Abstract:
A package for dissipating heat power and/or optical power from an optical fiber component of a device is provided. The package includes a heat sink packaging receptacle for accommodating the optical fiber component having a cavity for receiving a temperature sensitive portion of the optical fiber component. According to one aspect, the package may include a power-dissipative material for dissipating heat power or optical power, the power-dissipative material extending within the cavity and surrounding the temperature-sensitive portion of the optical fiber component. According to another aspect, the package may include at least one channel extending between the cavity and an end of the heat sink packaging receptacle, the channel being in intimate contact with the cladding of the optical fiber component for dissipating heat power and/or optical power from the optical fiber component.
Abstract:
A package for dissipating heat power and/or optical power from an optical fiber component of a device is provided. The package includes a heat sink packaging receptacle for accommodating the optical fiber component having a cavity for receiving a temperature sensitive portion of the optical fiber component. According to one aspect, the package may include a power-dissipative material for dissipating heat power or optical power, the power-dissipative material extending within the cavity and surrounding the temperature-sensitive portion of the optical fiber component. According to another aspect, the package may include at least one channel extending between the cavity and an end of the heat sink packaging receptacle, the channel being in intimate contact with the cladding of the optical fiber component for dissipating heat power and/or optical power from the optical fiber component.
Abstract:
A large mode field diameter optical fiber is disclosed. It is a single mode optical fiber which has a core and a cladding. The core of this fiber has two regions, an inner core region and an outer core region which has a refractive index lower than that of the inner core region. The inner core region is doped with a rare-earth element, such as Er2O3, and a co-dopant, such as Al2O3, and the outer core region is doped with a dopant such as GeO2. The types and amounts of the dopants and co-dopants are adjusted to obtain a fiber with a mode field diameter greater than 5.5 μm at a wavelength of 1550 nm.
Abstract translation:公开了一种大模场直径的光纤。 它是具有芯和包层的单模光纤。 该纤维的芯部具有折射率低于内芯区域的折射率的两个区域,内芯区域和外芯区域。 内核区域掺杂有稀土元素,例如Er 2 O 3 N 3,以及共掺杂剂,例如Al 2 O 3 > O 3,并且外芯区域掺杂有诸如GeO 2的掺杂剂。 调整掺杂剂和辅助掺杂剂的类型和量,以获得在1550nm波长下模场直径大于5.5μm的光纤。
Abstract:
An optically active glass and an optical fiber comprising such glass, having reduced photodarkening properties are provided. The optically active glass is mainly composed of silica representing from about 50 to 98 mol % of the glass. It also includes at least one active ion, such as a rear-earth ion, which induces a photodarkening effect in optical properties of the glass. Moreover, the glass includes an effective amount of phosphorus oxide providing the photodarkening reducing effect, preferably in an amount of from about 1 to 30 mol %. A method for reducing a photodarkening effect in optical properties of an optically active glass including the step of introducing phosphorus oxide to the glass is also provided.
Abstract:
A light-emitting device is provided which includes a gain medium having an optically-active phosphosilicate glass, wherein the phosphosilicate glass includes at least one active ion dopant and from about 1 to 30 mol % of phosphorus oxide. The phosphorous oxide may be present in an effective amount for reducing any photodarkening effect and increasing the saturation energy of the system. The active ion dopant may be a rare earth dopant. The light-emitting device may include an optical waveguide, the optical waveguide including the gain medium. The optical waveguide may have a core and at least one cladding, and the gain medium having the phosphosilicate glass may be found in the core and/or in one of the cladding
Abstract:
A double-clad optical fiber has an inner cladding with a pentagonal or heptagonal cross-section. The core of this fiber can be in the center or off-center. Moreover, the fiber may comprise stress field portions within the inner cladding which cause further distortions for deflecting pumped light to the core. In addition, the core may have a dual structure with an inner portion and an outer portion surrounding the inner portion. It is preferable that the inner cladding should have a lower index of refraction than the core and the outer cladding which surrounds the inner cladding should have a lower index of refraction than the inner cladding.
Abstract:
A method of manufacturing an optical fiber is provided. The method involves providing a fiber preform with an active core and a pump-guiding cladding, and assembling one or more side rods to the fiber preform. The side rods extend longitudinally along an outer surface of the pump-guiding cladding. The resulting fiber preform assembly is drawn into the optical fiber. Each side rod defines a longitudinal protrusion extending along the optical fiber. Each longitudinal protrusion may have a cross-section forming a middle bump projecting radially away from the outer surface of the pump-guiding cladding and smooth transition regions with this outer surface of the pump-guiding cladding on opposite sides of the middle bump.
Abstract:
The present relates to a spatially modulated cladding mode stripper and to an optical fiber comprising a spatially modulated cladding mode stripper. The spatially modulated cladding mode stripper comprises a series of alternating high cladding light extracting regions and low cladding light extracting regions located along a portion of a cladding to modulate extracting of cladding light therefrom.
Abstract:
A double clad optical fiber having a portion extending along its length along which an outer waveguide cladding and a protective jacket are absent and having faces of the second waveguide cladding at two lengthwisely opposite ends, wherein a water impervious sealant is applied to impede lengthwise diffusion of water through the faces of the second waveguide cladding
Abstract:
An optically active glass and an optical fiber comprising such glass, having reduced photodarkening properties are provided. The optically active glass is mainly composed of silica representing from about 50 to 98 mol % of the glass. It also includes at least one active ion, such as a rear-earth ion, which induces a photodarkening effect in optical properties of the glass. Moreover, the glass includes an effective amount of phosphorus oxide providing the photodarkening reducing effect, preferably in an amount of from about 1 to 30 mol %. A method for reducing a photodarkening effect in optical properties of an optically active glass including the step of introducing phosphorus oxide to the glass is also provided.