A GLASS/METAL PACKAGE AND METHOD FOR PRODUCING THE SAME
    1.
    发明申请
    A GLASS/METAL PACKAGE AND METHOD FOR PRODUCING THE SAME 审中-公开
    一种玻璃/金属包装及其制造方法

    公开(公告)号:WO1998009324A1

    公开(公告)日:1998-03-05

    申请号:PCT/US1997011436

    申请日:1997-07-08

    Applicant: MOTOROLA INC.

    Abstract: A method of producing a glass/metal package where a glass portion of the package is built up around a provided leadframe (10) using applications of solderable and glass pastes (20) which are subsequently fired (30). The glass paste and leadframe are chosen to have similar coefficients of expansion and the leadframe is pretreated to degasify and control oxidation of the metal to promote glass adhesion to the leadframe and prevent microcracking at a glass/metal interface. A seal ring is applied to the glass paste (40) and a lid is attached to the seal ring (50). The package is used to provide a sealed inert internal environment for sensitive electronic components such as a piezoelectric element. The package may be configured for leaded or surface mounting (60).

    Abstract translation: 一种制造玻璃/金属封装的方法,其中使用随后烧制(30)的可焊接和玻璃浆料(20),围绕提供的引线框架(10)构建封装的玻璃部分。 玻璃浆料和引线框架被选择为具有相似的膨胀系数,引线框架经预处理以对金属进行脱气和控制氧化,以促进玻璃与引线框架的粘附,并防止玻璃/金属界面的微裂纹。 将密封环施加到玻璃膏(40)上,并且将盖子附接到密封环(50)。 该封装用于为诸如压电元件的敏感电子部件提供密封的惰性内部环境。 封装可以被配置为用于引线或表面安装(60)。

    ELECTRODE EDGE WAVE PATTERNS FOR PIEZOELECTRIC RESONATOR
    2.
    发明公开
    ELECTRODE EDGE WAVE PATTERNS FOR PIEZOELECTRIC RESONATOR 失效
    兰德公司SHAFT焊条型号压电谐振器

    公开(公告)号:EP0943159A1

    公开(公告)日:1999-09-22

    申请号:EP98925098.0

    申请日:1998-06-02

    Applicant: MOTOROLA, INC.

    IPC: H03H9

    CPC classification number: H03H9/132

    Abstract: A resonator (104) including a piezoelectric plate (102) with an elecrode (108) having a random pattern (100) along a portion of an edge of the electrode (108). The random pattern (100) dampens or destructively interferes with undesirable and inharmonic vibrational modes. For example, a rectangular AT-cut quartz resonator, which vibrates in a thickness-shear mode may also possess undesirable flexure and face-shear modes. These modes not only present undesirable spurious frequencies, they also change over temperature, disturbing a frequency-temperature response of the resonator. The random pattern (100) causes diffuse and/or specular scattering to reduce these undesirable modes, providing a more uniform frequency-temperature response which is beneficial in temperature compensated crystal oscillator applications.

    A GLASS/METAL PACKAGE AND METHOD FOR PRODUCING THE SAME
    3.
    发明公开
    A GLASS/METAL PACKAGE AND METHOD FOR PRODUCING THE SAME 失效
    玻璃/金属封装及其制造方法

    公开(公告)号:EP0857355A1

    公开(公告)日:1998-08-12

    申请号:EP97934033.0

    申请日:1997-07-08

    Applicant: MOTOROLA, INC.

    Abstract: A method of producing a glass/metal package where a glass portion of the package is built up around a provided leadframe (10) using applications of solderable and glass pastes (20) which are subsequently fired (30). The glass paste and leadframe are chosen to have similar coefficients of expansion and the leadframe is pretreated to degasify and control oxidation of the metal to promote glass adhesion to the leadframe and prevent microcracking at a glass/metal interface. A seal ring is applied to the glass paste (40) and a lid is attached to the seal ring (50). The package is used to provide a sealed inert internal environment for sensitive electronic components such as a piezoelectric element. The package may be configured for leaded or surface mounting (60).

Patent Agency Ranking