公开(公告)号:JP2000033267A
公开(公告)日:2000-02-02
申请号:JP19066999
申请日:1999-07-05
Applicant: DEGUSSA
Inventor: VAN DEN TILLAART HANS DR , LEYRER JUERGEN DR , STREHLAU WOLFGANG DR , LOX EGBERT DR , KREUZER THOMAS DR , PLOG CARSTEN DR , ANDORF RENATO DR , MARKERT NORBERT , STENGEL THOMAS
IPC: B01D53/94 , B01J23/46 , B01J29/068 , B01J29/44
Abstract: PROBLEM TO BE SOLVED: To reduce nitrogen oxides by making iridium be contained on a carrier material comprising silicon dioxide or zeolite and the iridium exist on the outer surface of the carrier material in an average particle size within a specified range. SOLUTION: A catalyst is constituted by incorporating iridium on a carrier material comprising zeolite of the formula M2/nO.Al2O3.xSiO2.yH2O (wherein M is an n-valent cation; (x) is a modulus), which is silicon dioxide 10-30 nm in a particle size or an oxidized silicon/aluminum compound having a special crystal structure, and making iridium 5-30 nm in an average particle size exist on the outer surface face of the carrier material. The catalyst is used in the shape of a coating applied on the wall surface of the passage of a ceramic or metal honeycomb structure. In this way, nitrogen oxides can be reduced in an oxidative and reductive atmosphere.
-
公开(公告)号:BR9903053A
公开(公告)日:2000-05-09
申请号:BR9903053
申请日:1999-07-02
Applicant: DEGUSSA
Inventor: TILLAART HANS VAN DEN , LEYRER JUERGEN , STREHLAU WOLFGANG , LOX EGBERT , KREUZER THOMAS , PLOG CARSTEN , ANDORF RENATO , MARKERT NORBERT , STENGEL THOMAS
IPC: B01D53/94 , B01J23/46 , B01J29/068 , B01J29/44 , B01J103/76
Abstract: The catalyst for reducing nitrogen oxides in an oxidizing and reducing atmosphere contains iridium on a support material made of silicon dioxide or zeolite. The iridium on the outer surface has an average particle size of 5-30 nm. An Independent claim is also included for the production of the catalyst comprising impregnating the support material with a soluble precursor of iridium, drying the impregnated material and calcining in a gas stream containing hydrogen at 300-500 degrees C for 1-10 hours.
-
公开(公告)号:TR9901534A2
公开(公告)日:2000-02-21
申请号:TR9901534
申请日:1999-07-01
Applicant: DEGUSSA
Inventor: TILLAART DR HANS VAN DEN , LEYRER DR JURGEN , STREHLAU DR WOLFGANG , LOX DR EGBERT , KREUZER DR THOMAS , PLOG DR CARSTEN , ANDORF DR RENATO , MARKERT NORBERT , STENGEL THOMAS
CPC classification number: B01D53/9418 , B01D2255/1028 , B01D2255/504 , B01J23/468 , B01J35/006 , Y02T10/24
-
公开(公告)号:DE19930494A1
公开(公告)日:2000-02-03
申请号:DE19930494
申请日:1999-07-01
Applicant: DEGUSSA , DAIMLER CHRYSLER AG
Inventor: TILLAART HANS VAN DEN , LEYRER JUERGEN , STREHLAU WOLFGANG , LOX EGBERT , KREUZER THOMAS , PLOG CARSTEN , ANDORF RENATO , MARKERT NORBERT , STENGEL THOMAS
IPC: B01D53/94 , B01J23/46 , B01J29/068 , B01J29/44 , F01N3/20
Abstract: The catalyst for reducing nitrogen oxides in an oxidizing and reducing atmosphere contains iridium on a support material made of silicon dioxide or zeolite. The iridium on the outer surface has an average particle size of 5-30 nm. An Independent claim is also included for the production of the catalyst comprising impregnating the support material with a soluble precursor of iridium, drying the impregnated material and calcining in a gas stream containing hydrogen at 300-500 deg C for 1-10 hours.
-
公开(公告)号:ZA9904298B
公开(公告)日:2000-01-10
申请号:ZA9904298
申请日:1999-06-30
Applicant: DEGUSSA
Inventor: TILLAART HANS VAN DEN , LEYRER JUERGEN , STREHLAU WOLFGANG , LOX EGBERT , KREUZER THOMAS , PLOG CARSTEN , ANDORF RENATO , MARKERT NORBERT , STENGEL THOMAS
CPC classification number: B01D53/9418 , B01D2255/1028 , B01D2255/504 , B01J23/468 , B01J35/006 , Y02T10/24
-
公开(公告)号:TR199901534A2
公开(公告)日:2000-02-21
申请号:TR9901534
申请日:1999-07-01
Applicant: DEGUSSA
Inventor: TILLAART DR HANS VAN DEN , LEYRER DR JURGEN , STREHLAU DR WOLFGANG , LOX DR EGBERT , KREUZER DR THOMAS , PLOG DR CARSTEN , ANDORF DR RENATO , MARKERT NORBERT , STENGEL THOMAS
Abstract: The catalyst for reducing nitrogen oxides in an oxidizing and reducing atmosphere contains iridium on a support material made of silicon dioxide or zeolite. The iridium on the outer surface has an average particle size of 5-30 nm. An Independent claim is also included for the production of the catalyst comprising impregnating the support material with a soluble precursor of iridium, drying the impregnated material and calcining in a gas stream containing hydrogen at 300-500 degrees C for 1-10 hours.
-
公开(公告)号:AU3795799A
公开(公告)日:2000-01-20
申请号:AU3795799
申请日:1999-07-02
Applicant: DEGUSSA
Inventor: TILLAART HANS VAN DEN , STENGEL THOMAS , MARKERT NORBERT , ANDORF RENATO , PLOG CARSTEN , KREUZER THOMAS , LOX EGBERT , STREHLAU WOLFGANG , LEYRER JURGEN
Abstract: The catalyst for reducing nitrogen oxides in an oxidizing and reducing atmosphere contains iridium on a support material made of silicon dioxide or zeolite. The iridium on the outer surface has an average particle size of 5-30 nm. An Independent claim is also included for the production of the catalyst comprising impregnating the support material with a soluble precursor of iridium, drying the impregnated material and calcining in a gas stream containing hydrogen at 300-500 degrees C for 1-10 hours.
-
公开(公告)号:CZ9902405A3
公开(公告)日:2000-04-12
申请号:CZ240599
申请日:1999-07-02
Applicant: DEGUSSA
-
公开(公告)号:CZ240599A3
公开(公告)日:2000-04-12
申请号:CZ240599
申请日:1999-07-02
Applicant: DEGUSSA
-
公开(公告)号:ZA994298B
公开(公告)日:2000-01-10
申请号:ZA994298
申请日:1999-06-30
Applicant: DEGUSSA
Inventor: TILLAART HANS VAN DEN , LEYRER JUERGEN , STREHLAU WOLFGANG , LOX EGBERT , KREUZER THOMAS , PLOG CARSTEN , ANDORF RENATO , MARKERT NORBERT , STENGEL THOMAS
Abstract: The catalyst for reducing nitrogen oxides in an oxidizing and reducing atmosphere contains iridium on a support material made of silicon dioxide or zeolite. The iridium on the outer surface has an average particle size of 5-30 nm. An Independent claim is also included for the production of the catalyst comprising impregnating the support material with a soluble precursor of iridium, drying the impregnated material and calcining in a gas stream containing hydrogen at 300-500 degrees C for 1-10 hours.
-
-
-
-
-
-
-
-
-