Abstract:
The present disclosure relates to a polyolefin-based hot melt adhesive composition endowed, with a good balance between thermal properties, crystallinity, viscosity and adhesive properties, comprising: (A) 25-75 wt.% of a copolymer of butene- 1 with a Melt Flow Rate, measured according to 1SO 1133 (190°C, 2,16kg), higher than 1500; and (B) 75-25 wt.% of at least one additional component selected from among waxes, resins, plasticizers, additional polymers and mixtures thereof, wherein the amounts of A) and B) are referred to the total weight of A) + B).
Abstract:
The present disclosure relates to a polyolefin-based hot melt adhesive composition endowed, with a good, balance between thermal properties, crystallinity, viscosity and adhesive properties, comprising: (A) 28-75 wt.% of a copolymer of butene-1 with Melt Flow Rate values, measured according to ISO 1133 (190°C, 2,16kg), of from 200 to 1500 g/10min.; and (B) 25-72 wt.% of at least one additional component selected from among waxes, resins, plasticizers, additional polymers and mixtures thereof, wherein the amounts of A) and B) are referred to the total weight of A) + B).
Abstract:
A polymer composition comprising: A) from 70 wt% to 95 wt% of a propylene ethylene copolymer having: - an ethylene derived units content measured by 13C NMR ranging from 2.2 wt% and 9.8 wt% B) from 5.0 wt% to 30.0 wt% of a copolymer of 1-butene and ethylene containing from 3.0 wt% to 4.2 wt% of ethylene derived units the sum of the amounts of A) and B) being 100 wt%.
Abstract:
The present disclosure relates to a polyolefin composition having a high balance of melt flowability and impact resistance, comprising: A) from 88% to 99% by weight of an ethylene polymer having MIP of equal to or higher than 5 g/10 min, where MIP is the melt flow index at 190°C with a load of 5 kg, determined according to 1133-2:2011; B) from 1% to 12% by weight of a butene- 1 polymer having MIE of equal to or higher than 800 g/10 min., where MIE is the melt flow index at 190°C with a load of 2.16 kg, determined according to 1133-2:2011; wherein the amounts of A) and B) are referred to the total weight of A) + B).
Abstract:
A butene-1 polymer composition having MFR values of from 400 to 2000 g/10 min, measured according to ISO 1133 at 190°C with a load of 2.16 kg, comprising: A) a butene-1 homopolymer or a copolymer of butene-1 with one or more comonomers selected from ethylene and higher alpha-olefins, having a copolymerized comonomer content of up to 5% by mole; B) a copolymer of butene-1 with one or more comonomers selected from ethylene and higher alpha-olefins, having a copolymerized comonomer content of from 6% to 20% by mole; said composition having a total copolymerized comonomer content from 4% to 15% by mole, referred to the sum of A) and B), and a content of fraction soluble in xylene at 0°C of 60% by weight or less, determined on the total weight of A) and B).
Abstract:
The present disclosure relates to copolymer of butene-1 with hexene-1, particularly suited for the preparation of pipes, having the following features: 1) a content of hexene-1 comonomer units from 2 to 4% by weight; 2) a melting temperature TmI equal to or higher than 115°C.
Abstract:
A polyolefin composition comprising: a) from 85% to 98% by weight of a composition comprising: A) a copolymer of butene-1 with ethylene having a copolymerized ethylene content of up to 18% by mole and no melting peak detectable at the DSC at the second heating scan; and B) an inorganic filler; the B)/A) weight ratio being from 0.3 to 4; b) from 2% to 15% by weight of an additional polyolefin different from A).
Abstract:
A gasket for closures comprising a polyolefin composition (I) containing A) from 25 to 62% by weight of a copolymer of butene-1 with ethylene having a copolymerized ethylene content of up to 18% by mole and no melting peak detectable at the DSC at the second heating scan; B) from 38 to 75% by weight, of (i) a propylene homopolymer, or (ii) a propylene copolymer, or (iii) a mixture of two or more of (i) and (ii), having a melting temperature T m , measured by DSC at the second heating scan, of from 130°C to 165°C; wherein the amounts of A) and B) are referred to the total weight of A) + B).
Abstract:
Extruded or molded profiles comprising a polyolefin composition consisting of 85% by weight or more of a copolymer of 1-butene with ethylene (A) having an ethylene copolymerized content up to 18 % bymol, and having Mw/Mn lower than 3, hardness shore A (measured according to ISO 868) lower than 90, no melting point (TmII) detectable at the DSC after cancelling the thermal history, melting enthalpy (ΔHf), measured by DSC after 10 days of aging at room temperature,comprised between 4 and 15 J/g; and up to 15% by weight of a propylene copolymer or a composition of copolymers of propylene (B) having a melting point from about 26°C to 200°C, isotactic index greater than 90%.
Abstract:
The present disclosure relates to a butene-1 polymer composition, particularly suited for the preparation of pipes, comprising: A) from 97.5% to 99.85% by weight, with respect to the total weight of A) and B), of a butene-1 polymer or polymer composition; B) from 0.15% to 2.5% by weight, with respect to the total weight of A) and B), of talc in form of particles having a volume based particle diameter distribution Dv (0.95) of 45 µm or lower; and, optionally C) from 0.01% to 2% by weight of an ethylene polymer; the amount of C) being referred to the total weight of A) + B) + C), which amounts to 100%.