公开(公告)号:NO884136A
公开(公告)日:1989-03-20
申请号:NO884136
申请日:1988-09-16
Applicant: HOECHST AG
Inventor: WINGEN RAINER , DUEBAL HANS-ROLF , ESCHER CLAUS , HEMMERLING WOLFGANG , MUELLER INGRID , OHLENDOF DIETER
IPC: C07D239/26 , C07D239/34 , C09K19/34 , C09K19/46 , G02F1/137 , G02F1/141 , G02F1/13 , G09F9/35
CPC classification number: C07D239/26 , C07D239/34 , C09K19/3458
-
公开(公告)号:NO884136D0
公开(公告)日:1988-09-16
申请号:NO884136
申请日:1988-09-16
Applicant: HOECHST AG
Inventor: WINGEN RAINER , DUBAL HANS-ROLF , ESCHER CLAUS , HEMMERLING WOLFGANG , MULLER INGRID , OHLENDOF DIETER
IPC: C07D239/26 , C07D239/34 , C09K19/34 , C09K19/46 , G02F1/137 , G02F1/141 , C07D239/00 , G02F1/13
Abstract: Phenylpyrimidinyl trans-cyclohexanecarboxylates of the formula … … form, in addition to a relatively broad nematic phase, a smectic C phase if R denotes an alkyl radical having 10 to 16 carbon atoms, in particular 11 to 16 carbon atoms, or an alkyloxy radical having 8 to 14 carbon atoms and R denotes an alkyl radical having 2 to 9 carbon atoms. Accordingly, they are suitable in particular as components of liquid-crystalline mixtures having a smectic C phase, since they induce a relatively broad nematic phase or widen a narrow nematic phase present and enlarge the temperature range of the smectic C phase towards low, but in particular towards high temperatures.
-
公开(公告)号:NO176276B
公开(公告)日:1994-11-28
申请号:NO884136
申请日:1988-09-16
Applicant: HOECHST AG
Inventor: WINGEN RAINER , DUBAL HANS-ROLF , ESCHER CLAUS , HEMMERLING WOLFGANG , MULLER INGRID , OHLENDOF DIETER
IPC: C07D239/26 , C07D239/34 , C09K19/34 , C09K19/46 , G02F1/137 , G02F1/141 , G02F1/13 , G09F9/35
Abstract: Phenylpyrimidinyl trans-cyclohexanecarboxylates of the formula … … form, in addition to a relatively broad nematic phase, a smectic C phase if R denotes an alkyl radical having 10 to 16 carbon atoms, in particular 11 to 16 carbon atoms, or an alkyloxy radical having 8 to 14 carbon atoms and R denotes an alkyl radical having 2 to 9 carbon atoms. Accordingly, they are suitable in particular as components of liquid-crystalline mixtures having a smectic C phase, since they induce a relatively broad nematic phase or widen a narrow nematic phase present and enlarge the temperature range of the smectic C phase towards low, but in particular towards high temperatures.
-
公开(公告)号:NO176276C
公开(公告)日:1995-03-08
申请号:NO884136
申请日:1988-09-16
Applicant: HOECHST AG
Inventor: WINGEN RAINER , DUBAL HANS-ROLF , ESCHER CLAUS , HEMMERLING WOLFGANG , MULLER INGRID , OHLENDOF DIETER
IPC: C07D239/26 , C07D239/34 , C09K19/34 , C09K19/46 , G02F1/137 , G02F1/141 , G02F1/13 , G09F9/35
Abstract: Phenylpyrimidinyl trans-cyclohexanecarboxylates of the formula … … form, in addition to a relatively broad nematic phase, a smectic C phase if R denotes an alkyl radical having 10 to 16 carbon atoms, in particular 11 to 16 carbon atoms, or an alkyloxy radical having 8 to 14 carbon atoms and R denotes an alkyl radical having 2 to 9 carbon atoms. Accordingly, they are suitable in particular as components of liquid-crystalline mixtures having a smectic C phase, since they induce a relatively broad nematic phase or widen a narrow nematic phase present and enlarge the temperature range of the smectic C phase towards low, but in particular towards high temperatures.
-
公开(公告)号:NO884136L
公开(公告)日:1989-03-20
申请号:NO884136
申请日:1988-09-16
Applicant: HOECHST AG
Inventor: WINGEN RAINER , DUEBAL HANS-ROLF , ESCHER CLAUS , HEMMERLING WOLFGANG , MUELLER INGRID , OHLENDOF DIETER
IPC: C07D239/26 , C07D239/34 , C09K19/34 , C09K19/46 , G02F1/137 , G02F1/141 , G02F1/13 , G09F9/35
Abstract: Phenylpyrimidinyl trans-cyclohexanecarboxylates of the formula … … form, in addition to a relatively broad nematic phase, a smectic C phase if R denotes an alkyl radical having 10 to 16 carbon atoms, in particular 11 to 16 carbon atoms, or an alkyloxy radical having 8 to 14 carbon atoms and R denotes an alkyl radical having 2 to 9 carbon atoms. Accordingly, they are suitable in particular as components of liquid-crystalline mixtures having a smectic C phase, since they induce a relatively broad nematic phase or widen a narrow nematic phase present and enlarge the temperature range of the smectic C phase towards low, but in particular towards high temperatures.
-
-
-
-