公开(公告)号:FI96013C
公开(公告)日:1996-04-25
申请号:FI885459
申请日:1988-11-24
Applicant: HOECHST AG
Inventor: BOTHE LOTHAR , CRASS GUENTHER , SCHLOEGL GUNTER , WILHELM THOMAS
-
公开(公告)号:FI96013B
公开(公告)日:1996-01-15
申请号:FI885459
申请日:1988-11-24
Applicant: HOECHST AG
Inventor: BOTHE LOTHAR , CRASS GUENTHER , SCHLOEGL GUNTER , WILHELM THOMAS
IPC: B29K23/00 , B29K105/34 , B29L9/00 , B32B27/32 , C08L23/12 , B29C55/12 , H01B17/60 , H01G4/18 , B32B27/18 , B32B15/08 , H01B3/44 , H01G4/20
Abstract: The multilayered film comprises a base layer of high-purity raw material for films for use in the electrical sector, and outer layers on one or both sides. It is suitable as an electrical insulation film, in particular as a dielectric in an electrical capacitor, and has dielectric properties which are improved for this purpose. The base layer and the outer layer(s) contain propylene polymers and stabilisers for the propylene polymers. The raw material of the base layer has an idealised thermooxidation temperature in the range from 260 to 300 DEG C, preferably from 260 to 280 DEG C, and the raw material of the outer layer(s) has an idealised thermooxidation temperature in the range from 240 to 300 DEG C, preferably from 240 to 270 DEG C. The multilayer film as a whole has an idealised thermooxidation temperature of from 250 to 290 DEG C, in particular from 250 to 275 DEG C. The content of organic neutralisers, in particular calcium stearate, in the raw materials is less than or equal to 100 ppm.
-
公开(公告)号:FI885459A
公开(公告)日:1989-05-29
申请号:FI885459
申请日:1988-11-24
Applicant: HOECHST AG
Inventor: BOTHE LOTHAR , CRASS GUENTHER , SCHLOEGL GUNTER , WILHELM THOMAS
IPC: B29K23/00 , B29C55/12 , B29K105/34 , B29L9/00 , B32B27/32 , C08L23/12 , H01B17/60 , H01G4/18 , B32B
Abstract: The multilayered film comprises a base layer of high-purity raw material for films for use in the electrical sector, and outer layers on one or both sides. It is suitable as an electrical insulation film, in particular as a dielectric in an electrical capacitor, and has dielectric properties which are improved for this purpose. The base layer and the outer layer(s) contain propylene polymers and stabilisers for the propylene polymers. The raw material of the base layer has an idealised thermooxidation temperature in the range from 260 to 300 DEG C, preferably from 260 to 280 DEG C, and the raw material of the outer layer(s) has an idealised thermooxidation temperature in the range from 240 to 300 DEG C, preferably from 240 to 270 DEG C. The multilayer film as a whole has an idealised thermooxidation temperature of from 250 to 290 DEG C, in particular from 250 to 275 DEG C. The content of organic neutralisers, in particular calcium stearate, in the raw materials is less than or equal to 100 ppm.
-
公开(公告)号:FI103098B
公开(公告)日:1999-04-30
申请号:FI915213
申请日:1991-11-05
Applicant: HOECHST AG
Inventor: BOTHE LOTHAR , DOLLE VOLKER , WINTER ANDREAS , WILHELM THOMAS
-
公开(公告)号:ZA9108800B
公开(公告)日:1992-07-29
申请号:ZA9108800
申请日:1991-11-06
Applicant: HOECHST AG
Inventor: BOTHE LOTHAR , LOTHAR BOTHE , DOLLE VOLKER , VOLKER DOLLE , WINTER ANDREAS , ANDREAS WINTER , WILHELM THOMAS , THOMAS WILHELM
CPC classification number: B32B27/08 , B32B27/16 , B32B27/18 , B32B27/32 , B32B2323/10 , Y10S428/91 , Y10T428/24942 , Y10T428/254 , Y10T428/258 , Y10T428/259 , Y10T428/2826 , Y10T428/31692 , Y10T428/31757 , Y10T428/31913 , Y10T428/3192
-
公开(公告)号:CA2020003A1
公开(公告)日:1990-12-30
申请号:CA2020003
申请日:1990-06-27
Applicant: HOECHST AG
Inventor: WILHELM THOMAS , BOTHE LOTHAR , CRASS GUENTHER , SCHLOEGL GUNTER , MUSKALLA WINFRIED
Abstract: A biaxially-oriented film with high mechanical strength, which includes 69 to 94.99% by weight of a polyolefin, 5 to 30% by weight of a natural or synthetic resin having a softening point in the range from 70 DEG to 170 DEG C., and 0.01 to 1% by weight of a nucleating agent, based on the total weight of the film. A method for producing this film includes biaxially drawing the film at temperatures below the melting point of the polyolefin.
-
公开(公告)号:FI894319A0
公开(公告)日:1989-09-13
申请号:FI894319
申请日:1989-09-13
Applicant: HOECHST AG
Inventor: WILHELM THOMAS , SCHLOEGL GUNTER , BOTHE LOTHAR , CRASS GUENTHER
IPC: B29K23/00 , B29C55/12 , B29L7/00 , C08J5/18 , C08K5/09 , C08L23/10 , H01B3/44 , H01B17/60 , H01G4/18 , H01B
Abstract: The extruded, biaxially oriented dielectric film is composed of high-purity electrical film raw material. It is suitable as electrical insulating film in particular as a dielectric in an electrical capacitor, and exhibits improved dielectric properties for this prupose. The film comprises propylene polymers and stabilizers for the propylene polymers. The raw material of the film has an idealized thermo-oxidation temperature in the range from 260 DEG to 300 DEG C., preferably 260 DEG to 280 DEG C. The dielectric film has an idealized thermo-oxidation temperature of 250 DEG to 300 DEG C., in particular 250 DEG to 280 DEG C. The content of organic neutralizing agents, in particular calcium stearate, in the raw material is less than/equal to 100 ppm.
-
公开(公告)号:FI885459A0
公开(公告)日:1988-11-24
申请号:FI885459
申请日:1988-11-24
Applicant: HOECHST AG
Inventor: BOTHE LOTHAR , CRASS GUENTHER , SCHLOEGL GUNTER , WILHELM THOMAS
IPC: B29K23/00 , B29C55/12 , B29K105/34 , B29L9/00 , B32B27/32 , C08L23/12 , H01B17/60 , H01G4/18 , B32B
Abstract: The multilayered film comprises a base layer of high-purity raw material for films for use in the electrical sector, and outer layers on one or both sides. It is suitable as an electrical insulation film, in particular as a dielectric in an electrical capacitor, and has dielectric properties which are improved for this purpose. The base layer and the outer layer(s) contain propylene polymers and stabilisers for the propylene polymers. The raw material of the base layer has an idealised thermooxidation temperature in the range from 260 to 300 DEG C, preferably from 260 to 280 DEG C, and the raw material of the outer layer(s) has an idealised thermooxidation temperature in the range from 240 to 300 DEG C, preferably from 240 to 270 DEG C. The multilayer film as a whole has an idealised thermooxidation temperature of from 250 to 290 DEG C, in particular from 250 to 275 DEG C. The content of organic neutralisers, in particular calcium stearate, in the raw materials is less than or equal to 100 ppm.
-
公开(公告)号:FI103098B1
公开(公告)日:1999-04-30
申请号:FI915213
申请日:1991-11-05
Applicant: HOECHST AG
Inventor: BOTHE LOTHAR , DOLLE VOLKER , WINTER ANDREAS , WILHELM THOMAS
Abstract: A polyolefin film which comprises a polypropylene base layer and at least one top layer of a propylene polymer, wherein the base layer is formed of an isotactic polypropylene and the top layer of a syndiotactic polypropylene, has high sealed-seam strength and excellent optical properties and is useful as, for example, a packaging material.
-
公开(公告)号:MX9101939A
公开(公告)日:1993-07-01
申请号:MX9101939
申请日:1991-11-05
Applicant: HOECHST AG
Inventor: BOTHER LOTHAR , DOLLE VOLKER , WINTER ANDREAS , WILHELM THOMAS
Abstract: A polyolefin film which comprises a polypropylene base layer and at least one top layer of a propylene polymer, wherein the base layer is formed of an isotactic polypropylene and the top layer of a syndiotactic polypropylene, has high sealed-seam strength and excellent optical properties and is useful as, for example, a packaging material.
-
-
-
-
-
-
-
-
-