FIBER COMPOUND RESIN COMPOSITION AND METHOD OF MANUFACTURING THE SAME

    公开(公告)号:US20190284367A1

    公开(公告)日:2019-09-19

    申请号:US16254814

    申请日:2019-01-23

    Abstract: For a fiber compound resin composition, a melt-kneading process is performed together with a base resin 1, a dispersant, etc. without performing a pretreatment through wet dispersion for the purpose of defibration treatment and modification treatment of a fibrous filler 2. As a result, each fiber of the fibrous filler 2 is defibrated from end portions in a fiber length direction, while a dispersant component put in at the same time is more selectively adsorbed to defibrated portions 3 at the end portions defibrated and increased in surface area. As a result, hydrophobization of the defibrated portions 3 is promoted as compared to a non-defibrated portion 4, so that a difference in hydrophobicity is formed in the fiber length direction of the fibrous filler 2. Therefore, even when the fibrous filler 2 is added in large amount, a melt viscosity during molding may be lowered without reducing a strength of a molded article.

    COMPOSITE RESIN COMPOSITION
    2.
    发明申请

    公开(公告)号:US20180201770A1

    公开(公告)日:2018-07-19

    申请号:US15817879

    申请日:2017-11-20

    CPC classification number: C08L23/12 C08J5/045 C08J2323/02 C08J2323/12

    Abstract: Provided is a composite resin composition to be used as a material for a molded article produced by a molding machine. The composite resin composition includes a main ingredient resin 1 and a fibrous filler 2, and the fiber length direction end of the fibrous filler 2 is defibrated. The length of the defibrated portion 3 is 5% or more and 50% or less of the fiber length of the entire fibrous filler 2. The fiber diameter in the defibrated portion 3 of the fibrous filler 2 is 1/1000 or more and 1/10 or less the fiber diameter in the undefibrated portion. The modulus of elasticity of the fibrous filler 2 is higher than the modulus of elasticity of the main ingredient resin 1, and the difference between these moduli of elasticity is within 20 GPa.

Patent Agency Ranking