Impact-resistant modified polyester comprising hyperbranched polyesters/polycarbonates

    公开(公告)号:AU2005274504A1

    公开(公告)日:2006-02-23

    申请号:AU2005274504

    申请日:2005-08-02

    Applicant: BASF AG

    Abstract: Thermoplastic molding compositions, comprising A) from 10 to 98% by weight of at least one thermoplastic polyester, B) from 0.01 to 50% by weight of B1) at least one highly branched or hyperbranched polycarbonate with an OH number of from 1 to 600 mg KOH/g of polycarbonate (to DIN 53240, Part 2), or B2) at least one highly branched or hyperbranched polyester of AxBy type, where x is at least 1.1 and y is at least 2.1, or a mixture of these, C) from 1 to 40% by weight of an impact-modifying polymer, D) from 0 to 60% by weight of other additives, where the total of the percentages by weight of components A) to D) is 100%.

    16.
    发明专利
    未知

    公开(公告)号:BRPI0519853A2

    公开(公告)日:2009-08-18

    申请号:BRPI0519853

    申请日:2005-12-31

    Applicant: BASF AG

    Abstract: Thermoplastic molding compositions, comprising A) from 10 to 98.9% by weight of at least one thermoplastic polyester, B) from 0.01 to 50% by weight of B1) at least one highly branched or hyperbranched polycarbonate or B2) at least one highly branched or hyperbranched polyester of AxBy type, where x is at least 1.1 and y is at least 2.1 or a mixture of these C) from 0.1 to 10% by weight of at least one epoxidized naturally occurring oil or fatty acid ester, or a mixture of these, and D) from 0 to 60% by weight of other additives, where the total of the percentages by weight of components A) to D) is 100%.

    17.
    发明专利
    未知

    公开(公告)号:DE502005002777D1

    公开(公告)日:2008-03-20

    申请号:DE502005002777

    申请日:2005-10-08

    Applicant: BASF AG

    Abstract: Thermoplastic molding compositions, comprising A) from 10 to 98% by weight of at least one thermoplastic polymer, B) from 0.01 to 50% by weight of B1) at least one highly branched or hyperbranched polycarbonate with an OH number of from 1 to 600 mg KOH/g of polycarbonate (to DIN 53240, part 2), or B2) at least one highly branched or hyperbranched polyester of AxBy type, where x is at least 1.1 and y is at least 2.1, or a mixture of these, C) from 1 to 30% by weight of a flame retardant combination composed of, based on 100% by weight of C), C1) from 20 to 99% by weight of a halogen-containing flame retardant, C2) from 1 to 80% by weight of an antimony oxide, D) from 0 to 60% by weight of other additives, where the total of the percentages by weight of components A) to D) is 100%.

    19.
    发明专利
    未知

    公开(公告)号:DE502005002117D1

    公开(公告)日:2008-01-10

    申请号:DE502005002117

    申请日:2005-07-14

    Applicant: BASF AG

    Abstract: A thermoplastic molding composition comprising A) from 10 to 99.99% by weight of at least one thermoplastic polyester, B) from 0.01 to 50% by weight of a mixture composed of B1) at least one highly branched or hyperbranched polycarbonate having an OH number of from 1 to 600 mg KOH/g of polycarbonate (to DIN 53240, Part 2), and B2) at least one highly branched or hyperbranched polyester of A x B y type, where x is at least 1.1 and y is at least 2.1, and C) from 0 to 60% by weight of other additives, where the total of the percentages by weight of components A) to C) is 100%.

    PROCESO CONTINUO PARA PREPARAR ARILATOS DE POLIALQUILENO CON POLIESTERES Y/O POLICARBONATOS HIPERRAMIFICADOS.

    公开(公告)号:MX2007000077A

    公开(公告)日:2007-03-28

    申请号:MX2007000077

    申请日:2005-07-19

    Applicant: BASF AG

    Abstract: Un proceso continuo para la preparacion de arilatos A) de polialquileno que comprende polimeros B) altamente ramificados o hiperramificados y, si es apropiado, que comprende lubricantes C), esterificando o transesterificando un acido dicarboxulico aromatico o su ester o derivados de formacion de ester, con un exceso molar de un compuesto dihidroxi alifatico, y policondensando el producto de transesterificacion o esterificacion resultante, que comprende, despues de lograr cuando menos 80% del numero de viscosidad deseado, anadir el componente B) y tambien, si es apropiado, C) a la fusion de polimero y, si es apropiado, condensar posteriormente la fusion y luego descargar, enfriar y granularla, y tambien usando, como componente B), cuando menos un policarbonato Bi) altamente ramificado o hiperramificado con un numero OH de 1 a 600 mg KOH/g de policarbonato (a DIN 53240, Parte 2), o cuando menos un poliester B2) aLtamente ramificado o biperramificado de tipo en donde x es cuando menos 1.1 e y es cuando menos 2.1, o una mezcla de estos.