Abstract:
The present disclosure relates to a filled polyolefin composition comprising butene-1 copolymers having high melt flow and an inorganic filler, said compositions being endowed with a good balance between the melt flow rate and the elastic properties, and being suitable for carpet backing.
Abstract:
A butene-1 polymer having: a) a Melt Flow Rate value of from 20 to less than 100 g/10 min., measured according to ISO 1133 at 190°C with a load of 2.16 kg; • b) an intrinsic viscosity (IV) measured in tetrahydronaphthalene (THN) at 135°C equal to lower than 0.95 dl/g; • c) a Mw/Mn value equal to or lower than 3.5, the lower limit being of 1.5; • d) a Mz value of 180,000 g/mol or higher; • e) a comonomer content, when comonomer is present, of up to 5% by weight.
Abstract:
A butene-1 polymer having: a) a Melt Flow Rate value of from 100 to 300 g/10 min., measured according to ISO 133 at 190°C with a load of 2.16 kg; b) an intrinsic viscosity (IV) measured in tetrahydronaphthalene (THN) at 135°C equal to lower than 0.70 dl/g; c) a Mw/Mn value equal to or lower than 2.8; d) a Mz value of 90,000 g/mol or higher; e) a comonomer content, when comonomer is present, of up to 10% by mole.
Abstract:
A butene-1 polymer composition having MFR values of from 400 to 2000 g/10 min, measured according to ISO 1133 at 190°C with a load of 2.16 kg, comprising: A) a butene-1 homopolymer or a copolymer of butene-1 with one or more comonomers selected from ethylene and higher alpha-olefins, having a copolymerized comonomer content of up to 5% by mole; B) a copolymer of butene-1 with one or more comonomers selected from ethylene and higher alpha-olefins, having a copolymerized comonomer content of from 6% to 25% by mole; said composition having a total copolymerized comonomer content from 5% to 18% by mole, referred to the sum of A) and B), and a content of fraction soluble in xylene at 0°C of 65% by weight or more, determined on the total weight of A) and B).
Abstract:
A polyolefin composition, particularly suited for preparing gaskets for closures, comprising: A) from 60 to 89% by weight of a copolymer of butene-1 with ethylene having a copolymerized ethylene content of up to 18% by mole and no melting peak detectable at the DSC at the second heating scan; B) from 11 to 40% by weight of an ethylene polymer having density of from 0.900 to 0.970 g/cm3, measured according to ISO 1183 at 23°C; wherein the amounts of A) and B) are referred to the total weight of A) + B).
Abstract translation:一种聚烯烃组合物,特别适合于制备用于封闭的垫圈的聚烯烃组合物,其包含:A)60-89重量%的丁烯-1与乙烯的共聚物,共聚乙烯含量最高达18% 在第二次加热扫描时在DSC处没有可检测到的熔融峰; B)11至40重量%的密度为0.900至0.970g / cm 3的乙烯聚合物,其根据ISO 1183在23℃下测量; 其中A)和B)的量是指A)+ B)的总重量
Abstract:
A hot melt adhesive polyolefin composition comprising a high melt flow butene-1 copolymer suitable to be used as a glue in paper and packaging industry, in furniture manufacture e.g. for edgebands, particularly square edges and softforming, for paneling in high moisture environments, particularly suitable for acting as a glue in tufted or needle punched carpets.
Abstract:
A polymer composition comprising: A) from 70 wt% to 95 wt% of a propylene-based polymer composition comprising: a) from 15 wt% to 35 wt% of a copolymer of propylene and 1 -hexene containing from 6.2 to 8.5 % by weight, of 1-hexene derived units b) from 15 wt% to 35 wt% of a copolymer of propylene and 1 -hexene containing from 10.4 wt% to 14.5 wt%, of 1-hexene derived units c) from 38 wt% to 68 wt% of a propylene ethylene copolymerthe sum of the amount of a), b) and c) being 100; B) from 5.0 wt% to 30.0 wt% of a copolymer of 1 -butene and ethylene containing from 3.0 wt% to 4.2 wt% of ethylene derived units; the sum of the amounts of A) and B) being 100 wt%.
Abstract:
A butene-1 polymer composition having MFR values of from 100 to 300 g/10 min., measured according to ISO 1133 at 190°C with a load of 2.16 kg, comprising: A) a butene-1 homopolymer or a copolymer of butene-1 with one or more comonomers selected from ethylene and higher alpha-olefins, having a copolymerized comonomer content of up to 5% by mole; B) a copolymer of butene-1 with one or more comonomers selected from ethylene and higher alpha-olefins, having a copolymerized comonomer content of from 6% to 20% by mole; said composition having a total copolymerized comonomer content from 4% to 15% by mole, referred to the sum of A) and B), and a content of fraction soluble in xylene at 0°C of 75% by weight or less, determined on the total weight of A) and B).
Abstract:
A butene-1 polymer composition having MFR values of from 20 to less than 100 g/10 min., measured according to ISO 1133 at 190°C with a load of 2.16 kg, comprising: A) a butene-1 homopolymer or a copolymer of butene-1 with one or more comonomers selected from ethylene and higher alpha-olefins, having a copolymerized comonomer content of up to 5% by mole; B) a copolymer of butene-1 with one or more comonomers selected from ethylene and higher alpha-olefins, having a copolymerized comonomer content of from 6% to 20% by mole; said composition having a total copolymerized comonomer content from 4% to 15% by mole, referred to the sum of A) and B), and a content of fraction soluble in xylene at 0°C of 75% by weight or less, determined on the total weight of A) and B).
Abstract:
A polyolefin composition having a melting enthalpy ΔH fus , measured by DSC at the second heating scan, of from 7 to 30 J/g, comprising: A) from 63 to 78% by weight of a copolymer of butene-1 with ethylene having a copolymerized ethylene content of up to 18% by mole and no melting peak detectable at the DSC at the second heating scan; B) from 22 to 37% by weight of (i) a propylene homopolymer, or (ii) a propylene copolymer, or (iii) a mixture of two or more of (i) and (ii), having a melting temperature T m , measured by DSC at the second heating scan, of from 130°C to 165°C; wherein the amounts of A) and B) are referred to the total weight of A) + B).