Abstract:
A method of manufacturing a hydrophobic material is provided, which includes: (a) mixing a sol-gel precursor, water, and catalyst to perform a sol-gel reaction for forming a solution having particles therein, (b) modifying the particles with a hydrophobic agent to form surface-modified particles, (c) adding a small-molecular surfactant to the solution containing the surface-modified particles to form a first dispersion, (d) mixing a resin, a water soluble polymer, and water to form a second dispersion, and (e) mixing the first dispersion and the second dispersion to obtain a hydrophobic material.
Abstract:
The present disclosure provides a method for forming an inorganic polymer material, including mixing 10 to 80 parts by weight of tetraalkoxysilane and 10 to 80 parts by weight of trialkoxysilane to form a mixture; and performing a reaction at pH of 0 to 4 by adding 5 to 30 parts by weight of a catalyst to the mixture to form an inorganic polymer material.