公开(公告)号:JPH08319396A
公开(公告)日:1996-12-03
申请号:JP13213896
申请日:1996-05-27
Applicant: BASF AG
Inventor: REEROFU BARUKU , CLAASSEN PETER , GRAALMANN ONNO , AAN DE MEULEN LEONARDUS , VISSEREN MARINUS
-
公开(公告)号:EP0744418A3
公开(公告)日:1997-12-29
申请号:EP96107842
申请日:1996-05-17
Applicant: BASF AG
Inventor: BALK ROELOF DR , CLAASSEN PETER , GRAALMANN ONNO DR , AAN DE MEULEN LEONARDUS , VISSEREN MARINUS
CPC classification number: C08J9/30 , C08F236/04 , C08J2309/10 , C08K3/22 , C08L13/02
-
公开(公告)号:DE102005037113A1
公开(公告)日:2007-02-08
申请号:DE102005037113
申请日:2005-08-03
Applicant: BASF AG
Inventor: WEISS AXEL , WEBER MANFRED , CLAASSEN PETER , RECK BERND
Abstract: The present invention relates to the use of a heat-curable aqueous composition comprising dispersed polymer particles of at least a) one polymer A1 comprising, 98-100% by weight of ethylenically unsaturated monomers A, it being possible for up to 20% by weight of the monomers A to comprise glycidyl and/or hydroxyl groups and/or amino/amido groups, and the polymer comprising, incorporated in the form of polymerized units,
-
公开(公告)号:AT260366T
公开(公告)日:2004-03-15
申请号:AT01936153
申请日:2001-03-29
Applicant: BASF AG
Inventor: SEYFFER HERMANN , LEMAN TITUS DR , CLAASSEN PETER , OLFERMANN KAI , WIRTH THOMAS , SCHMIDT-THUEMMES JUERGEN
Abstract: A process for impregnating base paper or fiber webs with an aqueous dispersion of a polymer of free-radically polymerizable compounds (monomers), which comprises from 0.1 to 5% by weight of the monomers being methacrylic acid.
-
公开(公告)号:AU6214601A
公开(公告)日:2001-10-23
申请号:AU6214601
申请日:2001-03-29
Applicant: BASF AG
Inventor: SEYFFER HERMANN , LEMAN TITUS , CLAASSEN PETER , OLFERMANN KAI , WIRTH THOMAS , SCHMIDT-THUMMES JURGEN
Abstract: A process for impregnating base paper or fiber webs with an aqueous dispersion of a polymer of free-radically polymerizable compounds (monomers), which comprises from 0.1 to 5% by weight of the monomers being methacrylic acid.
-
公开(公告)号:DK0744418T3
公开(公告)日:2001-04-23
申请号:DK96107842
申请日:1996-05-17
Applicant: BASF AG
Inventor: ROELOF DR BALK , CLAASSEN PETER , ONNO DR GRAALMANN , AAN DE MEULEN LEONARDUS , VISSEREN MARINUS
IPC: C08F2/24 , C08F2/38 , C08F220/12 , C08F236/04 , C08J9/00 , C08J9/30 , C08L9/10
-
公开(公告)号:AT199917T
公开(公告)日:2001-04-15
申请号:AT96107842
申请日:1996-05-17
Applicant: BASF AG
Inventor: BALK ROELOF DR , CLAASSEN PETER , GRAALMANN ONNO DR , AAN DE MEULEN LEONARDUS , VISSEREN MARINUS
IPC: C08F2/24 , C08F2/38 , C08F220/12 , C08F236/04 , C08J9/00 , C08J9/30 , C08L9/10
-
公开(公告)号:BR9709136A
公开(公告)日:1999-08-03
申请号:BR9709136
申请日:1997-04-24
Applicant: BASF AG
Inventor: CLAASSEN PETER , GRAALMANN ONNO , HORMUTH WOLFGANG ALOIS , MULLER-ENGEL KLAUS JOACHIM
Abstract: A process for producing dip-coated articles in which a heated moulding with an electrolyte adsorbing surface is dipped into an aqueous latex preparation, the latex of which is stabilised substantially by emulsifiers with anionic sulphonate groups and is heat-sensitised by a silicon-organic tenside having non-ionic polyether groups and a cloud temperature in the range from 30 to 40 DEG C.
-
公开(公告)号:DE59601259D1
公开(公告)日:1999-03-18
申请号:DE59601259
申请日:1996-11-27
Applicant: BASF AG
Inventor: CLAASSEN PETER , GRAALMANN ONNO DR , HORMUTH WOLFGANG ALOIS , VISSEREN MARINUS VISSEREN MARI
IPC: C08F2/22 , C08F2/24 , C08F36/04 , C08F236/04
Abstract: Process for preparing an aqueous polymer dispersion by radical aqueous emulsion polymerisation of a mixture of monomers having at least one ethylenically unsaturated group, the mixture containing at least 30 wt. % in total mixture of monomers (A) containing two conjugated ethylenically unsaturated double bonds, comprises (a) dividing the monomer mixture into n portions, where n is at least 2; (b) introducing the first monomer portion into the polymerisation reactor together with dispersing agent, radical polymerisation initiator and aqueous dispersing medium and polymerising in a first stage commencing at a polymerisation starting temperature TP1 of 0 degrees C ≤ TP1 ≤ 50 degrees C such that the temperature of the polymerisation mixture rises by at least 20 degrees C to a highest value of TP1H without exceeding 80 degrees C, and then holding the temperature constant within the range TP1H to TP1H-10 degrees C until the conversion U1 of monomer to polymer is at least 60 but at most 90 mol %, after which the polymerisation mixture is cooled to a polymerisation starting temperature TP2 where TP2 = TP1 plus or minus 10 degrees C and 0 degrees C ≤ TP2 ≤ 50 degrees C; (c) adding the second monomer portion and polymerising the monomer mixture present in the reactor in the presence of the polymer already formed, the dispersing agent and the polymerisation initiator in a second polymerisation stage commencing at the polymerisation starting temperature TP2 such that the temperature of the polymerisation mixture rises by at least 20 degrees C to a highest value of TP2H without exceeding 80 degrees C, and then holding the temperature constant within the range TP2H to TP2H-10 degrees C until the conversion U2 of monomer to polymer is at least 60 but at most 90 mol %, after which the polymerisation mixture is cooled to a polymerisation starting temperature TP3 where TP3 = TP1 plus or minus 10 degrees C and 0 degrees C ≤ TP3 ≤ 50 degrees C; (d) adding and polymerising the remaining n-2 portions of the monomer mixture successively in the same way as the second portion and (e) after the nth polymerisation stage, optionally continuing the polymerisation at a temperature of 0-50 degrees C to a total conversion Utot of monomers introduced to polymer of at least 95mol. %.
-
公开(公告)号:NO965167D0
公开(公告)日:1996-12-03
申请号:NO965167
申请日:1996-12-03
Applicant: BASF AG
Inventor: CLAASSEN PETER , GRAALMANN ONNO , HORMUTH WOLFGANG ALOIS , VISSEREN MARINUS
IPC: C08F2/22 , C08F2/24 , C08F36/04 , C08F236/04 , C08F
Abstract: Process for preparing an aqueous polymer dispersion by radical aqueous emulsion polymerisation of a mixture of monomers having at least one ethylenically unsaturated group, the mixture containing at least 30 wt. % in total mixture of monomers (A) containing two conjugated ethylenically unsaturated double bonds, comprises (a) dividing the monomer mixture into n portions, where n is at least 2; (b) introducing the first monomer portion into the polymerisation reactor together with dispersing agent, radical polymerisation initiator and aqueous dispersing medium and polymerising in a first stage commencing at a polymerisation starting temperature TP1 of 0 degrees C ≤ TP1 ≤ 50 degrees C such that the temperature of the polymerisation mixture rises by at least 20 degrees C to a highest value of TP1H without exceeding 80 degrees C, and then holding the temperature constant within the range TP1H to TP1H-10 degrees C until the conversion U1 of monomer to polymer is at least 60 but at most 90 mol %, after which the polymerisation mixture is cooled to a polymerisation starting temperature TP2 where TP2 = TP1 plus or minus 10 degrees C and 0 degrees C ≤ TP2 ≤ 50 degrees C; (c) adding the second monomer portion and polymerising the monomer mixture present in the reactor in the presence of the polymer already formed, the dispersing agent and the polymerisation initiator in a second polymerisation stage commencing at the polymerisation starting temperature TP2 such that the temperature of the polymerisation mixture rises by at least 20 degrees C to a highest value of TP2H without exceeding 80 degrees C, and then holding the temperature constant within the range TP2H to TP2H-10 degrees C until the conversion U2 of monomer to polymer is at least 60 but at most 90 mol %, after which the polymerisation mixture is cooled to a polymerisation starting temperature TP3 where TP3 = TP1 plus or minus 10 degrees C and 0 degrees C ≤ TP3 ≤ 50 degrees C; (d) adding and polymerising the remaining n-2 portions of the monomer mixture successively in the same way as the second portion and (e) after the nth polymerisation stage, optionally continuing the polymerisation at a temperature of 0-50 degrees C to a total conversion Utot of monomers introduced to polymer of at least 95mol. %.
-
-
-
-
-
-
-
-
-