POROUS PARTICLES AND COSMETICS
    1.
    发明公开
    POROUS PARTICLES AND COSMETICS 有权
    PORÖSETEILCHEN UND KOSMETIKA

    公开(公告)号:EP1591473A4

    公开(公告)日:2006-06-14

    申请号:EP04707626

    申请日:2004-02-03

    Applicant: KAO CORP

    Abstract: The invention provides porous particles having a mean particle diameter of as small as 75μm or below; composite porous particles obtained by incorporating an active ingredient into the above porous particles; processes for the production of both; and cosmetics containing the same. The invention relates to porous particles which are made mainly of a polyethylene resin having a degree of crystallization of 70% or above and have a mean particle diameter of 75μm or below; composite porous particles obtained by incorporating an active ingredient into the above porous particles; cosmetics containing the porous particles or the composite porous particles; and a process for the production of the porous particles which comprises mixing a polyethylene resin having a degree of crystallization of 70% or above with a low-molecular compound having a melting point lower than the softening (or melting) point of the polyethylene resin at a temperature equal to or higher than the softening (melting) point of the polyethylene resin, spraying the obtained mixture into a gas phase or a solvent at such a temperature that the mixture exhibits a viscosity of 600mPa s or below, and removing the low-molecular compound from the resulting particles.

    Abstract translation: 本发明提供多孔颗粒,多孔颗粒的制造方法和包含多孔颗粒的化妆品。 本发明的多孔粒子的平均粒径为75μm以下,结晶度为70%以上的聚乙烯树脂。 多孔颗粒还包含活性成分。 制造多孔颗粒的方法包括混合结晶度为70%以上的聚乙烯树脂和熔点低于聚乙烯树脂的软化温度(或熔点)的低分子量化合物, 另外在不低于聚乙烯树脂的软化温度(或熔点)的温度下,在混合物的粘度变为600mPa·s以下的温度下将混合物喷入气相或溶剂中, 从所得颗粒中除去低分子量化合物。

    PROCESS FOR PRODUCING NON-CRYSTALLINE CELLULOSE

    公开(公告)号:CA2762523A1

    公开(公告)日:2010-11-25

    申请号:CA2762523

    申请日:2010-05-19

    Applicant: KAO CORP

    Abstract: A process for producing non-crystalline cellulose with excellent productivity, wherein a cellulosic raw material in which the components thereof excluding water have a cellulose content of 20 mass% or higher and the cellulose has a cellulose I crystallinity, shown by the following calculation formula (1), of higher than 33% and which has a water content of 1.8 mass% or lower is treated with a pulverizer to reduce the cellulose I crystallinity thereof to 33% or lower. Cellulose I crystallinity (%) = [(I22.6-I18.5)/I22.6]×100 (1) [I22.6 indicates the X-ray diffraction intensity of the lattice plane (002) (diffraction angle 2? = 22.6º) and I18.5 indicates the X-ray diffraction intensity of the amorphous part (diffraction angle 2? = 18.5º).]

    PRODUCTION METHOD FOR CATIONIC HYDROXYPROPYL CELLULOSE
    5.
    发明公开
    PRODUCTION METHOD FOR CATIONIC HYDROXYPROPYL CELLULOSE 有权
    于制备阳离子性羟丙基

    公开(公告)号:EP2495259A4

    公开(公告)日:2013-11-27

    申请号:EP10826863

    申请日:2010-10-29

    Applicant: KAO CORP

    Abstract: The present invention relates to a process for producing a cationic hydroxypropyl cellulose including the step of reacting a low-crystalline powdery cellulose with a cationizing agent represented by the following general formula (1) and/or a cationizing agent represented by the following general formula (2), and propylene oxide in the presence of water in an amount of from 10 to 60% by mass on the basis of the low-crystalline powdery cellulose, and a catalyst: wherein R 1 to R 3 are each independently a linear or branched hydrocarbon group having 1 to 4 carbon atoms; and X and Z are each a halogen atom and may be the same or different from each other.

Patent Agency Ranking