公开(公告)号:US20220314587A1
公开(公告)日:2022-10-06
申请号:US17597263
申请日:2020-01-30
Applicant: NITTO DENKO CORPORATION
Inventor: Fumika KAWATAKE , Asuka GOMI , Kenichi OKADA , Akinori TAMURA
IPC: B32B27/08 , B32B27/30 , B32B27/28 , B32B7/12 , B32B7/06 , C08F220/18 , C08F220/36 , C08J5/18
Abstract: A surface modification sheet (X) of the present invention includes a release sheet (10) and a surface modification layer (20) thereon. The surface modification layer (20) contains a polymer having a side chain containing an ethylenic double bond. The side chain of the polymer preferably includes a unit derived from an isocyanate compound containing the ethylenic double bond.
-
公开(公告)号:US20200063004A1
公开(公告)日:2020-02-27
申请号:US16465492
申请日:2017-11-29
Applicant: NITTO DENKO CORPORATION
Inventor: Ryoko ASAI , Kayo SHIMOKAWA , Kensuke TANI , Yoshiko KIRA , Kenichi OKADA
IPC: C09J133/10 , C09J121/00 , C09J135/00 , C09J123/22 , C09J7/20 , C08G18/76
Abstract: The present invention relates to an adhesive composition containing a base polymer, a water-absorbing material, and a moisture-curable component, wherein the moisture-curable component is contained in an unreacted state, an adhesive layer made from the adhesive composition, and an adhesive sheet including the adhesive layer.
-
公开(公告)号:US20190016925A1
公开(公告)日:2019-01-17
申请号:US16069259
申请日:2017-01-10
Applicant: NITTO DENKO CORPORATION
Inventor: Akiko TANAKA , Keisuke SHIMOKITA , Kenichi OKADA , Masayuki MINAKATA
IPC: C09J7/30 , C09J5/00 , C09J7/40 , C09J11/06 , C09J163/00
Abstract: A stickable-curable adhesive sheet bonds a deformation/conversion device to an adherend. The stickable-curable adhesive sheet contains a stickable-curable adhesive component and a curing component curing the stickable-curable adhesive component. The stickable-curable adhesive component has pressure-sensitive adhesiveness before curing and the initial tensile elastic modulus at 25° C. of the stickable-curable adhesive sheet after curing is 5×108 Pa or more.
-
公开(公告)号:US20240141217A1
公开(公告)日:2024-05-02
申请号:US18280161
申请日:2022-02-28
Applicant: NITTO DENKO CORPORATION
Inventor: Satoshi HONDA , Masahiro KUZE , Kenichi OKADA , Takayuki KUROKAWA , Jian Ping GONG
IPC: C09J167/00 , C08J5/18 , C09J7/38 , C09J133/08
CPC classification number: C09J167/00 , C08J5/18 , C09J7/38 , C09J133/08
Abstract: Provided is a resin film that has a stress integral value of greater than 10 MPa and 1000 MPa or less when uniaxially stretched at a tensile speed of 300 mm/min at 25° C. until it breaks. The resin film showing these properties is supple and durable.
-
公开(公告)号:US20190030829A1
公开(公告)日:2019-01-31
申请号:US16070239
申请日:2017-01-13
Applicant: NITTO DENKO CORPORATION
Inventor: Kenichi OKADA , Keisuke SHIMOKITA , Akiko TANAKA , Eriko FUNATSU , Asuka GOMI , Akira SHIMAZU
Abstract: A surface-modified thermoplastic resin in which sufficient bonding strength is applied to a thermoplastic resin and a method thereof are provided. A bonded structure capable of exhibiting sufficient bonding strength and a method thereof are provided. A thermal transfer surface-modifying sheet that can be preferably used in the method for manufacturing a surface-modified thermoplastic resin is provided. A thermoplastic resin with a thermal transfer surface-modifying sheet including the thermal transfer surface-modifying sheet is provided. The method for manufacturing a surface-modified thermoplastic resin, in which an easy adherence layer is laminated on a thermoplastic resin having a melting point of T° C., the method includes: providing the easy adherence layer on at least a part of a surface of the thermoplastic resin; and performing heat welding at a temperature equal to or higher than (T−50)° C.
-
公开(公告)号:US20180327635A1
公开(公告)日:2018-11-15
申请号:US15773586
申请日:2016-10-31
Applicant: NITTO DENKO CORPORATION
Inventor: Akiko YOSHIDA , Kenichi OKADA , Koji AKAZAWA
IPC: C09J5/04 , C09J7/40 , C09J163/00
Abstract: An adhesion method including: a step (1), disposing a stickable-curable adhesive layer on a first adherend; a step (2), disposing a curing agent layer on a second adherend, the curing agent layer being able to cure the stickable-curable adhesive layer by contacting and reacting with the stickable-curable adhesive layer; and a step (3), bringing the stickable-curable adhesive layer into contact with the curing agent layer so that they are sandwiched by the first adherend and the second adherend.
-
公开(公告)号:US20220186093A1
公开(公告)日:2022-06-16
申请号:US17684126
申请日:2022-03-01
Applicant: NITTO DENKO CORPORATION
Inventor: Ryoko ASAI , Kayo SHIMOKAWA , Kensuke TANI , Yoshiko KIRA , Kenichi OKADA
IPC: C09J153/02 , C09J7/32 , C09J11/06 , C09J7/20 , C09J7/00 , C09J11/08 , C09J201/00 , C09J133/00 , C09J121/00 , C08G18/76 , C09J123/22 , C09J133/10 , C09J135/00
Abstract: The present invention relates to an adhesive composition containing a base polymer, a water-absorbing material, and a moisture-curable component, wherein the moisture-curable component is contained in an unreacted state, an adhesive layer made from the adhesive composition, and an adhesive sheet including the adhesive layer.
-
8.
公开(公告)号:US20210214587A1
公开(公告)日:2021-07-15
申请号:US16967504
申请日:2019-01-28
Applicant: Nitto Denko Corporation
Inventor: Naofumi KOSAKA , Yosuke SHIMIZU , Satoshi HONDA , Taiki SHIMOKURI , Shou TAKARADA , Masayuki SATAKE , Kenichi OKADA , Atsushi TAKASHIMA , Ginji MIZUHARA , Masayuki OKAMOTO , Ryoko ASAI
IPC: C09J7/38 , C09J11/08 , C09J11/06 , C09J133/08 , B32B27/30 , B32B27/18 , B32B7/06 , B32B37/12 , B32B37/18 , B32B38/10
Abstract: Provided is a PSA sheet having a PSA layer. The PSA layer includes a layer A forming at least one surface thereof. The PSA sheet has an adhesive strength N0 of 2.0 N/10 mm or greater, after one day at room temperature following application of the layer A side to a surface of an alkaline float glass plate as an adherend having a contact angle of 5°-10° with distilled water; has an N1 to N0 reduction rate of 30% or lower, wherein N1 is a water-resistant adhesive strength measured after stored at room temperature for one day, immersed in water for 30 minutes, taken out from the water and then residual water is wiped off; and has an N2 to N0 reduction rate of 40% or higher, wherein N2 is a water-peel strength measured after stored at room temperature for one day, 20 μL distilled water is dropped onto the adherend and is allowed to enter a PSA layer/adherend interfacial edge. N2 is measured at a tensile speed of 300 mm/min at a peel angle of 180°.
-
公开(公告)号:US20190016923A1
公开(公告)日:2019-01-17
申请号:US15551062
申请日:2016-03-07
Applicant: NITTO DENKO CORPORATION
Inventor: Kensuke TANI , Mizuho NAGATA , Kaori MIZOBATA , Masatsugu SOGA , Ryota MASUDA , Masayuki SATAKE , Kenichi OKADA , Naofumi KOSAKA , Keisuke SHIMOKITA
IPC: C09J7/02
Abstract: Provided is an adhesive member to be adhesively fixed through pressure which has both position adjustability and adhesiveness and is capable of producing a sufficient adhesive strength in addition to the position adjustability. The adhesive member comprises a support, a pressure-sensitive adhesive layer provided on one surface of the support, and a plurality of protrusion elements arranged, in spaced-apart relation to each other, on a principal surface of the pressure-sensitive adhesive layer on a side opposite to the support. Each of the protrusion elements is composed of an aggregation of a plurality of cohesive particles, wherein the adhesive member has a frictional force of 0.4 N/cm2 or less, with respect to a stainless steel plate serving as an adherend, as measured when the protrusion elements are in contact with a surface of the adherend, and a shear adhesive strength of 45 N/cm2 or more.
-
10.
公开(公告)号:US20240368435A1
公开(公告)日:2024-11-07
申请号:US18773082
申请日:2024-07-15
Applicant: NITTO DENKO CORPORATION
Inventor: Naofumi KOSAKA , Yosuke SHIMIZU , Satoshi HONDA , Taiki SHIMOKURI , Shou TAKARADA , Masayuki SATAKE , Kenichi OKADA , Atsushi TAKASHIMA , Ginji MIZUHARA , Masayuki OKAMOTO , Ryoko ASAI
IPC: C09J7/38 , B32B7/06 , B32B27/18 , B32B27/30 , B32B37/12 , B32B37/18 , B32B38/10 , C09J11/06 , C09J11/08 , C09J133/08
Abstract: Provided is a PSA sheet having a PSA layer. The PSA layer includes a layer A forming at least one surface thereof. The PSA sheet has an adhesive strength N0 of 2.0 N/10 mm or greater, after one day at room temperature following application of the layer A side to a surface of an alkaline float glass plate as an adherend having a contact angle of 5°-10° with distilled water; has an N1 to N0 reduction rate of 30% or lower, wherein N1 is a water-resistant adhesive strength measured after stored at room temperature for one day, immersed in water for 30 minutes, taken out from the water and then residual water is wiped off, and has an N2 to N0 reduction rate of 40% or higher, wherein N2 is a water-peel strength measured after stored at room temperature for one day, 20 μL distilled water is dropped onto the adherend and is allowed to enter a PSA layer/adherend interfacial edge. N2 is measured at a tensile speed of 300 mm/min at a peel angle of 180°.
-
-
-
-
-
-
-
-
-