Abstract:
The present invention relates to an adhesive composition containing at least a polymer and an ionic liquid, in which when an adhesive layer is formed of a composition composed of components other than the ionic liquid among components contained in the adhesive composition, the adhesive layer has a relative permittivity of 5 or more at a frequency of 100 Hz, after being left to stand in an environment of 22° C. and 20% RH for 3 days.
Abstract:
Provided is a PSA sheet having a PSA layer. The PSA layer includes a layer A forming at least one surface thereof. The PSA sheet has an adhesive strength N0 of 2.0 N/10 mm or greater, after one day at room temperature following application of the layer A side to a surface of an alkaline float glass plate as an adherend having a contact angle of 5°-10° with distilled water; has an N1 to N0 reduction rate of 30% or lower, wherein N1 is a water-resistant adhesive strength measured after stored at room temperature for one day, immersed in water for 30 minutes, taken out from the water and then residual water is wiped off; and has an N2 to N0 reduction rate of 40% or higher, wherein N2 is a water-peel strength measured after stored at room temperature for one day, 20 μL distilled water is dropped onto the adherend and is allowed to enter a PSA layer/adherend interfacial edge. N2 is measured at a tensile speed of 300 mm/min at a peel angle of 180°.
Abstract:
A pressure-sensitive adhesive composition includes: 100 parts by mass of a polymer (A) having a glass transition temperature lower than 0° C.; 0.05 parts by mass to 3 parts by mass of a (meth)acrylic polymer (B) having a weight average molecular weight (MwB) of 1000≦MwB
Abstract:
An acrylic pressure-sensitive adhesive composition contains 100 parts by mass of an acrylic polymer (A), 1 to 70 parts by mass of a (meth)acrylic polymer (B) having a weight average molecular weight (Mw) of 1000≦Mw
Abstract:
Provided is a PSA sheet having a PSA layer. The PSA layer includes a layer A forming at least one surface thereof. The PSA sheet has an adhesive strength N0 of 2.0 N/10 mm or greater, after one day at room temperature following application of the layer A side to a surface of an alkaline float glass plate as an adherend having a contact angle of 5°-10° with distilled water; has an N1 to N0 reduction rate of 30% or lower, wherein N1 is a water-resistant adhesive strength measured after stored at room temperature for one day, immersed in water for 30 minutes, taken out from the water and then residual water is wiped off, and has an N2 to N0 reduction rate of 40% or higher, wherein N2 is a water-peel strength measured after stored at room temperature for one day, 20 μL distilled water is dropped onto the adherend and is allowed to enter a PSA layer/adherend interfacial edge. N2 is measured at a tensile speed of 300 mm/min at a peel angle of 180°.
Abstract:
A polarizing film has a transparent protective film provided on at least one side of a polarizer through an adhesive layer. The transparent protective film is a cellulose-based resin film. The adhesive layer is formed by a cured layer obtained by irradiating an active energy ray-curable adhesive composition with active energy rays. The composition contains 0.0% by weight to 4.0% by weight of an active energy ray-curable compound (A) having an SP value of 29.0 (MJ/m3)1/2 to 32.0 (MJ/m3)1/2, 5.0% by weight to 98.0% by weight of an active energy ray-curable compound (B) having the SP value of 18.0 (MJ/m3)1/2 to 21.0 (MJ/m3)1/2 (exclusive of 21.0 (MJ/m3)1/2), and 5.0% by weight to 98.0% by weight of an active energy ray-curable compound (C) having the SP value of 21.0 (MJ/m3)1/2 to 26.0 (MJ/m3)1/2 on a basis of 100% by weight of a total amount of the composition.
Abstract:
A pressure-sensitive adhesive composition includes: 100 parts by mass of a polymer (A) (Tg:lower than 0° C.); 0.05 to 3 parts by mass of a (meth)acrylic polymer (B) (MWB:1000≦MWB
Abstract:
An acrylic pressure-sensitive adhesive composition contains: an acrylic polymer (A); and a (meth)acrylic polymer (B) that includes, as a monomer unit, a (meth)acrylic monomer having a tricyclic or higher alicyclic structure and that has a weight average molecular weight of 1000 or more and less than 30000.
Abstract:
Provided is an optical PSA composition that can be easily peeled using an aqueous liquid such as water and has sufficient adhesive strength. An optical PSA composition comprising an acrylic polymer is provided. The PSA composition comprises at least one species of compound A selected among surfactants and compounds having polyoxyalkylene backbones. The monomers forming the acrylic polymer comprises less than 20 wt % alkoxyalkyl (meth)acrylate and less than 20 wt % alkoxypolyalkylene glycol (meth)acrylate. Alternatively, the compound A content is less than 1 part by weight to 100 parts by weight of the acrylic polymer.
Abstract: