Abstract:
The present disclosure generally relates to durable solar mirror films, methods of making durable solar mirror films, and constructions including durable solar mirror films. In one embodiment, the present disclosure relates to a solar mirror film comprising: a multilayer optical film layer including having a coefficient of hygroscopic expansion of less than about 30 ppm per percent relative humidity; and a reflective layer having a coefficient of hygroscopic expansion.
Abstract:
Optical bodies are disclosed that include a first optical film, a second optical film and at least one rough strippable boundary layer disposed between the first and second optical films. Also disclosed are optical bodies including a strippable boundary layer disposed between the first and second optical films and including a first polymer and a second polymer that is substantially immiscible in the first polymer. The present disclosure also provides methods of processing optical bodies that include stretching the optical bodies.
Abstract:
Broadband reflectors include a UV-reflective multilayer optical film and a VIS/IR-reflective layer. In various embodiments, the VIS/IR reflective layer may be a reflective metal layer or a multilayer optical film. Concentrated solar power systems and methods of harnessing solar energy using the broadband reflectors and optionally comprising a celestial tracking mechanism are also disclosed.
Abstract:
Optical bodies are disclosed that include an optical film and at least one rough strippable skin layer. The at least one rough strippable skin layer can include a continuous phase and a disperse phase. In some embodiments, the at least one rough strippable skin layer can include a first polymer, a second polymer different from the first polymer and an additional material that is substantially immiscible in at least one of the first and second polymers. In some exemplary embodiments, a surface of the at least one rough strippable skin layer adjacent to the optical film comprises a plurality of protrusions and the adjacent surface of the optical film comprises a plurality of asymmetric depressions substantially corresponding to said plurality of protrusions. Methods of making such exemplary optical bodies are also disclosed.
Abstract:
Multi-layer optical film comprising optical layers reflecting at least 50 percent of incident UV light over specified wavelength ranges. Embodiments of the multi-layer optical films are useful, for example, as a UV protective covering.
Abstract:
Articles including bi-layers of anionic and cationic self-limited monolayers are described. One monolayer comprises titanium dioxide and the other layer comprises a fluorinated polyelectrolyte. The use of titanium dioxide nanoparticles and perfluorinated polymers such as perfluorosulfonic acid polymer are described. Layer-by-layer, self-assembled layers and processes of producing such layers are also described.
Abstract:
The present disclosure relates generally to anti-soiling compositions, methods of applying anti-soiling compositions, and equipment for applying anti-soiling compositions. In some embodiments, the present disclosure relates to a method of forming a durable coating on a glass substrate, comprising: (1) applying a coating composition to a glass substrate, the applied coating composition having a thickness of greater than 4 microns; the coating composition consisting essentially of about 0.25% to about 10% by weight of non-oxidizing nanoparticles, an acid, and water; (2) allowing the coating composition to remain on the glass substrate for at least an amount of time sufficient to permit at least some of the nanoparticles to bond to the glass substrate; (3) reducing the thickness of the coating composition to about 0.25 to 4 microns, and (4) evaporating at least some of the water to form the durable coating.
Abstract:
A backlight that includes a front reflector and a back reflector that form a hollow light recycling cavity including an output surface is disclosed. The backlight further includes one or more light sources disposed to emit light into the light recycling cavity. The front reflector includes an on-axis average reflectivity of at least 90% for visible light polarized in a first plane, and an on-axis average reflectivity of at least 25% but less than 90% for visible light polarized in a second plane perpendicular to the first plane.