公开(公告)号:BG108522A
公开(公告)日:2004-12-30
申请号:BG10852204
申请日:2004-01-12
Applicant: BASF AG
Inventor: EMRI IGOR , VON BERNSTORFF BERND-STEFFEN , RAUSCHENBERGER VOLKER , HORN HANS
IPC: C08L67/00 , C08L67/02 , C08L77/00 , C08L77/02 , C08L77/06 , C08L77/12 , C08L101/02 , C08L101/12
Abstract: The thermoplastic mixture contains m polymers Pn, m representing a natural number higher than 1, and n is a natural number bigger than 1, and n is a natural number from 1 to m, and each of the polymers has: a) one or more functional groups with structure -(R1)x-C(O)-(R2)y- found as a recurring unit in the polymer chain of Pn, wherein x and y represent 0 or 1 and x + y = 1, R1 and R2 independent ly represent oxygen or nitrogen linked in the main polymer chain; b) numerical value - mean molecular weight Mn(Pn); c) average molecular weight Mw(Pn); d) z average molecular weight Mz(Pn); e) a heterogeneity index Mw(Pn)/Mn(Pn); and f) molecular weight Mp(Pn) and polymers Pn differ for each other by 1, 2, 3, 4, 5 and 6 of the properties of a), b), c), d), e) and f), and wherein the polymer mixturehas numerical value - mean molecular weight Mn(P)1, weight average molecular weight Mw(P)1, z - a weight average molecular weight Mz(P)1, heterogeneity index Mw(P)1/Mn(P)1 and molecular weight Mp(P)1, and after ageing of the polymer mixture at its melting point, it has numerical value - average molecular weight Mn(P)2, weight average molecular weight Mw(P)2, z - mean molecular weight Mz(P)2, heterogeneity index Mw(P)2, and molecular weight Mp(P)2 and these values Mn(P)2, Mw(P)2/Mn(P), Mz(P)2, Mw(P)2/Mn(P)2 lie within the triple replication standard deviation sigma (r) in relation to Mn(P)1, Mw(P)1, Mz(P)1, Mw(P)1/Mn(P)1 and Mp(P)1.
-
公开(公告)号:CZ20033513A3
公开(公告)日:2004-05-12
申请号:CZ20033513
申请日:2002-06-13
Applicant: BASF AG
Abstract: A thermoplastic polymer mixture comprising m polymers Pn, where m is a natural number greater than 1 and n is a natural number from 1 to m, where n is a natural number from 1 to m, where each of the polymers has one or more functional groups of the structure -(R )x-C(O)-(R )y- present as repeat units in the main chain of polymer Pn where x and y, independently of one another, are 0 or 1, and x+y=1 R and R , independently of one another, are oxygen or nitrogen bonded into the main polymer chain, where in the differential distribution curve W(M) determined to DIN 55672-2 in hexafluoroisopropanol as eluent the polymer mixture has at least two maxima of the relative frequency W, and after aging of the polymer mixture at the melting point of the polymer mixture determined to ISO 11357-1 and 11357-3 for 5 minutes, the polymer mixture has in the differential distribution curve W(M) determined to DIN 55672-2 in hexafluoroisopropanol as eluent at least 2 maxima of the relative frequency W, and the position of the maxima here after aging of the polymer mixture at the melting point of the polymer mixture is within three times the recurrent standard deviation sigma(r) of MP in percentage of the value measured to DIN 55672-2, based on the position of the maxima prior to aging of the polymer mixture at the melting point of the polymer mixture.
-
公开(公告)号:SK15472003A3
公开(公告)日:2004-04-06
申请号:SK15472003
申请日:2002-06-14
Applicant: BASF AG
IPC: C08L67/00 , C08L67/02 , C08L77/00 , C08L77/02 , C08L77/06 , C08L77/12 , C08L101/02 , C08L101/12
Abstract: The invention relates to a thermoplastic polymer mixture containing m, m representing a natural number higher than 1, polymers Pn wherein n represents a natural number between 1 and m, and at least one recurring functional group contained in the Pn polymer chain, said group(s) having the structure -(R )x-C(O)-(R )y- wherein x and y independently represent 0 or 1, and x+y=1, and R , R independently represent oxygen or nitrogen linked into the main polymer chain. The polymers Pn differ in terms of at least one characteristic related to molecular weight. The polymer mixture has a number average molecular weight Mn(P)1, a weight average molecular weight Mw(P)1, a Z average molecular weight Mz(P)1, a heterogeneity index Mw(P)1/Mn(P)1, and a molecular weight Mp(P)1 defined according to DIN 55672-2 in hexafluoroisopropanol as an elution agent. After maintaining the polymer mixture at the melting point of the same, defined according to ISO 11357-1 and 11357-3, for five minutes, the polymer mixture has a number average molecular weight Mn(P)2, a weight average molecular weight Mw(P)2, a Z average molecular weight Mz(P)2, a heterogeneity index Mw(P)2/Mn(P)2, and a molecular weight Mp(P)2 defined according to DIN 55672-2 in hexafluoroisopropanol as an elution agent. The values Mn(P)2, Mw(P)2, Mz(P)2, Mw(P)2/Mn(P)2 and Mp(P)2 lie within the triple replication standard deviation sigma (r) in relation to Mn(P)1, Mw(P)1, Mz(P)1, Mw(P)1/Mn(P)1 and Mp(P
-
公开(公告)号:DE10129532A1
公开(公告)日:2003-01-09
申请号:DE10129532
申请日:2001-06-21
Applicant: BASF AG
Inventor: EMRI IGOR , BERNSTORFF BERND-STEFFEN VON , RAUSCHENBERGER VOLKER , HORN HANS CHRISTOPH , KISSEL JUTTA , MOLNAR FERENC
IPC: C08G63/16 , C08G63/20 , C08G69/02 , C08G69/26 , C08G69/44 , C08L77/00 , C08G69/28 , C08J5/02 , C08K7/16 , C08L51/06 , C08L101/02
Abstract: The invention relates to a thermoplastic polymer, whose parent chain contains one or more recurrent functional groups with the structure - (R )x - C(O) - (R )y -. In said structure x and y independently of one another represent 0 or 1, whereby x + y = 1 or 2 and R and R independently of one another represent oxygen or nitrogen that are bound into the polymer parent chain. Said polymer is characterised in that the number of at least one species of reactive terminal groups (EG) in the polymer parent chain, (in relation to the sum of all said species of reactive terminal groups in the polymer parent chain), satisfies the inequation EG
-
公开(公告)号:DE10129524A1
公开(公告)日:2003-01-09
申请号:DE10129524
申请日:2001-06-21
Applicant: BASF AG
Abstract: A thermoplastic polymer mixture (I) of polymers with in-chain functional groups shows a differential distribution curve W(M) (DIN 55672-2) with at least 2 peaks of relative frequency W before and after 5 minutes at the melting point of (I), the peak positions after storage being within 3 times the repeat standard deviation of Mp based on peak positions before storage. A thermoplastic polymer mixture (I) containing m polymers (Pn) with one or more functional groups in the main chain (where m = more than 1 and n = 1-m), in which the differential distribution curve W(M) determined in accordance with DIN 55672-2 using hexafluoroisopropanol as eluant shows at least 2 peaks of relative frequency W before and after storage at the melting point of (I) (determined as in ISO 11357-1 and 11357-3) for 5 minutes, the peak positions after storage being within 3 times the repeat standard deviation (sigma(r)) of Mp as a percentage of the measured value (DIN 55672-2) based on peak positions before storage. Independent claims are also included for (1) a method for the production of (I) from a mixture of solid polymers Pn by melting, mixing and solidifying the mixture; (2) a method for the production of (I) by adding part of polymers Pn in molten or solid form to another part of Pn in molten form, then mixing in the melt and solidifying; and (3) fibres, sheet materials and molded products obtained from (I).
-
公开(公告)号:PL375040A1
公开(公告)日:2005-11-14
申请号:PL37504002
申请日:2002-06-13
Applicant: BASF AG
Abstract: A thermoplastic polymer mixture comprising m polymers Pn, where m is a natural number greater than 1 and n is a natural number from 1 to m, where n is a natural number from 1 to m, where each of the polymers has one or more functional groups of the structure -(R )x-C(O)-(R )y- present as repeat units in the main chain of polymer Pn where x and y, independently of one another, are 0 or 1, and x+y=1 R and R , independently of one another, are oxygen or nitrogen bonded into the main polymer chain, where in the differential distribution curve W(M) determined to DIN 55672-2 in hexafluoroisopropanol as eluent the polymer mixture has at least two maxima of the relative frequency W, and after aging of the polymer mixture at the melting point of the polymer mixture determined to ISO 11357-1 and 11357-3 for 5 minutes, the polymer mixture has in the differential distribution curve W(M) determined to DIN 55672-2 in hexafluoroisopropanol as eluent at least 2 maxima of the relative frequency W, and the position of the maxima here after aging of the polymer mixture at the melting point of the polymer mixture is within three times the recurrent standard deviation sigma(r) of MP in percentage of the value measured to DIN 55672-2, based on the position of the maxima prior to aging of the polymer mixture at the melting point of the polymer mixture.
-
公开(公告)号:BR0210567A
公开(公告)日:2004-06-08
申请号:BR0210567
申请日:2002-06-14
Applicant: BASF AG
Inventor: EMRI IGOR , BERNSTORFF BERN-STEFFEN VON , RAUSCHENBERGER VOLKER , HORN HANS CHRISTOPH
IPC: C08L67/00 , C08L67/02 , C08L77/00 , C08L77/02 , C08L77/06 , C08L77/12 , C08L101/02 , C08L101/12
Abstract: The invention relates to a thermoplastic polymer mixture containing m, m representing a natural number higher than 1, polymers Pn wherein n represents a natural number between 1 and m, and at least one recurring functional group contained in the Pn polymer chain, said group(s) having the structure -(R )x-C(O)-(R )y- wherein x and y independently represent 0 or 1, and x+y=1, and R , R independently represent oxygen or nitrogen linked into the main polymer chain. The polymers Pn differ in terms of at least one characteristic related to molecular weight. The polymer mixture has a number average molecular weight Mn(P)1, a weight average molecular weight Mw(P)1, a Z average molecular weight Mz(P)1, a heterogeneity index Mw(P)1/Mn(P)1, and a molecular weight Mp(P)1 defined according to DIN 55672-2 in hexafluoroisopropanol as an elution agent. After maintaining the polymer mixture at the melting point of the same, defined according to ISO 11357-1 and 11357-3, for five minutes, the polymer mixture has a number average molecular weight Mn(P)2, a weight average molecular weight Mw(P)2, a Z average molecular weight Mz(P)2, a heterogeneity index Mw(P)2/Mn(P)2, and a molecular weight Mp(P)2 defined according to DIN 55672-2 in hexafluoroisopropanol as an elution agent. The values Mn(P)2, Mw(P)2, Mz(P)2, Mw(P)2/Mn(P)2 and Mp(P)2 lie within the triple replication standard deviation sigma (r) in relation to Mn(P)1, Mw(P)1, Mz(P)1, Mw(P)1/Mn(P)1 and Mp(P
-
公开(公告)号:SK15482003A3
公开(公告)日:2004-04-06
申请号:SK15482003
申请日:2002-06-13
Applicant: BASF AG
Abstract: A thermoplastic polymer mixture comprising m polymers Pn, where m is a natural number greater than 1 and n is a natural number from 1 to m, where n is a natural number from 1 to m, where each of the polymers has one or more functional groups of the structure -(R )x-C(O)-(R )y- present as repeat units in the main chain of polymer Pn where x and y, independently of one another, are 0 or 1, and x+y=1 R and R , independently of one another, are oxygen or nitrogen bonded into the main polymer chain, where in the differential distribution curve W(M) determined to DIN 55672-2 in hexafluoroisopropanol as eluent the polymer mixture has at least two maxima of the relative frequency W, and after aging of the polymer mixture at the melting point of the polymer mixture determined to ISO 11357-1 and 11357-3 for 5 minutes, the polymer mixture has in the differential distribution curve W(M) determined to DIN 55672-2 in hexafluoroisopropanol as eluent at least 2 maxima of the relative frequency W, and the position of the maxima here after aging of the polymer mixture at the melting point of the polymer mixture is within three times the recurrent standard deviation sigma(r) of MP in percentage of the value measured to DIN 55672-2, based on the position of the maxima prior to aging of the polymer mixture at the melting point of the polymer mixture.
-
公开(公告)号:DE10129525A1
公开(公告)日:2003-01-09
申请号:DE10129525
申请日:2001-06-21
Applicant: BASF AG
IPC: C08L67/00 , C08L67/02 , C08L77/00 , C08L77/02 , C08L77/06 , C08L77/12 , C08G63/83 , C08G69/04 , C08K7/16 , C08J3/11 , C08J5/02 , C08L51/06
Abstract: A thermoplastic polymer mixture comprising m polymers Pn, where m is a natural number greater than 1 and n is a natural number from 1 to m, where n is a natural number from 1 to m, where each of the polymers has one or more functional groups of the structure -(R )x-C(O)-(R )y- present as repeat units in the main chain of polymer Pn where x and y, independently of one another, are 0 or 1, and x+y=1 R and R , independently of one another, are oxygen or nitrogen bonded into the main polymer chain, where in the differential distribution curve W(M) determined to DIN 55672-2 in hexafluoroisopropanol as eluent the polymer mixture has at least two maxima of the relative frequency W, and after aging of the polymer mixture at the melting point of the polymer mixture determined to ISO 11357-1 and 11357-3 for 5 minutes, the polymer mixture has in the differential distribution curve W(M) determined to DIN 55672-2 in hexafluoroisopropanol as eluent at least 2 maxima of the relative frequency W, and the position of the maxima here after aging of the polymer mixture at the melting point of the polymer mixture is within three times the recurrent standard deviation sigma(r) of MP in percentage of the value measured to DIN 55672-2, based on the position of the maxima prior to aging of the polymer mixture at the melting point of the polymer mixture.
-
公开(公告)号:CA2449893A1
公开(公告)日:2003-01-03
申请号:CA2449893
申请日:2002-06-13
Applicant: BASF AG
Abstract: Published without an
-
-
-
-
-
-
-
-
-