Abstract:
The present disclosure is directed to a method of making an optical fiber with improved bend performance, the optical fiber having a core and at least one cladding layer, and a chlorine content in the in the last layer of the at least one cladding layer that is greater than 500 ppm by weight. The fiber is prepared using a mixture of a carrier gas, a gaseous chlorine source material and a gaseous reducing agent during the sintering of the last or outermost layer of the at least one cladding layer. The inclusion of the reducing gas into a mixture of the carrier gas and gaseous chlorine material reduces oxygen-rich defects that results in at least a 20% reduction in TTP during hydrogen aging testing.
Abstract:
Ultralow expansion titania-silica glass. The glass has high hydroxyl content and optionally include one or more dopants. Representative optional dopants include boron, alkali elements, alkaline earth elements or metals such as Nb, Ta, Al, Mn, Sn Cu and Sn. The glass is prepared by a process that includes steam consolidation to increase the hydroxyl content. The high hydroxyl content or combination of dopant(s) and high hydroxyl content lowers the fictive temperature of the glass to provide a glass having a very low coefficient of thermal expansion (CTE), low fictive temperature (Tf), and low expansivity slope.
Abstract:
A method for adjusting an etchability of a first borosilicate glass by heating the first borosilicate glass; combining the first borosilicate glass with a second borosilicate glass to form a composite; and etching the composite with an etchant. A material having a protrusive phase and a recessive phase, where the protrusive phase protrudes from the recessive phase to form a plurality of nanoscale surface features, and where the protrusive phase and the recessive phase have the same composition.
Abstract:
The invention relates to a multimode optical fiber having a refractive index profile, comprising a light-guiding core surrounded by one or more cladding layers. The present invention furthermore relates to an optical communication system comprising a transmitter, a receiver and a multimode optical fiber.
Abstract:
Methods for making active laser fibers include the production of an optical fiber with disturbed (or deviated) cylindrical symmetry on the glass surface of the fiber. The methods include a preform containing a central core made of glass. In one embodiment, the preform is circular and surrounded by additional glass rods and an outer glass jacket tube. In a first alternative embodiment, this preform is merged during fiber drawing. In a second alternative embodiment, the preform merged in a process forming a compact glass body with disturbed cylindrical symmetry. This compact preform is drawn into a fiber under conditions maintaining the disturbed cylindrical symmetry.
Abstract:
According to one example of the invention an optical fiber comprises: (i) silica based, rare earth doped core having a first index of refraction n1; (ii) at least one silica based cladding surrounding the core and having a second index of refraction n2, such that n1>n2; wherein at least one of the core or cladding is doped with Al2O3, such that the ratio of max wt % to min wt % of Al2O3 concentration is less than 2:1.
Abstract translation:根据本发明的一个示例,光纤包括:(i)具有第一折射率n1的二氧化硅基稀土掺杂的核; (ii)至少一个围绕所述芯并且具有第二折射率n2的基于二氧化硅的包层,使得n1> n2; 其中所述芯或包层中的至少一个掺杂有Al 2 O 3,使得最大wt%与Al 2 O 3浓度的最小重量%的比率小于2:1。
Abstract:
The invention relates to an optical fiber, in particular a laser fiber, containing a doped glass fiber core (1) and cladding (2) around the latter with a refraction index profile which decreases outwards from the fiber core. The optical fiber is distinguished by at least one intermediate layer (3, 4, 5) being disposed between the glass fiber core and the cladding to reduce the mechanical tension therebetween. In one advantageous embodiment, the intermediate layer is doped in such a way as to ensure a stepped mechanical tension distribution between the glass fiber core and the cladding, and is co-doped in such a way as to reduce the refractive index and counteract the refraction index-increasing effect of the intermediate layer doping. The invention further relates to an application of at least one doped barrier layer to a core region during preparation of the preform to avoid diffusion of special core dopants from the core during the collapse process, and to allow the diffusion of special dopants between the barrier layer and the core layer.
Abstract:
An optical fiber comprising: (i) a silica based passive core having a first index of refraction n1; (ii) a silica based cladding surrounding the core and having a second index of refraction n2, such that n1>n2, said cladding having at least one stress rod and at least one air hole extending longitudinally through the length of said optical fiber; and (iii) wherein said optical fiber supports a single polarization mode or poses polarization maintaining properties within the operating wavelength range.
Abstract:
According to one example of the invention an optical fiber comprises: (i) silica based, rare earth doped core having a first index of refraction n1; (ii) at least one silica based cladding surrounding the core and having a second index of refraction n2, such that n1>n2; wherein at least one of the core or cladding is doped with Al2O3, such that the ratio of max wt % to min wt % of Al2O3 concentration is less than 2:1.
Abstract translation:根据本发明的一个示例,光纤包括:(i)具有第一折射率n 1的二氧化硅基稀土掺杂的核; (ii)至少一个二氧化硅基包层,其围绕所述芯并具有第二折射率n 2 2,使得n 1/2 2 n 2 ; 其中所述芯或包层中的至少一个掺杂有Al 2 O 3 3,使得Al 2 O 3的最大重量%与最小重量%的比例< / 3 3 3浓度小于2:1。
Abstract:
In one aspect, the invention features a fiber waveguide having a waveguide axis, including a first portion extending along the waveguide axis, and a second portion different from the first portion extending along the waveguide axis surrounding the first portion, wherein at least one of the first and second portions comprises a chalcogenide glass selected from the group consisting of Selenium chalcogenide glasses and Tellurium chalcogenide glasses, both the first and second portions have a viscosity greater than 103 Poise at some temperature, T, and the fiber waveguide is a photonic crystal fiber.