Abstract:
Melt processed polyarylene sulfide compositions are described as are methods of forming the melt processed polyarylene sulfide compositions. The melt processed polyarylene sulfide compositions are formed according to a melt processing method that includes melt processing a mixture that includes a starting polyarylene sulfide, a disulfide compound and a filler. The melt processed polyarylene sulfide compositions may provide low chlorine content products having excellent strength characteristics.
Abstract:
Disclosed is a UV stabilized polyarylene sulfide composition, methods of forming the composition, and UV stabilized products that can be formed of the composition. The UV stabilized polyarylene sulfide composition can include a reactively functionalized polyarylene sulfide polymer in conjunction with a UV stabilizer. The reactivity of the polyarylene sulfide polymer is formed during melt processing via reaction of a reactively functionalized disulfide compound with a starting polyarylene sulfide. The reactivity of the polyarylene sulfide can encourage interaction between the polyarylene sulfide polymer and the UV stabilizer, which can improve dispersion of the UV stabilizer throughout the composition and improve miscibility between the polyarylene sulfide polymer and the UV stabilizer. Products can incorporate high concentrations of UV stabilizer and/or can be formed to very small cross sectional dimensions without phase separation between the UV stabilizer and the polyarylene sulfide.
Abstract:
Blow molded articles are made from a polymeric composition containing a mixture of polyphenylene sulfide resins. For instance, the polymeric composition may contain a linear polyphenylene sulfide resin combined with a branched polyphenylene sulfide resin. The composition can further contain a reinforcing agent, such as glass fibers, a polytetrafluoroethylene polymer, a polyphenylene oxide polymer, a silane coupling agent, and/or an impact modifier. Compositions made according to the present disclosure can have relatively high near zero shear rate melt strengths while also having high shear rate melt viscosities and high engineering stresses at a high percent elongations, making the compositions amenable to extrusion and molding processes. Compositions made according to the present disclosure are particularly well suited to molding articles with a complex shape. When producing blow molded articles, for instance, the composition provides better control over wall thickness while having improved interior surface smoothness at higher throughput and extrusion rates.
Abstract:
An injection molded housing for a portable electronic device is provided. The housing contains a thermoplastic composition that includes a polyarylene sulfide melt processed in the presence of a disulfide compound and a filler. Without intending to be limited by theory, it is believed that the disulfide can undergo a chain scission reaction with the starting polyarylene sulfide to lower its melt viscosity, which can lead to decreased attrition of the filler and thus improved mechanical properties. Due to this ability to reduce viscosity during melt processing, the present inventors have discovered that relatively high molecular weight polyarylene sulfides can be fed to the extruder with little difficulty.
Abstract:
A polymer composition that contains a polyaryletherketone and a liquid crystalline polymer that includes repeating units derived from naphthenic hydroxycarboxylic acids, naphthenic dicarboxylic acids, or a combination thereof in an amount of about 15 mol. % or less of the polymer is provided. The composition optionally contains reinforcing fibers (e.g., glass fibers) in an amount of no more than about 10 wt. %.