公开(公告)号:ES2273362T3
公开(公告)日:2007-05-01
申请号:ES97911471
申请日:1997-11-06
Applicant: TORAY INDUSTRIES
Inventor: ISHIBASHI SOICHI , KYONO TETSUYUKI
IPC: C08J5/04 , C08L101/00 , B29B9/14 , B29B11/16 , B29C45/00 , B29C70/50 , B32B5/28 , C08K7/02 , C08K7/14 , C08L23/00 , C08L23/02 , C08L65/00 , C08L69/00 , C08L77/00
Abstract: LA PRESENTE INVENCION PROPONE UN MATERIAL DE MOLDEO QUE ES FACIL DE PRODUCIR Y PERMITE OBTENER UNA BUENA DISPERSION DE UN HAZ DE FIBRAS DE REFUERZO EN EL PRODUCTO MOLDEADO OBTENIDO POR MOLDEO POR INYECCION, ETC., UN PROCESO PARA SU PRODUCCION, UNA COMPOSICION DE RESINA BASADA EN POLIAMIDA CON BUENA FLUIDEZ, Y PRODUCTOS MOLDEADOS OBTENIDOS A PARTIR DE ELLOS. UN MATERIAL DE MOLDEO, QUE INCLUYE AL MENOS LOS COMPONENTES SIGUIENTES [A], [B] Y [C], CON EL COMPONENTE [C] DISPUESTO DE MODO QUE ENTRA EN CONTACTO CON UN COMPOSITE QUE INCLUYE LOS COMPONENTES [A] Y [B]. [A] UN HAZ DE FIBRAS CONTINUAS DE REFUERZO [B] UN OLIGOMERO O POLIMERO TERMOPLASTICO CON UN PESO MOLECULAR PROMEDIO PONDERADO DE ENTRE 200 Y 50000 Y UNA VISCOSIDAD EN FUNDIDO INFERIOR A LA DEL COMPONENTE [C] [C] UNA RESINA TERMOPLASTICA CON UN PESO MOLECULAR PROMEDIO PONDERADO DE 10000 O MAS.
-
公开(公告)号:CA2241863C
公开(公告)日:2008-07-29
申请号:CA2241863
申请日:1997-11-06
Applicant: TORAY INDUSTRIES
Inventor: KYONO TETSUYUKI , ISHIBASHI SOICHI
IPC: C08J5/04 , C08L77/00 , B29B9/14 , B29C45/00 , B29C70/40 , B29C70/50 , B32B5/26 , B32B5/28 , C08K7/02 , C08K7/14 , C08L23/02
Abstract: A molding material which is easy to prepare and in which reinforcing fiber bundles are well dispersible in the step of, e.g., injection molding; a process for preparing the same; a polyamide resin composition having a good fluidity, and moldings prepared therefrom. The molding material is characterized by comprising at least the following constituent elements (A), (B), and (C), the constituent element (C) being arranged so as to be in contact with a composite composed of the constituent elements (A) and (B): (A) a continuous reinforcing fiber bundle; (B) a thermoplastic polymer having a weight-average molecular weight of 200 to 50,000 and a lower melt viscosity than the constituent feature (C); and (C) a thermoplastic resin having a weight-average molecular weight of not less than 10,000.
-
公开(公告)号:DE69736802T2
公开(公告)日:2007-01-18
申请号:DE69736802
申请日:1997-11-06
Applicant: TORAY INDUSTRIES
Inventor: ISHIBASHI SOICHI , KYONO TETSUYUKI
IPC: C08J5/04 , C08L101/00 , B29B9/14 , B29B11/16 , B29C45/00 , B29C70/50 , B32B5/28 , C08K7/02 , C08K7/14 , C08L23/00 , C08L23/02 , C08L65/00 , C08L69/00 , C08L77/00
Abstract: The present invention provides a molding material which is easy to produce and allows a reinforcing fiber bundle to be well dispersed in the molded product obtained by injection molding, etc., a production process thereof, a polyamide based resin composition with good flowability, and molded products obtained from them. A molding material, comprising at least the following components ÄAÜ, ÄBÜ and ÄCÜ, with the component ÄCÜ arranged to contact a composite comprising the components ÄAÜ and ÄBÜ. ÄAÜ A continuous reinforcing fiber bundle ÄBÜ A thermoplastic polymer or oligomer with a weight average molecular weight of 200 to 50,000 and a melt viscosity lower than that of the component ÄCÜ ÄCÜ A thermoplastic resin with a weight average molecular weight of 10,000 or more.
-
公开(公告)号:AT513880T
公开(公告)日:2011-07-15
申请号:AT02710472
申请日:2002-02-01
Applicant: TORAY INDUSTRIES
Inventor: WADAHARA EISUKE , HONMA MASATO , ISHIBASHI SOICHI , NAGASHIMA YASUNORI , KOJIMA YUJI
IPC: C08L101/00 , C08J5/00 , C08J5/04 , C08K7/06 , C08K7/24
Abstract: The present invention relates to carbon fiber reinforced resin compositions comprising the following essential components (A), (B) and (C), and to molding compounds and molded products made by processing and molding the carbon fiber reinforced resin composition; Component (A): 0.01 to 0.7% by weight of vapor grown carbon fiber and/or nanotubes based on 100% by weight of the carbon fiber reinforced resin composition, of which the average diameter of single fiber ranges from 1 to 45 nm; Component (B): 6 to 40% by weight of carbon fiber based on 100% by weight of the carbon fiber reinforced resin composition, of which the average diameter of single fiber ranges from 1 to 20 mu m; and Component (C): resin. The present invention provides carbon fiber reinforced resin composition, molding compounds and molded products therefrom, having good conductivity, mechanical properties and moldability by the above constitution.
-
公开(公告)号:DE69736802D1
公开(公告)日:2006-11-23
申请号:DE69736802
申请日:1997-11-06
Applicant: TORAY INDUSTRIES
Inventor: ISHIBASHI SOICHI , KYONO TETSUYUKI
IPC: C08J5/04 , C08L101/00 , B29B9/14 , B29B11/16 , B29C45/00 , B29C70/50 , B32B5/28 , C08K7/02 , C08K7/14 , C08L23/00 , C08L23/02 , C08L65/00 , C08L69/00 , C08L77/00
Abstract: The present invention provides a molding material which is easy to produce and allows a reinforcing fiber bundle to be well dispersed in the molded product obtained by injection molding, etc., a production process thereof, a polyamide based resin composition with good flowability, and molded products obtained from them. A molding material, comprising at least the following components ÄAÜ, ÄBÜ and ÄCÜ, with the component ÄCÜ arranged to contact a composite comprising the components ÄAÜ and ÄBÜ. ÄAÜ A continuous reinforcing fiber bundle ÄBÜ A thermoplastic polymer or oligomer with a weight average molecular weight of 200 to 50,000 and a melt viscosity lower than that of the component ÄCÜ ÄCÜ A thermoplastic resin with a weight average molecular weight of 10,000 or more.
-
公开(公告)号:CA2241863A1
公开(公告)日:1998-05-14
申请号:CA2241863
申请日:1997-11-06
Applicant: TORAY INDUSTRIES
Inventor: KYONO TETSUYUKI , ISHIBASHI SOICHI
IPC: C08J5/04 , B29B9/14 , B29C45/00 , B29C70/50 , B32B5/28 , C08K7/02 , C08K7/14 , C08L23/02 , C08L77/00 , B32B5/26 , B29C70/40
Abstract: A molding material which is easy to prepare and in which reinforcing fiber bundles are well dispersible in the step of, e.g., injection molding; a process for preparing the same; a polyamide resin composition having a good fluidity, and moldings prepared therefrom. The molding material is characterized by comprising at least the following constituent elements (A), (B), and (C), the constituent element (C) being arranged so as to be in contact with a composite composed of the constituent elements (A) and (B): (A) a continuous reinforcing fiber bundle; (B) a thermoplastic polymer having a weight-average molecular weight of 200 to 50,000 and a lower melt viscosity than the constituent feature (C); and (C) a thermoplastic resin having a weight-average molecular weight of not less than 10,000.
-
公开(公告)号:EP2695722A4
公开(公告)日:2014-08-27
申请号:EP12767314
申请日:2012-02-23
Applicant: TORAY INDUSTRIES
Inventor: ISHIBASHI SOICHI , KOSHI MASAYUKI
IPC: B29C65/02
CPC classification number: B29C65/02 , B29C65/04 , B29C65/06 , B29C65/08 , B29C65/10 , B29C65/106 , B29C65/14 , B29C65/16 , B29C65/20 , B29C65/22 , B29C65/3416 , B29C65/3436 , B29C65/3492 , B29C65/3616 , B29C65/3636 , B29C65/3684 , B29C65/38 , B29C65/4815 , B29C65/5057 , B29C66/1122 , B29C66/301 , B29C66/54 , B29C66/71 , B29C66/712 , B29C66/7212 , B29C66/7214 , B29C66/72141 , B29C66/72143 , B29C66/723 , B29C66/7311 , B29C66/73774 , B29C66/73776 , B29C66/73921 , B29C66/73941 , B29C66/8322 , B29C70/00 , B29C70/345 , B32B27/28 , B32B27/34 , Y10T428/31728 , Y10T428/31909 , B29K2081/04 , B29K2077/00 , B29K2307/04
-
8.
公开(公告)号:JP2004256940A
公开(公告)日:2004-09-16
申请号:JP2003047016
申请日:2003-02-25
Applicant: TORAY INDUSTRIES
Inventor: HONMA MASATO , TSUCHIYA ATSUKI , ISHIBASHI SOICHI
IPC: C08J5/04 , B29C45/00 , B29K67/00 , B29K71/00 , B29K77/00 , B29K96/04 , B29K105/12 , C08K9/04 , C08L101/00 , D06M15/59
Abstract: PROBLEM TO BE SOLVED: To obtain a reinforced fiber which has excellent economic efficiency and productivity, is suitable for direct molding and combines bundling property and dispersibility, and to provide a molding material and a method for producing a molding. SOLUTION: The reinforced fiber for direct molding is obtained by attaching 0.1-20 wt.% of a block copolymer constituted of (a) 10-99 wt.% of an oxyalkylene group-containing block component and (b) 1-90 wt.% of at least one block component selected from (b1) a polyether, (b2) a polyester, (b3) a polyamide and (b4) a polyurethane to a reinforced fiber. COPYRIGHT: (C)2004,JPO&NCIPI
-
公开(公告)号:JP2002234999A
公开(公告)日:2002-08-23
申请号:JP2001033463
申请日:2001-02-09
Applicant: TORAY INDUSTRIES
Inventor: HONMA MASATO , NAGASHIMA YASUNORI , ISHIBASHI SOICHI
Abstract: PROBLEM TO BE SOLVED: To provide a molding material which gives a molded article having excellent mechanical characteristics, mechanical characteristics in a moisture absorption state, dimensional stability and external appearances without detriment to inherent molding properties, and its manufacturing method. SOLUTION: The pillar-shaped molding material comprises a component (A): a polyamide resin comprising at least (a1) a hexamethylenediamine adipamide unit, (a2) a hexamethylene isophthalamide unit and (a3) a capramide unit, and a component (B): a reinforcing fiber bundle, where the component (B) is arranged nearly parallel with the direction of the axis and has the substantially same length as that of the molding material. The manufacturing method of the molding material comprises the first step; a stranding step where the component (A) is molten and subsequently a continuous component (B) is caused to pass therethrough thereby to give a continuous strand, and the second step; a cutting step where the continuous strand is cooled and subsequently cut to give a pillar-shaped molding material.
-
公开(公告)号:JP2002088259A
公开(公告)日:2002-03-27
申请号:JP2000282100
申请日:2000-09-18
Applicant: TORAY INDUSTRIES
Inventor: WADAHARA EISUKE , ISHIBASHI SOICHI , SAWAOKA RYUJI , OHARA HARUO
IPC: C08J5/00 , B29B9/02 , B29B11/16 , C08K7/02 , C08L101/00
Abstract: PROBLEM TO BE SOLVED: To provide a molding material which can obtain a molded article having well-balanced mechanical properties, particularly impact strength and rigidity and, in addition, has excellent moldability, particularly flowability on molding and high productivity as well, its manufacturing method, and a molded article to be obtained therefrom. SOLUTION: The molding material comprises at least reinforcing fibers and two types of resins (A) and (B), and the resin (A) forms its domain in the matrix of the resin (B) and, simultaneously, has an islands-sea structure having a domain diameter of 0.4-15 mm. Further, the method for manufacturing the molding material comprises previously opening reinforcing fibers, preheating them, and impregnating the bundle of the reinforcing fibers with the resin (A) to form a composite of the reinforcing fibers with the resin (A), then coating the above composite with at least resin (B), and subsequently taking up the coated composite at a rate of >=10 m/min.
-
-
-
-
-
-
-
-
-