Abstract:
Components for automobiles are described that exhibit high strength and flexibility. The components are formed from a polyarylene sulfide that exhibits high strength and flexibility characteristics. Methods for forming the components are also described. Formation methods include dynamic vulcanization of a polyarylene sulfide composition that includes an impact modifier dispersed throughout the polyarylene sulfide. A crosslinking agent is combined with the other components of the composition following dispersal of the impact modifier throughout the composition. The automotive components can include tubular member such as pipes and hoses that can be utilized in exhaust systems, charge air systems, urea tanks, fuel systems, and so forth.
Abstract:
Pipe sections and methods for forming pipe sections are disclosed. A pipe section includes a hollow body formed from a polymer material, the hollow body having an inner surface and an outer surface, the inner surface defining an interior. The pipe section further includes a barrier layer surrounding and unbonded from the hollow body, the barrier layer having an inner surface and an outer surface. The barrier layer is formed from a continuous fiber reinforced thermoplastic material. Such pipe sections may be lightweight and flexible while exhibiting improved strength characteristics.
Abstract:
Pipe sections and methods for forming pipe sections are disclosed. A pipe section includes a hollow body, the hollow body having an inner surface and an outer surface, the inner surface defining an interior. The pipe section further includes a barrier layer surrounding the hollow body, the barrier layer having an inner surface and an outer surface. The barrier layer is formed from a polyarylene sulfide composition. The polyarylene sulfide composition includes a polyarylene sulfide and a crosslinked impact modifier. Such pipe sections exhibit high strength characteristics and flexibility as well as resistance to degradation, even in extreme temperature environments, while maintaining desirable processing characteristics.
Abstract:
A thermoplastic composition for use in a fine pitch electrical connector is provided. The thermoplastic composition contains a liquid crystalline polymer and a plurality of fibers. The volume average length of the fibers in the thermoplastic composition is selectively controlled according to the present invention so that it is within a certain range, such as from about 80 to about 250 micrometers. The fibers also have a narrow length distribution. That is, at least about 70% by volume of the fibers have a length within a certain range. Through the use of a liquid crystalline polymer and fibers of a certain weight average length and narrow length distribution, the present inventors have discovered that the resulting thermoplastic composition is able to achieve a desirable combination of strength and flowability, which enables it to be uniquely suited for the walls of a fine pitch connector.
Abstract:
Components formed of blow molded thermoplastic compositions are described. The blow molded thermoplastic compositions exhibit high strength and flexibility. Methods for forming the thermoplastic compositions are also described. Formation methods include dynamic vulcanization of a composition that includes an impact modifier dispersed throughout a polyarylene sulfide. A crosslinking agent is combined with the other components of the composition following dispersal of the impact modifier. The crosslinking agent reacts with the impact modifier to form crosslinks within and among the polymer chains of the impact modifier. The compositions can exhibit excellent physical characteristics at extreme temperatures and can be used to form, e.g., tubular member such as pipes and hoses and fibers.
Abstract:
Polyarylene sulfide compositions are described that exhibit high strength and flexibility. Methods for forming the polyarylene sulfide compositions are also described. Formation methods include dynamic vulcanization of a polyarylene sulfide composition that includes an impact modifier dispersed throughout the polyarylene sulfide. A crosslinking agent is combined with the other components of the composition following dispersal of the impact modifier throughout the composition. The crosslinking agent reacts with the impact modifier to form crosslinks within and among the polymer chains of the impact modifier. The compositions can exhibit excellent physical characteristics at extreme temperatures and can be used to form, e.g., tubular member such as pipes and hoses and fibers.
Abstract:
A polymer composition that contains at least one high performance polymer and at least one aromatic amide oligomer is provided. The oligomer can serve as a flow aid that lowers the overall viscosity of the polymer matrix under shear.
Abstract:
Pipe sections and methods for forming pipe sections are disclosed. A pipe section includes a hollow body formed from a metal material, the hollow body having an inner surface and an outer surface, the inner surface defining an interior. The pipe section further includes a barrier layer surrounding and bonded to the hollow body, the barrier layer having an inner surface and an outer surface. The barrier layer is formed from a continuous fiber reinforced thermoplastic material. Such pipe sections may be lightweight and flexible while exhibiting improved strength characteristics.
Abstract:
A polymer composition that contains a polyaryletherketone and a liquid crystalline polymer that includes repeating units derived from naphthenic hydroxycarboxylic acids, naphthenic dicarboxylic acids, or a combination thereof in an amount of about 15 mol. % or less of the polymer is provided. The composition optionally contains reinforcing fibers (e.g., glass fibers) in an amount of no more than about 10 wt. %.