HARDENER INDICATING USABLE PERIOD FOR EPOXY RESIN SYSTEM DILUTED BY WATER

    公开(公告)号:JPH1081732A

    公开(公告)日:1998-03-31

    申请号:JP20010497

    申请日:1997-07-25

    Applicant: HOECHST AG

    Abstract: PROBLEM TO BE SOLVED: To obtain a water-dispersing hardener for an epoxy resin, manifesting a good emulsifying activities with the liquid epoxy resin, excellent in compatibility with a solid resin disperse substance and obviously increasing the viscosity at the end of the processing time when the hardener is combined with the epoxy resin. SOLUTION: This curing agent is obtained by reacting (A) a mixture of two or more aliphatic polyols having 200-20,000g/mol weight average molecular weight MW of the mixture and including at least one kind of the polyols having >=4,000g/mol weight average molecular weight MW with (B) at least one kind of epoxy compound having at least two epoxy groups in a molecule and 500-10,000mmol/kg specific content of the epoxy group (100-2,000g/mol epoxy equivalent) at the first reaction stage to provide epoxide-polyol adduct, and further reacting the epoxy-polyol adduct with (C) polyamines having at least three aminic hydrogen atoms and at least one primary amino group per molecule.

    2.
    发明专利
    未知

    公开(公告)号:DE19515967A1

    公开(公告)日:1996-11-07

    申请号:DE19515967

    申请日:1995-05-02

    Applicant: HOECHST AG

    Abstract: The prodn. of water-dilutable polyvinyl butyral (PVB) dispersions (I) comprises reacting (A) aliphatic acid(s) contg. 1-3 isocyanate-reactive gps. and 1-3 acid gps. with (B) polyisocyanates with an average functionality of at least 2, in an amt. such that the ratio of NCO gps. in (B) to NCO-reactive gps. in (A) = (2.2:1)-(1.7:1), until the content of residual NCO gps. reaches the calcd. value, then reacting 25-75% of the remaining NCO gps. with (C) mono-alcohol(s) and/or mono-amine(s), until the calculated NCO gp. content is obtd., and reacting the NCO- functional emulsifier resin thus obtd. with (D) a mixt. of (D1) 30-100 wt% PVB and (D2) 0-70 wt% suitable plasticiser resin(s) in the presence of suitable solvents, until all the NCO gps. are completely reacted, to give a prod. contg. acid gps. in an amt. such that the solid resin has an acid no. of 5-50 mg/g. Also claimed are: (i) aq. PVB dispersions (I) obtd. by this process, and aq. PVB dispersions contg. 0.5-20 wt% organic solvent; (ii) mixts. of aq. binders contg. (I), pref. together with aq. dispersions of phenolic resins or amino resins.

Patent Agency Ranking