公开(公告)号:US20230312936A1
公开(公告)日:2023-10-05
申请号:US18331261
申请日:2023-06-08
Applicant: CubicPV Inc.
Inventor: Michael Irwin , Erin Sanehira
CPC classification number: C09D1/00 , B05D3/0254 , C03C17/25 , C03C2218/32 , C03C2217/217 , C03C2218/113
Abstract: A method for preparing a nickel oxide precursor ink comprising: preparing a solvent comprising diols and alcohol amines; adding nickel nitrate into the solvent to form a nickel nitrate containing solution; adding at least one metal acetate into the nickel nitrate containing solution to form a nickel nitrate and metal acetate containing solution; adding water to the nickel nitrate and metal acetate containing solution to form a nickel oxide precursor mixture; heating the nickel oxide precursor mixture to 60 to 75 Celsius; and cooling the nickel oxide precursor mixture to form the nickel oxide precursor ink.
-
公开(公告)号:US20240392135A1
公开(公告)日:2024-11-28
申请号:US18790753
申请日:2024-07-31
Applicant: CubicPV Inc.
Inventor: Michael D. Irwin , Erin Sanehira
Abstract: A method for preparing a nickel oxide precursor ink comprising: preparing a solvent comprising diols and alcohol amines; adding nickel nitrate into the solvent to form a nickel nitrate containing solution; adding at least one metal acetate into the nickel nitrate containing solution to form a nickel nitrate and metal acetate containing solution; adding water to the nickel nitrate and metal acetate containing solution to form a nickel oxide precursor mixture; heating the nickel oxide precursor mixture to 60 to 75 Celsius; and cooling the nickel oxide precursor mixture to form the nickel oxide precursor ink.
-
公开(公告)号:US12084580B2
公开(公告)日:2024-09-10
申请号:US18331261
申请日:2023-06-08
Applicant: CubicPV Inc.
Inventor: Michael Irwin , Erin Sanehira
CPC classification number: C09D1/00 , B05D3/0254 , C03C17/25 , C03C2217/217 , C03C2218/113 , C03C2218/32
Abstract: A method for forming a nickel oxide layer is disclosed herein. In some embodiments, a method includes depositing a nickel oxide precursor ink on a substrate, wherein the nickel oxide precursor ink comprises a solvent comprising diols, alcohol amines, and water, Ni(NO3)2·6H2O, and at least one metal acetate selected from the group consisting of Ni(CH3CO2)2·4H2O and Cu(CH3CO2)2·1H2O, annealing the nickel oxide precursor ink at a temperature between 250° to 400° Celsius for between 10 minutes and 6 hours to form a nickel oxide layer, and cooling the nickel oxide layer.
-
公开(公告)号:US11713396B2
公开(公告)日:2023-08-01
申请号:US17136503
申请日:2020-12-29
Applicant: CUBICPV INC.
Inventor: Michael D. Irwin , Erin Sanehira
CPC classification number: C09D1/00 , B05D3/0254 , C03C17/25 , C03C2217/217 , C03C2218/113 , C03C2218/32
Abstract: A method for preparing a nickel oxide precursor ink comprising: preparing a solvent comprising diols and alcohol amines; adding nickel nitrate into the solvent to form a nickel nitrate containing solution; adding at least one metal acetate into the nickel nitrate containing solution to form a nickel nitrate and metal acetate containing solution; adding water to the nickel nitrate and metal acetate containing solution to form a nickel oxide precursor mixture; heating the nickel oxide precursor mixture to 60 to 75 Celsius; and cooling the nickel oxide precursor mixture to form the nickel oxide precursor ink.
-
-
-