COMPOSITE MOLDING OF SHOCK ABSORBING PROPYLENE POLYMER

    公开(公告)号:JPH05138784A

    公开(公告)日:1993-06-08

    申请号:JP34089691

    申请日:1991-12-24

    Applicant: BASF AG

    Abstract: PURPOSE: To make it possible to recycled use as well as obtain good durability, shock resistance, mechanical properties and surface property by constituting a composite molding using a propylene polymer as a main body and making a polymer adhere to both sides of a foamed core with a hot-melt adhesive layer. CONSTITUTION: This shock-absorbing propylene polymer composite molding comprises: (a) a layer with a thickness of 0.5 to 10 mm containing a propylene polymer having a melting point of 130 to 165 deg.C, (b) an intermediate layer with a thickness of 0.05 to 0.5 mm containing a hot-melt adhesive of olefin copolymer having a melting point of 90 to 140 deg.C as a main body, (c) a foamed layer with a thickness of 3 to 200 mm containing a propylene copolymer having a melting point of 125 to 155 deg.C as a main body and a density of 0.015 to 0.1 g/cm , (d) an intermediate layer with a thickness of 0.05 to 0.5 mm containing a hot-melt adhesive of olefin copolymer having a melting point of 90 to 140 deg.C as a main body, and (e) a layer with a thickness of 0.5 to 10 mm containing a propylene polymer having a melting point of 130 to 165 deg.C.

    2.
    发明专利
    未知

    公开(公告)号:NO177341B

    公开(公告)日:1995-05-22

    申请号:NO920295

    申请日:1992-01-22

    Applicant: BASF AG

    Abstract: Shock-absorbing propylene polymer composite moulded articles containing …… a. a layer of thickness 0.5 to 10 mm, containing a propylene polymer of melting point 130 to 165 DEG C, … b. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … c. a foam layer of thickness 3 to 200 mm having a density of 0.015 to 0.1 g/cm based on a propylene copolymer of melting point 125 to 155 DEG C, … d. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … e. a layer of thickness 0.5 to 10 mm containing a propylene polymer of melting point 130 to 165 DEG C. …

    3.
    发明专利
    未知

    公开(公告)号:DE59103836D1

    公开(公告)日:1995-01-26

    申请号:DE59103836

    申请日:1991-03-02

    Applicant: BASF AG

    Abstract: A construction element having a virtually rectangular force-movement characteristic, consisting of an elongated polymer foam body (1) of rectangular cross-section having the rectangular sides a and b, and having a recess (2), which extends over the complete longitudinal extent and on one side of the body, of width d and of height c, the said dimensions satisfying specific equations. … …

    4.
    发明专利
    未知

    公开(公告)号:NO920295L

    公开(公告)日:1992-07-24

    申请号:NO920295

    申请日:1992-01-22

    Applicant: BASF AG

    Abstract: Shock-absorbing propylene polymer composite moulded articles containing …… a. a layer of thickness 0.5 to 10 mm, containing a propylene polymer of melting point 130 to 165 DEG C, … b. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … c. a foam layer of thickness 3 to 200 mm having a density of 0.015 to 0.1 g/cm based on a propylene copolymer of melting point 125 to 155 DEG C, … d. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … e. a layer of thickness 0.5 to 10 mm containing a propylene polymer of melting point 130 to 165 DEG C. …

    6.
    发明专利
    未知

    公开(公告)号:MX9200249A

    公开(公告)日:1992-10-01

    申请号:MX9200249

    申请日:1992-01-21

    Applicant: BASF AG

    Abstract: Shock-absorbing propylene polymer composite moulded articles containing …… a. a layer of thickness 0.5 to 10 mm, containing a propylene polymer of melting point 130 to 165 DEG C, … b. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … c. a foam layer of thickness 3 to 200 mm having a density of 0.015 to 0.1 g/cm based on a propylene copolymer of melting point 125 to 155 DEG C, … d. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … e. a layer of thickness 0.5 to 10 mm containing a propylene polymer of melting point 130 to 165 DEG C. …

    SHOCK-ABSORBING PROPYLENE POLYMER COMPOSITE MOLDINGS

    公开(公告)号:CA2059257A1

    公开(公告)日:1992-07-24

    申请号:CA2059257

    申请日:1992-01-15

    Applicant: BASF AG

    Abstract: O.Z. 0050/42154 A shock-absorbing propylene polymer composite molding contains a. a layer with a thickness of from 0.5 to 10 mm which contains a propylene polymer having a melting point of from 130 to 165.degree.C, b. an intermediate layer with a thickness of from 0.05 to 0.5 mm comprising a hot-melt adhesive based on an olefin copolymer having a melting point of from 90 to 140.degree.C, c. a foam layer with a thickness of from 3 to 200 mm and a density of from 0.015 to 0.1 g/cm3 based on a propylene copolymer having a melting point of from 125 to 155.degree.C, d. an intermediate layer with a thickness of from 0.05 to 0.5 mm comprising a hot-melt adhesive based on an olefin copolymer having a melting point of from 90 to 140.degree.C, e. a layer with a thickness of from 0.5 to 10 mm which contains a propylene polymer having a melting point of from 130 to 165.degree.C.

    10.
    发明专利
    未知

    公开(公告)号:AT164345T

    公开(公告)日:1998-04-15

    申请号:AT91122249

    申请日:1991-12-27

    Applicant: BASF AG

    Abstract: Shock-absorbing propylene polymer composite moulded articles containing …… a. a layer of thickness 0.5 to 10 mm, containing a propylene polymer of melting point 130 to 165 DEG C, … b. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … c. a foam layer of thickness 3 to 200 mm having a density of 0.015 to 0.1 g/cm based on a propylene copolymer of melting point 125 to 155 DEG C, … d. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … e. a layer of thickness 0.5 to 10 mm containing a propylene polymer of melting point 130 to 165 DEG C. …