of the glass. The laser is desirable operated at a repetition rate of about 15 kHz or below. An array of holes thus produced may then be enlarged by etching. The front surface may be polished prior to etching, if desired.
Abstract:
A method for controlling formation of glass bumps in a glass article with laser-irradiation without the use of a growth-limiting structure. Standard deviation of height between the glass bumps on the article is less than 1 micron by controlling the laser radiation dose provided on the glass article.
Abstract:
Disclosed herein are transparent articles and methods and systems for processing transparent articles. Systems for processing transparent articles, e.g. cutting glass, may include at least one initial laser and at least one polarizing beam splitter, where the polarizing beam splitter is configured to split an initial laser beam into a plurality of laser beams, and wherein the plurality of laser beams are useful for processing transparent articles. Methods for processing transparent articles comprise creating at least one flaw in the transparent articles with a plurality of laser beams.