    Abstract: A polypropylene resin composition is provided to improve melt tension, fluidity and cooling velocity, to prevent the generation of swirl mark in case of injection molding and to enhance the foaming rate and impact resistance of foamed product. A polypropylene resin composition comprises 5-20 wt% of a polypropylene master batch which comprises a propylene homopolymer, a propylene-ethylene copolymer or their mixture; 35-60 wt% of a high crystalline polypropylene resin having a melt index of 60-100 g/10 min (230 deg.C) and an isotacticity of 99-100; 5-15 wt% of an ethylene-styrene copolymer rubber which contains 20-50 wt% of styrene and has a polydispersity index of 8-12 and a melt index of 10-30 g/10 min (230 deg.C); 5-15 wt% of an ethylene-alpha-olefin copolymer rubber; and an inorganic filler.

    Abstract translation: 提供聚丙烯树脂组合物以改善熔体张力,流动性和冷却速度,以防止在注射成型的情况下产生旋转痕迹,并提高发泡产品的起泡速率和抗冲击性。 聚丙烯树脂组合物包含5-20重量%的聚丙烯母料,其包含丙烯均聚物,丙烯 - 乙烯共聚物或它们的混合物; 35-60重量%的熔融指数为60-100克/ 10分钟(230℃)和等规度为99-100的高结晶聚丙烯树脂; 5-15重量%的乙烯 - 苯乙烯共聚物橡胶,其含有20-50重量%的苯乙烯,多分散指数为8-12,熔体指数为10-30克/ 10分钟(230℃); 5-15重量%的乙烯-α-烯烃共聚物橡胶; 和无机填料。

    인공신경망을 이용한 자동차 시트표피재의 촉감 평가 방법및 시스템
    12.
    发明公开
    인공신경망을 이용한 자동차 시트표피재의 촉감 평가 방법및 시스템 有权
    使用人工神经网络的汽车座椅的手术感测的测量过程和系统

    公开(公告)号:KR1020070041806A

    公开(公告)日:2007-04-20

    申请号:KR1020050097296

    申请日:2005-10-17

    CPC classification number: B60N2/58

    Abstract: 본 발명은 인공신경망을 이용한 자동차 시트표피재의 촉감 평가 방법 및 시스템에 관한 것이다.
    본 발명은 자동차 시트표피재의 역학적 및 열ㆍ생리적 특성을 측정계로 측정하여 물리량을 취득한 후, 이를 사람이 느끼는 촉감의 양으로 전환하기 위해 통계적 회귀모델을 이용함으로써, 피혁(Leather)의 경우 밀림에 대한 저항감(Sticky), 유연한(Soft), 탱글탱글한(Elastic), 서늘한(Coolness to the touch), 온습한(Thermal and humid) 촉감을, 직물(Cloth)의 경우 유연한(Soft), 탱글탱글한(Elastic), 풍성한(Voluminous), 매끄러운(Smooth), 서늘한(Coolness to the touch), 온습한(Thermal and humid)의 촉감을 정량적으로 평가할 수 있고, 직물(Cloth)의 경우 유연한(Soft), 탱글탱글한(Elastic), 풍성한(Voluminous), 매끄러운(Smooth), 서늘한(Coolness to the touch), 온습한(Thermal and humid)의 촉감을 정량적으로 평가할 수 있으며, 최종적으로 인공신경망 모델을 거쳐 스포티하고, 하이-클래스의 촉감을 정량적으로 평가할 수 있도록 한 인공신경망을 이용한 자동차 시트표피재의 촉감 평가 방법 및 시스템을 제공하고자 한 것이다.
    자동차, 시트표피재, 촉감, 인공신경망, 통계적 회귀모델

    친환경 저수축 천연가죽의 제조방법
    13.
    发明授权
    친환경 저수축 천연가죽의 제조방법 有权
    环保低收缩天然皮革的制造方法

    公开(公告)号:KR100706407B1

    公开(公告)日:2007-04-10

    申请号:KR1020060046144

    申请日:2006-05-23

    Abstract: 본 발명은 친환경 저수축 천연가죽의 제조방법에 관한 것으로서, 더욱 상세하게는 준비, 유성, 염색 및 도장단계로 이루어진 천연가죽의 제조 시, 상기 유성단계에서 알데히드계 탄닝제를 사용하고, 염색단계에서 베지터블계 리탄닝제를 선택 사용하여, 유해물질 방출을 배제시키며, 내열, 내열 및 내습 수축율이 우수한 천연가죽의 제조방법에 관한 것이다.
    천연가죽, 수축, 탄닝제, 크롬, 알데하이드

    Abstract translation: 另外,本发明环保型低轮廓涉及一种天然皮革的制造方法,并且更具体地,涉及制备,油,染色,并在制造由涂布工序,采用在油相中的基于醛的碳ningje皮革,在染色工序 使用基于利坦ningje所选蔬菜,sikimyeo排除释放的有害物质,一种制造耐热,耐热和耐湿的皮革的收缩的方法是优异的。

    자동차 내장재 표피재용 폴리프로필렌계 수지 조성물
    14.
    发明授权
    자동차 내장재 표피재용 폴리프로필렌계 수지 조성물 有权
    一种汽车内饰材料用聚丙烯树脂组合物

    公开(公告)号:KR100551787B1

    公开(公告)日:2006-02-13

    申请号:KR1020040047800

    申请日:2004-06-24

    Abstract: 본 발명은 자동차 내장재 표피재용 폴리프로필렌계 수지 조성물에 관한 것으로, 더욱 상세하게는 폴리프로필렌계 공중합체, 에틸렌-옥텐 고무와 에틸렌-α-올레핀 공중합체 고무에 가공유(Process Oil) 및 폴리프로필렌 왁스를 적정 함량으로 마스터 배치화하여 고무류의 함량이 높음에도 불구하고 고무 성분의 가교없이 사출 성형성이 우수할 뿐만 아니라 저온 충격성, 내열성이 우수하고 냄새가 없는 자동차 내장재 인스트루먼트 판넬(Instrument Panel, 이하 인판넬) 표피재, 도어트림 표피재 또는 필라류 표피재로 이용 가능한 폴리프로필렌계 수지 조성물에 관한 것이다.
    폴리프로필렌계 공중합체, 에틸렌-α-올레핀 공중합체 고무, 폴리프로필렌 왁스, 사출 성형, 자동차 내장 표피재

    분체 성형용 열가소성 엘라스토머 조성물
    16.
    发明授权
    분체 성형용 열가소성 엘라스토머 조성물 有权
    분체성형용열가소성엘라스토머조성분

    公开(公告)号:KR100448144B1

    公开(公告)日:2004-09-10

    申请号:KR1020010059755

    申请日:2001-09-26

    Abstract: PURPOSE: Provided is an olefin-based thermoplastic elastomer composition for forming powder, which is excellent in melt fluidity, tensile strength, folded-part restoring ability, and properties and can be applied to the interior material and the coating material of cars. CONSTITUTION: The thermoplastic elastomer composition contains 100pts.wt. of a polypropylene resin having a melt index of 50-300g/10min(ASTM D 1238, 230deg.C, 2.16kg), 5-150pts.wt. of a propylene-ethylene copolymer resin having a melt index of 3-50g/10min(230deg.C, 2.16kg) and a shore D hardness of less than 40(ASTM D 2240), 50-200pts.wt. of a hydrogenated styrene butadiene rubber having a melt index of more than 5g/10min(230deg.C, 2.16kg) and containing 5-20% of styrene, and 50-200pts.wt. of an ethylene-octene copolymer elastomer having Mooney viscosity of 1-10(ML1+4, ASTM D 927, 121deg.C) and a shore A hardness of less than 80(ASTM D 2240).

    Abstract translation: 目的:提供一种用于形成粉末的烯烃基热塑性弹性体组合物,其具有优异的熔体流动性,拉伸强度,折叠部分恢复能力和性能,并可应用于汽车的内部材料和涂层材料。 构成:热塑性弹性体组合物含有100pts.wt。 熔体指数为50-300g / 10min(ASTM D 1238,230℃,2.16kg)的聚丙烯树脂,5-150pts.wt。 熔体指数为3-50g / 10min(230℃,2.16kg)且肖氏D硬度小于40(ASTM D 2240)的丙烯 - 乙烯共聚物树脂,50-200pts.wt。 的熔体指数大于5g / 10min(230℃,2.16kg)并含有5-20%苯乙烯和50-200pts.wt的氢化苯乙烯丁二烯橡胶。 的门尼粘度为1-10(ML1 + 4,ASTM D927,121℃)和肖氏A硬度小于80(ASTM D 2240)的乙烯 - 辛烯共聚物弹性体。

    분체 성형용 열가소성 엘라스토머 조성물
    17.
    发明公开
    분체 성형용 열가소성 엘라스토머 조성물 有权
    用于形成粉末的热塑性弹性体组合物

    公开(公告)号:KR1020030026673A

    公开(公告)日:2003-04-03

    申请号:KR1020010059755

    申请日:2001-09-26

    Abstract: PURPOSE: Provided is an olefin-based thermoplastic elastomer composition for forming powder, which is excellent in melt fluidity, tensile strength, folded-part restoring ability, and properties and can be applied to the interior material and the coating material of cars. CONSTITUTION: The thermoplastic elastomer composition contains 100pts.wt. of a polypropylene resin having a melt index of 50-300g/10min(ASTM D 1238, 230deg.C, 2.16kg), 5-150pts.wt. of a propylene-ethylene copolymer resin having a melt index of 3-50g/10min(230deg.C, 2.16kg) and a shore D hardness of less than 40(ASTM D 2240), 50-200pts.wt. of a hydrogenated styrene butadiene rubber having a melt index of more than 5g/10min(230deg.C, 2.16kg) and containing 5-20% of styrene, and 50-200pts.wt. of an ethylene-octene copolymer elastomer having Mooney viscosity of 1-10(ML1+4, ASTM D 927, 121deg.C) and a shore A hardness of less than 80(ASTM D 2240).

    Abstract translation: 目的:提供一种用于形成粉末的烯烃类热塑性弹性体组合物,其熔融流动性,拉伸强度,折叠部分恢复能力和性能优异,并且可以应用于汽车的内部材料和涂料。 构成:热塑性弹性体组合物含有100pts.wt。 的熔体指数为50〜300g / 10min的聚丙烯树脂(ASTM D 1238,230℃,2.16kg),5-150pts.wt。 的熔体指数为3-50g / 10min(230℃,2.16kg),肖氏D硬度小于40的丙烯 - 乙烯共聚物树脂(ASTM D 2240),50-200pts.wt。 的熔体指数大于5g / 10min(230℃,2.16kg)并含有5-20%苯乙烯和50-200pts.wt。的氢化苯乙烯丁二烯橡胶。 的门尼粘度为1-10(ML1 + 4,ASTM D 927,121deg.C)和Shore A硬度小于80(ASTM D 2240)的乙烯 - 辛烯共聚物弹性体。

    도전성 접착제 및 이를 이용한 복합소재의 접합방법
    20.
    发明授权
    도전성 접착제 및 이를 이용한 복합소재의 접합방법 有权
    导电粘合剂和使用该粘合剂的复合材料的粘合方法

    公开(公告)号:KR101836566B1

    公开(公告)日:2018-03-08

    申请号:KR1020150067966

    申请日:2015-05-15

    Abstract: 본발명은도전성접착제및 이를이용한복합소재의접합방법에관한것으로, 보다상세하게는 1 액형접착제또는 2 액형접착제에전도성섬유를혼합함으로써전도성이우수하여통전이보다원활히이루어지며, 접착성능및 온도변화에따른내구성을향상시킬수 있으며, 이를이용하여루프와같은복합소재부품의차체접합또는후드, 도어, 휀더, 트렁크리드복합소재부품과스틸부품의접합등에활용가능한도전성접착제및 이를이용한복합소재의접합방법에관한것이다.

    Abstract translation: 本发明是一种导电性粘接剂,并通过在粘合剂或两部分粘合剂的导电性纤维混合制成yiwoosu使用相同的,更具体地单组分涉及的复合材料的接合方法,从而平稳比通电的导电性,根据粘着性和温度 它可以提高耐久性,根据在导电性粘接剂使用的可以采取复合部件,诸如环或罩,门,挡泥板,行李箱盖复合部件和所述钢部件的接合和使用相同的这样的车体接合的优点这种复合材料的接合方法。 会的。

Patent Agency Ranking