公开(公告)号:KR790001965B1
公开(公告)日:1979-12-30
申请号:KR750002251
申请日:1975-10-16
Applicant: STANDARD OIL CO OHIO
Inventor: COFFEY G P , LI G S
IPC: C08F220/44
Abstract: Acrylonitrile-indene copolymer(I) and acrylonitrile-coumarone copolymer contg. 50-90% acrylonitrile(II) having thermoplastic properties and can be readily thermoformed into containers with high heat-distorsion temp. (Td), low permeability to gas and exccllent resistance to solvents. Thus, I was prepd. 86% yield by stirring the mixt. of water 300, GAFAC RE-610 (emulsifier) 3, II 70, indene 30, n-dodecyl mercaptan 0.2 and K persulfate 0.3 wt. parts at 70OC for 16hr in N2 stream.
-
公开(公告)号:KR790001048B1
公开(公告)日:1979-08-22
申请号:KR750002839
申请日:1975-12-26
Applicant: STANDARD OIL CO OHIO
Inventor: COFFEY G P , GEORGE SU-HSIANG LI
Abstract: Graft acrylonitrile-butadiene-indene polymer, having good impact resistance, low permeability to gases, and high softening temp., was prepd. by grafting acrylonitrile and indene on nitrile rubber. Thus, an aq. emulsion of acrylonitrile 70, indene 17.5 and rubber latex 15 parts was polymd. at 60≦̸C for 6hr using K2S2O8 as catalyst and limonene dimercaptane, and then the reaction mixt. was heated to 70≦̸C and K2S2O8 0.2, indene 12.5 and limonene dimercaptane 0.5 part were added over a period 5hr to give I.
-
公开(公告)号:SE431878B
公开(公告)日:1984-03-05
申请号:SE7705741
申请日:1977-05-16
Applicant: STANDARD OIL CO OHIO
Inventor: COFFEY G P , MAZEKE H F
IPC: C08F2/00 , C08F2/38 , C08F20/00 , C08F20/42 , C08F220/42 , C08F255/06 , C08F279/00 , C08F279/02
-
公开(公告)号:SE416305B
公开(公告)日:1980-12-15
申请号:SE7510222
申请日:1975-09-12
Applicant: STANDARD OIL CO OHIO
Inventor: LI G S-H , COFFEY G P
IPC: C08F220/00 , C08F32/00 , C08F34/00 , C08F220/42 , C08F220/44
Abstract: Polymeric compositions having high heat-distortion temperatures which function as gas and vapor barrier materials which are composed of an olefinically unsaturated nitrile, such as acrylonitrile, and indene are described.
-
公开(公告)号:AU511583B2
公开(公告)日:1980-08-28
申请号:AU2472477
申请日:1977-04-29
Applicant: STANDARD OIL CO OHIO
Inventor: COFFEY G P , MAZEKE H F
IPC: C08F2/00 , C08F2/38 , C08F20/00 , C08F20/42 , C08F220/42 , C08F255/06 , C08F279/00 , C08F279/02 , C08F220/44
-
公开(公告)号:SE407581B
公开(公告)日:1979-04-02
申请号:SE7510548
申请日:1975-09-19
Applicant: STANDARD OIL CO OHIO
Inventor: COFFEY G P
IPC: C08F6/00 , C08F6/06 , C08F6/16 , C08F20/00 , C08F20/42 , C08F279/02 , C08F220/42 , C08F279/04
-
公开(公告)号:SE7513811A
公开(公告)日:1977-06-10
申请号:SE7513811
申请日:1975-12-08
Applicant: STANDARD OIL CO OHIO
Inventor: HENSLEY L W , LI G S-H , COFFEY G P
IPC: C08F279/00 , C08F244/00 , C08F279/02 , C08F291/00 , C08L7/00 , C08L21/00 , C08L33/00 , C08L33/02 , C08L51/00 , C08L51/04 , C08F291/02
CPC classification number: C08F279/02 , Y10S525/915 , Y10S525/933 , C08F220/42 , C08F220/10 , C08F232/08 , C08F220/12 , C08F234/02
-
公开(公告)号:NO754132L
公开(公告)日:1976-06-10
申请号:NO754132
申请日:1975-12-08
Applicant: STANDARD OIL CO OHIO
Inventor: HENSLEY L W , LI G S-H , COFFEY G P
IPC: C08F279/00 , C08F244/00 , C08F279/02 , C08F291/00 , C08L7/00 , C08L21/00 , C08L33/00 , C08L33/02 , C08L51/00 , C08L51/04 , C08F
-
公开(公告)号:NO753149L
公开(公告)日:1976-05-21
申请号:NO753149
申请日:1975-09-16
Applicant: STANDARD OIL CO OHIO
Inventor: LI G S-H , COFFEY G P
IPC: C08F220/00 , C08F32/00 , C08F34/00 , C08F220/42 , C08F220/44 , C08F244/00
Abstract: Polymeric compositions having high heat-distortion temperatures which function as gas and vapor barrier materials which are composed of an olefinically unsaturated nitrile, such as acrylonitrile, and indene are described.
-
公开(公告)号:DK142953B
公开(公告)日:1981-03-02
申请号:DK543371
申请日:1971-11-05
Applicant: STANDARD OIL CO OHIO
Inventor: COFFEY G P , BALL L E
IPC: C08F2/22 , C08F279/02
Abstract: 1360685 Graft polymers STANDARD OIL CO 21 Oct 1971 [13 Nov 1970] 48958/71 Heading C3G A graft polymer is produced by polymerization of (A) from 70 to 85% by weight of an olefinically unsaturated nitrile, (B) 2 to 13% of an alpha-olefin of structure wherein R 1 and R 11 are C 1 to C 7 -alkyl groups, (C) 2 to 30% of a monomer selected from a vinyl ester, acrylate ester, an acrylamide or a methacrylate ester, and (D) up to 17% of a vinyl or vinylidene aromatic monomer, wherein the combined amount of (A)+(B)+(C)+(D) is 100%, in the presence of from 1 to 30 parts by weight per 100 parts of (A) + (B) + (C)+(D) of (E) a rubbery polymer of 50 to 100% by weight of polymerized conjugated diene monomer and 50 to 0% of a polymerized vinyl or vinylidene aromatic monomer. In the examples, graft polymers are prepared in aqueous emulsion from (a) butadiene-styrene rubber or polybutadiene, acrylonitrile, isobutylene, styrene and methyl acrylate, N-t-octyl acrylamide, N-t-butyl acrylamide or vinyl acetate and (b) polybutadiene, acrylonitrile, diisobutylene, styrene and methyl acrylate.
-
-
-
-
-
-
-
-
-