公开(公告)号:NO934657A
公开(公告)日:1994-06-20
申请号:NO934657
申请日:1993-12-16
Applicant: HOECHST AG
Inventor: HIMMRICH JOHANNES , SCHIMMEL GUNTHER , POLLMANN KLAUS
CPC classification number: C09K3/185
-
公开(公告)号:CA2110422A1
公开(公告)日:1994-06-18
申请号:CA2110422
申请日:1993-12-01
Applicant: HOECHST AG
Inventor: HIMMRICH JOHANNES , SCHIMMEL GUENTHER , POELLMANN KLAUS
Abstract: Alkaline earth metal sodium acetate, a process for its preparation and its use The alkaline earth metal sodium acetate according to the invention comprises 18 to 22 % by weight of calcium (Ca++), 0 to 1 % by weight of magnesium (Mg++), 4 to 7 % by weight of sodium (Na+), 66 to 75 % by weight of acetate (CH3COO-), 0 to 7 % by weight of water and 0 to 2 % by weight of water-insoluble components For its preparation, a calcium oxide containing at least 85% of CaO, acetic acid and sodium hydroxide solution are reacted with one another and the reaction product is granulated to give particles of 0.5 to 5 mm. The alkaline earth metal sodium acetate according to the invention can be used as an environment-friendly deicing agent causing little corrosion.
-
公开(公告)号:CA2110317A1
公开(公告)日:1994-06-18
申请号:CA2110317
申请日:1993-11-30
Applicant: HOECHST AG
Inventor: HIMMRICH JOHANNES , SCHIMMEL GUENTHER , POELLMANN KLAUS
Abstract: Alkaline earth metal potassium acetate, a process for its preparation and its use The alkaline earth metal potassium acetate according to the invention comprises 14 to 19 % by weight of calcium (Ca++), 0 to 1 % by weight of magnesium (Mg++), 11 to 16 % by weight of potassium (K+), 62 to 71 % by weight of acetate (CH3COO-), 0 to 7 % by weight of water and 0 to 2 % by weight of water-insoluble components For its preparation, a calcium oxide containing at least 85% of CaO, acetic acid and potassium hydroxide solution are reacted with one another and the reaction product is granulated to give particles of 0.5 to 5 mm. The alkaline earth metal potassium acetate according to the invention can be used as an environment-friendly deicing agent causing little corrosion.
-
公开(公告)号:FI935636A
公开(公告)日:1994-06-18
申请号:FI935636
申请日:1993-12-15
Applicant: HOECHST AG
Inventor: HIMMRICH JOHANNES , SCHIMMEL GUENTHER , POELLMANN KLAUS
Abstract: The alkaline earth metal/sodium acetate according to the invention comprises from 18 to 22 % by weight of calcium (Ca ), from 0 to 1 % by weight of magnesium (Mg ), from 4 to 7 % by weight of sodium (Na ), from 66 to 75 % by weight of acetate (CH3COO ), from 0 to 7 % by weight of water, and from 0 to 2 % by weight of water-insoluble components. It is prepared by reacting a calcium oxide containing at least 85 % of CaO with acetic acid and sodium hydroxide solution and granulating the reaction product to give particles of from 0.5 to 5 mm. The alkaline earth metal/sodium acetate according to the invention can be used as an environmentally friendly and low-corrosion deicing agent.
-
公开(公告)号:FI935635A
公开(公告)日:1994-06-18
申请号:FI935635
申请日:1993-12-15
Applicant: HOECHST AG
Inventor: HIMMRICH JOHANNES , SCHIMMEL GUENTHER , POELLMANN KLAUS
Abstract: The alkaline earth metal/potassium acetate according to the invention comprises from 14 to 19 % by weight of calcium (Ca ), from 0 to 1 % by weight of magnesium (Mg ), from 11 to 16 % by weight of potassium (K ), from 62 to 71 % by weight of acetate (CH3COO ), from 0 to 7 % by weight of water, and from 0 to 2 % by weight of water-insoluble components. It is prepared by reacting a calcium oxide containing at least 85 % of CaO with acetic acid and potassium hydroxide solution and granulating the reaction product to give particles of from 0.5 to 5 mm. The alkaline earth metal/potassium acetate according to the invention can be used as an environmentally friendly and low-corrosion deicing agent.
-
公开(公告)号:NO934657D0
公开(公告)日:1993-12-16
申请号:NO934657
申请日:1993-12-16
Applicant: HOECHST AG
Inventor: HIMMRICH JOHANNES , SCHIMMEL GUENTHER , POELLMANN KLAUS
Abstract: The alkaline earth metal/sodium acetate according to the invention comprises from 18 to 22 % by weight of calcium (Ca ), from 0 to 1 % by weight of magnesium (Mg ), from 4 to 7 % by weight of sodium (Na ), from 66 to 75 % by weight of acetate (CH3COO ), from 0 to 7 % by weight of water, and from 0 to 2 % by weight of water-insoluble components. It is prepared by reacting a calcium oxide containing at least 85 % of CaO with acetic acid and sodium hydroxide solution and granulating the reaction product to give particles of from 0.5 to 5 mm. The alkaline earth metal/sodium acetate according to the invention can be used as an environmentally friendly and low-corrosion deicing agent.
-
公开(公告)号:CA2084854A1
公开(公告)日:1993-06-15
申请号:CA2084854
申请日:1992-12-08
Applicant: HOECHST AG
Inventor: BETTERMANN GERHARD , SCHIMMEL GUENTHER , HIMMRICH JOHANNES
Abstract: HOE 91/H 030 Process for the preparation of alkali metal acetates To prepare a corrosion-inhibitlng liquid de-icing agent based on alkali metal acetates, 30 to 50 percent strength by weight alkali metal hydroxide solution is introduced into a reaction container provided with a cooling device and a mixing device, and 85 to 100% strength acetic acid is metered into the reaction container until the ratio by weight of acetic acid to alkali metal hydroxide solution therein (0.30 to 0.45) : 1. A portion of this solution is transferred from the reaction container to a stirred dissolving tank and 0.03 to 1% by weight, relative to the batch, of benzotriazole and/or tolyltriazole and/or imidazole is dissolved therein. The resulting solution containing azole is introduced into the reaction container along with 0.01 to 0.2% by weight of phosphoric acid, relative to the batch. Acetic acid continues to be metered into the reaction container until the density of the solution in the reaction container is 1.07 to 1.39 g/cm3 at 20.degree.C. Small amounts of alkali metal hydroxide solution or acetic acid are then introduced into the reaction container until the pH of the solution therein is 9.2 to 9.8. Finally, this solution is withdrawn from the reaction container as a liquid de-icing agent.
-
公开(公告)号:NO301649B1
公开(公告)日:1997-11-24
申请号:NO934656
申请日:1993-12-16
Applicant: HOECHST AG
Inventor: HIMMRICH JOHANNES , SCHIMMEL GUENTHER , POELLMANN KLAUS
Abstract: The alkaline earth metal/potassium acetate according to the invention comprises from 14 to 19 % by weight of calcium (Ca ), from 0 to 1 % by weight of magnesium (Mg ), from 11 to 16 % by weight of potassium (K ), from 62 to 71 % by weight of acetate (CH3COO ), from 0 to 7 % by weight of water, and from 0 to 2 % by weight of water-insoluble components. It is prepared by reacting a calcium oxide containing at least 85 % of CaO with acetic acid and potassium hydroxide solution and granulating the reaction product to give particles of from 0.5 to 5 mm. The alkaline earth metal/potassium acetate according to the invention can be used as an environmentally friendly and low-corrosion deicing agent.
-
9.
公开(公告)号:HUT66799A
公开(公告)日:1994-12-28
申请号:HU9303644
申请日:1993-12-17
Applicant: HOECHST AG
Inventor: POELLMANN KLAUS , SCHIMMEL GUENTHER , HIMMRICH JOHANNES
Abstract: The alkaline earth metal/potassium acetate according to the invention comprises from 14 to 19 % by weight of calcium (Ca ), from 0 to 1 % by weight of magnesium (Mg ), from 11 to 16 % by weight of potassium (K ), from 62 to 71 % by weight of acetate (CH3COO ), from 0 to 7 % by weight of water, and from 0 to 2 % by weight of water-insoluble components. It is prepared by reacting a calcium oxide containing at least 85 % of CaO with acetic acid and potassium hydroxide solution and granulating the reaction product to give particles of from 0.5 to 5 mm. The alkaline earth metal/potassium acetate according to the invention can be used as an environmentally friendly and low-corrosion deicing agent.
-