公开(公告)号:JPS60219253A
公开(公告)日:1985-11-01
申请号:JP6103885
申请日:1985-03-27
Applicant: HOECHST AG
Inventor: BURG KARLHEINZ , CHERDRON HARALD , KLOOS FRIEDRICH , SCHLAF HELMUT
-
公开(公告)号:JPH0657097A
公开(公告)日:1994-03-01
申请号:JP13794893
申请日:1993-06-08
Applicant: HOECHST AG
Inventor: BURG KARLHEINZ , CHERDRON HARALD , KLOOS FRIEDRICH , SCHLAF HELMUT
-
公开(公告)号:AU679009B2
公开(公告)日:1997-06-19
申请号:AU5203693
申请日:1993-11-30
Applicant: HOECHST AG
Inventor: WINTER ANDREAS , VOLLMAR ANNETTE , KLOOS FRIEDRICH , BACHMANN BERND
IPC: C08F10/00 , C08F8/00 , C08F10/06 , C08F110/06 , C08F210/04 , C08F210/06 , C08F210/16 , C08L23/00 , C08L23/02 , C08L23/10 , C08L23/14 , D01D5/08 , D01F6/00 , D01F6/06 , D01F6/46 , C08L23/12 , C08L23/06 , C08L23/16 , D01F6/30
Abstract: A polyolefin moulding composition essentially comprising a polyolefin which comprises an olefin having at least 3 carbon atoms, of the formula R -CH=CH-R , in which R and R are identical or different and are hydrogen or straight-chain or branched C1-C15-alkyl, or R and R , together with the atoms connecting them, form a ring system, and from 0 to 10% by weight of ethylene or a second olefin as defined above as comonomer, characterised in that the MFI (230/2.16) is from 5 to 1000 g/10 min, the MFI (230/5) is from 15 to 3000 g/10 min, the molecular weight Mw is from 75,000 to 350,000 g/mol, the polydispersity Mw/Mn is from 1.8 to 3.5, the viscosity index is from 70 to 300 cm /g, the melting point is from 120 to 165@C and the isotactic block length is from 25 to 150, and an ether-extractable content of less than 2% by weight, based on the total weight of the polymer.
-
公开(公告)号:FI935359A
公开(公告)日:1994-06-03
申请号:FI935359
申请日:1993-11-30
Applicant: HOECHST AG
Inventor: WINTER ANDREAS , VOLLMAR ANNETTE , KLOOS FRIEDRICH , BACHMANN BERND
IPC: C08F10/00 , C08F8/00 , C08F10/06 , C08F110/06 , C08F210/04 , C08F210/06 , C08F210/16 , C08L23/00 , C08L23/02 , C08L23/10 , C08L23/14 , D01D5/08 , D01F6/00 , D01F6/06 , D01F6/46 , D01F6/04
Abstract: A polyolefin moulding composition essentially comprising a polyolefin which comprises an olefin having at least 3 carbon atoms, of the formula R -CH=CH-R , in which R and R are identical or different and are hydrogen or straight-chain or branched C1-C15-alkyl, or R and R , together with the atoms connecting them, form a ring system, and from 0 to 10% by weight of ethylene or a second olefin as defined above as comonomer, characterised in that the MFI (230/2.16) is from 5 to 1000 g/10 min, the MFI (230/5) is from 15 to 3000 g/10 min, the molecular weight Mw is from 75,000 to 350,000 g/mol, the polydispersity Mw/Mn is from 1.8 to 3.5, the viscosity index is from 70 to 300 cm /g, the melting point is from 120 to 165@C and the isotactic block length is from 25 to 150, and an ether-extractable content of less than 2% by weight, based on the total weight of the polymer.
-
公开(公告)号:CA2110441A1
公开(公告)日:1994-06-03
申请号:CA2110441
申请日:1993-12-01
Applicant: HOECHST AG
Inventor: WINTER ANDREAS , VOLLMAR ANNETTE , KLOOS FRIEDRICH , BACHMANN BERND
IPC: C08F10/00 , C08F8/00 , C08F10/06 , C08F110/06 , C08F210/04 , C08F210/06 , C08F210/16 , C08L23/00 , C08L23/02 , C08L23/10 , C08L23/14 , D01D5/08 , D01F6/00 , D01F6/06 , D01F6/46
Abstract: : Polyolefin molding composition for producing fibers, filaments and webs by melt spinning Polyolefin molding composition consisting essentially of a polyolefin formed from an olefin having at least 3 carbon atoms of the formula Ra-CH = CH-Rb, where Ra and Rb are identical or different and each is hydrogen or C1-C15-alkyl, straight-chain or branched, or Ra and Rb together with the atoms joining them together form a ring system, and from 0 to 10% by weight of ethylene or of a second olefin have the abovementioned meaning as comonomer, characterized by a 230/2.16 MFI from 5 to 1000 g/10 min, a 230/5 MFI from 15 to 3000 g/10 min, a molecular weight (Mw) from 75,000 to 350,000 g/mol, a polydispersity (Mw/Mn) from 1.8 to 3.5, a viscosity number from 70 to 300 cm3/g, a melting point from 120 to 165.degree.C, an isotactic block length from 25 to 150, and ether extractables less than 2% by weight, based on the total weight of the polymer.
-
公开(公告)号:FI935359A0
公开(公告)日:1993-11-30
申请号:FI935359
申请日:1993-11-30
Applicant: HOECHST AG
Inventor: WINTER ANDREAS , VOLLMAR ANNETTE , KLOOS FRIEDRICH , BACHMANN BERND
IPC: C08F10/00 , C08F8/00 , C08F10/06 , C08F110/06 , C08F210/04 , C08F210/06 , C08F210/16 , C08L23/00 , C08L23/02 , C08L23/10 , C08L23/14 , D01D5/08 , D01F6/00 , D01F6/06 , D01F6/46 , C08L , D01F
Abstract: A polyolefin moulding composition essentially comprising a polyolefin which comprises an olefin having at least 3 carbon atoms, of the formula R -CH=CH-R , in which R and R are identical or different and are hydrogen or straight-chain or branched C1-C15-alkyl, or R and R , together with the atoms connecting them, form a ring system, and from 0 to 10% by weight of ethylene or a second olefin as defined above as comonomer, characterised in that the MFI (230/2.16) is from 5 to 1000 g/10 min, the MFI (230/5) is from 15 to 3000 g/10 min, the molecular weight Mw is from 75,000 to 350,000 g/mol, the polydispersity Mw/Mn is from 1.8 to 3.5, the viscosity index is from 70 to 300 cm /g, the melting point is from 120 to 165@C and the isotactic block length is from 25 to 150, and an ether-extractable content of less than 2% by weight, based on the total weight of the polymer.
-
公开(公告)号:DE3582442D1
公开(公告)日:1991-05-16
申请号:DE3582442
申请日:1985-03-19
Applicant: HOECHST AG
Inventor: BURG KARLHEINZ , CHERDRON HARALD , KLOOS FRIEDRICH , SCHLAF HELMUT
IPC: C08L51/04 , C08F279/02 , C08L7/00 , C08L21/00 , C08L23/00 , C08L33/00 , C08L33/02 , C08L35/02 , C08L51/00 , C08L51/02 , C08L51/06 , C08L51/08 , C08L59/00 , C08L59/02 , C08L67/00 , C08L67/02 , C08L75/04 , C08L77/00 , C08L101/00
Abstract: A mixture essentially comprising polyoxymethylene (component A), a rubber-elastic graft copolymer whose particles are built from a rubber-elastic, single-phase core based on polydiene and a hard graft shell (component B), and, if desired, a third polymeric component (component C), and a three-component mixture comprising components A, B' and C, where, in the case of B', the core comprises predominantly or fully poly(meth)acrylic acid esters or silicone rubber instead of polydiene. The mouldings produced from these mixtures have, in particular, good low-temperature impact strength.
-
公开(公告)号:AU603422B2
公开(公告)日:1990-11-15
申请号:AU1148588
申请日:1988-02-10
Applicant: HOECHST AG
Inventor: HELBERG JURGEN , HEUFER GERT , KLOOS FRIEDRICH , LOW WOLFGANG
-
公开(公告)号:DK67988A
公开(公告)日:1988-08-12
申请号:DK67988
申请日:1988-02-10
Applicant: HOECHST AG
Inventor: HELBERG JUERGEN , HEUFER GERT , KLOOS FRIEDRICH , LOEW WOLFGANG
-
公开(公告)号:DK67988D0
公开(公告)日:1988-02-10
申请号:DK67988
申请日:1988-02-10
Applicant: HOECHST AG
Inventor: HELBERG JUERGEN , HEUFER GERT , KLOOS FRIEDRICH , LOEW WOLFGANG
-
-
-
-
-
-
-
-
-