15.
    发明专利
    未知

    公开(公告)号:DE4414054A1

    公开(公告)日:1995-10-26

    申请号:DE4414054

    申请日:1994-04-21

    Applicant: BASF AG

    Abstract: Moulding compounds containing: A) polyarylene ethers with recurring units (I) or units (I) containing substituted arylene groups or their mixtures, in which t and q may be a whole number 0, 1, 2, or 3, T, Q and Z are a chemical bond or a group selected from -O-, -S-, -SO2-, S=O, C=O, -N=N-, R C=CR - and -CR R -, provided that at least one of the groups T, Q or Z is -SO2- or C=O, R and R are each a hydrogen atom or a C1 to C10 alkyl group, R and R are each a hydrogen atom, a C1 to C10 alkyl, C4 to C10 cycloalkyl, C1 to C10 alkoxy or C6 to C18 aryl group, in which the aforementioned groups may be substituted by fluorine and/or chlorine atoms, Ar and Ar are C6 to C18 aryl groups which can have substituents selected from C1 to C10 alkyl, C6 to C18 aryl, C1 to C10 alkoxy and halogen; B) metal fibres based on iron, copper or silver coated with a polyarylene ether sulphone skim, and C) alkaline earth titanate, alkaline earth silicate or glass fibres or their mixtures. The invention also relates to the use of these moulding compounds.

    17.
    发明专利
    未知

    公开(公告)号:DE4326774A1

    公开(公告)日:1995-02-16

    申请号:DE4326774

    申请日:1993-08-10

    Applicant: BASF AG

    Abstract: In order to prepare polyarylene ether ketones by Friedel-Crafts polycondensation, a reaction mixture comprising A. a monomer system, B. a Lewis acid, C. optionally a Lewis base and D. an inert solvent is polycondensed in two reaction zones and discharged in plug flow from the second reaction zone and formulated. In this process, the reaction mixture is polycondensed in the first reaction zone with stirring to a viscosity of about 2000 mPa.s, transferred into the second reaction zone and discharged therefrom by means of an inert solvent or by means of an inert gas saturated with the solvent under a pressure of from about 6 to 65 bar, preferably even 10 to 25 bar, where the conveying pressure is reduced in at least two steps and the pressure reduction in the first step is at most 20%.

Patent Agency Ranking