公开(公告)号:FI971380A0
公开(公告)日:1997-04-03
申请号:FI971380
申请日:1997-04-03
Applicant: BASF AG
Inventor: BAUMSTARK ROLAND , RUPANER ROBERT
IPC: C08F2/00 , C08F2/16 , C08F2/22 , C08F4/40 , C08F6/00 , C08F12/08 , C08F14/06 , C08F14/08 , C08F18/08 , C08F18/10 , C08F20/04 , C08F20/12 , C08F20/56 , C08F
Abstract: PCT No. PCT/EP95/03770 Sec. 371 Date Apr. 3, 1997 Sec. 102(e) Date Apr. 3, 1997 PCT Filed Sep. 23, 1995 PCT Pub. No. WO96/10588 PCT Pub. Date Apr. 11, 1996A process for the preparation of an aqueous polymer emulsion, in which an aqueous emulsion of a polymer which contains at least one chemically bonded monomer having at least one ethylenically unsaturated group is produced in a manner known per se so that the total content of free monomers having at least one ethylenically unsaturated double bond, ie. monomers of this type which are not chemically bonded, in the aqueous polymer emulsion is from >0 to
-
公开(公告)号:FI971380A
公开(公告)日:1997-04-03
申请号:FI971380
申请日:1997-04-03
Applicant: BASF AG
Inventor: BAUMSTARK ROLAND , RUPANER ROBERT
IPC: C08F2/00 , C08F2/16 , C08F2/22 , C08F4/40 , C08F6/00 , C08F12/08 , C08F14/06 , C08F14/08 , C08F18/08 , C08F18/10 , C08F20/04 , C08F20/12 , C08F20/56 , C08F
Abstract: PCT No. PCT/EP95/03770 Sec. 371 Date Apr. 3, 1997 Sec. 102(e) Date Apr. 3, 1997 PCT Filed Sep. 23, 1995 PCT Pub. No. WO96/10588 PCT Pub. Date Apr. 11, 1996A process for the preparation of an aqueous polymer emulsion, in which an aqueous emulsion of a polymer which contains at least one chemically bonded monomer having at least one ethylenically unsaturated group is produced in a manner known per se so that the total content of free monomers having at least one ethylenically unsaturated double bond, ie. monomers of this type which are not chemically bonded, in the aqueous polymer emulsion is from >0 to
-
公开(公告)号:AU2005229399B2
公开(公告)日:2011-06-09
申请号:AU2005229399
申请日:2005-03-26
Applicant: BASF AG
Inventor: RANFT MEIK , DERSCH ROLF , SCHLARB BERNHARD , BAUMSTARK ROLAND , RUPANER ROBERT , LACH CHRISTIAN
IPC: C08F220/12 , C09D133/06
-
公开(公告)号:DK0882094T4
公开(公告)日:2008-11-10
申请号:DK97905049
申请日:1997-02-19
Applicant: BASF AG
Inventor: WISTUBA ECKEHARDT , RECK BERND , BECKERLE WILHELM FRIEDRICH , KISTENMACHER AXEL , RUPANER ROBERT , HUMMERICH RAINER
IPC: B05D7/24 , C08L57/00 , B05D1/00 , C08F8/30 , C08J7/04 , C08K5/17 , C08L23/26 , C08L35/00 , C08L57/10 , C09D135/00
Abstract: PCT No. PCT/EP97/00773 Sec. 371 Date Aug. 19, 1998 Sec. 102(e) Date Aug. 19, 1998 PCT Filed Feb. 19, 1997 PCT Pub. No. WO97/31060 PCT Pub. Date Aug. 28, 1997The use of a formaldehyde-free aqueous binder comprising A) a polymer obtained by free-radical polymerization comprising 5-100% by weight of an ethylenically unsaturated acid anhydride or of an ethylenically unsaturated dicarboxylic acid whose carboxyl groups may form an anhydride group, and B) an alkanolamine having at least two hydroxyl groups as a coating composition for shaped articles.
-
公开(公告)号:DE59809028D1
公开(公告)日:2003-08-21
申请号:DE59809028
申请日:1998-09-17
Applicant: BASF AG
Inventor: RUPANER ROBERT , BAUER GERHARD , LAWRENZ SVEN , HEIBEL CLAUDIA , DOBBELAAR JOHANNES
IPC: C08F6/00
Abstract: A process is described for effectively reducing the residual monomer content of an aqueous polymer dispersion by aftertreatment at atmospheric pressure or above with an initiator system comprising a) a hydroperoxide, hydrogen peroxide or a peracid, and b) an alpha-hydroxy carboxylic acid, such as tartaric acid, or with a salt thereof.
-
公开(公告)号:AU748776B2
公开(公告)日:2002-06-13
申请号:AU8079998
申请日:1998-08-18
Applicant: BASF AG
Inventor: HUBINGER WOLFGANG , WUNDER RAINER , BAUER GERHARD , DOBBELAAR JOHANNES , LAWRENZ SVEN , MUESELER FRANZ-JOSEF , NAHSTOLL JURGEN , RUPANER ROBERT , SCHMIDT CHRISTIAN-ULRICH
Abstract: A method for cooling dispersions or liquids (D/L) after a deodorising process comprising (a) passing steam through the D/L in a boiler (1), causing it to foam, (b) taking the foam from the top of the boiler into an evacuated separator (4) through a jet (5) and thus breaking the foam, (c) condensing the water vapour from the foam in a heat exchanger (8) and removing organic volatiles, and (d) returning the broken foam to (1). This process is continued until the D/L is deodorised to the required extent, then the hot D/L is cooled by transferring it from the bottom of (1) to the evacuated separator (4) via jet (5), the water vapour produced is condensed in (8) as before, and the cooled D/L is taken off at the bottom of (4).
-
公开(公告)号:ID26637A
公开(公告)日:2001-01-25
申请号:ID20001969
申请日:1999-03-31
Applicant: BASF AG
Inventor: RUPANER ROBERT , SCHOLTISSEK MARTIN , SCHUMACHER KARL-HEINZ , ANGEL MAXIMILIAN
-
公开(公告)号:DK0882093T3
公开(公告)日:1999-12-20
申请号:DK97905047
申请日:1997-02-19
Applicant: BASF AG
Inventor: RECK BERND , BECKERLE WILHELM FRIEDRICH , KISTENMACHER AXEL , RUPANER ROBERT , WISTUBA ECKEHARDT , HUMMERICH RAINER
IPC: B05D1/00 , B27N1/02 , B27N3/00 , C08F8/30 , C08K5/17 , C08L33/02 , C08L35/00 , C08L57/00 , C08L97/02
Abstract: PCT No. PCT/EP97/00768 Sec. 371 Date Aug. 21, 1998 Sec. 102(e) Date Aug. 21, 1998 PCT Filed Feb. 19, 1997 PCT Pub. No. WO97/31059 PCT Pub. Date Aug. 28, 1997A method for forming shaped products by mixing a formaldehyde-free aqueous binder comprising A) a free-radically polymerized polymer containing from 5 to 100% by weight of units derived from an ethylenically unsaturated acid anhydride or from an ethylenically unsaturated dicarboxylic acid whose carboxyl group can form an anhydride group, and B) an alkanolamine having at least two hydroxyl groups, with fibers or chips to form a shaped article, wherein said binder has a property of drying at 50 DEG C. in 72 hours to a film from 0.3 to 1 mm in thickness and, following a subsequent 15 minute cure at 130 DEG C. in air, has a gel content of above 50% by weight, wherein the binder includes less than 0.1% by weight, based on A)+B), of a phosphorus-containing reaction accelerant with fibers or chips.
-
公开(公告)号:AT186066T
公开(公告)日:1999-11-15
申请号:AT97905049
申请日:1997-02-19
Applicant: BASF AG
Inventor: RECK BERND , WISTUBA ECKEHARDT , BECKERLE WILHELM FRIEDRICH , KISTENMACHER AXEL , RUPANER ROBERT , HUMMERICH RAINER
IPC: B05D7/24 , B05D1/00 , C08F8/30 , C08J7/04 , C08K5/17 , C08L23/26 , C08L35/00 , C08L57/00 , C08L57/10 , C09D135/00
Abstract: PCT No. PCT/EP97/00773 Sec. 371 Date Aug. 19, 1998 Sec. 102(e) Date Aug. 19, 1998 PCT Filed Feb. 19, 1997 PCT Pub. No. WO97/31060 PCT Pub. Date Aug. 28, 1997The use of a formaldehyde-free aqueous binder comprising A) a polymer obtained by free-radical polymerization comprising 5-100% by weight of an ethylenically unsaturated acid anhydride or of an ethylenically unsaturated dicarboxylic acid whose carboxyl groups may form an anhydride group, and B) an alkanolamine having at least two hydroxyl groups as a coating composition for shaped articles.
-
公开(公告)号:BR9707573A
公开(公告)日:1999-07-27
申请号:BR9707573
申请日:1997-02-19
Applicant: BASF AG
Inventor: RECK BERND , WISTUBA ECKEHARDT , BECKERLE WILHELM FRIEDRICH , KISTENMACHER AXEL , RUPANER ROBERT , HUMMERICH RAINER
IPC: B05D1/00 , B27N1/02 , B27N3/00 , C08F8/30 , C08K5/17 , C08L33/02 , C08L35/00 , C08L57/00 , C08L97/02
Abstract: PCT No. PCT/EP97/00768 Sec. 371 Date Aug. 21, 1998 Sec. 102(e) Date Aug. 21, 1998 PCT Filed Feb. 19, 1997 PCT Pub. No. WO97/31059 PCT Pub. Date Aug. 28, 1997A method for forming shaped products by mixing a formaldehyde-free aqueous binder comprising A) a free-radically polymerized polymer containing from 5 to 100% by weight of units derived from an ethylenically unsaturated acid anhydride or from an ethylenically unsaturated dicarboxylic acid whose carboxyl group can form an anhydride group, and B) an alkanolamine having at least two hydroxyl groups, with fibers or chips to form a shaped article, wherein said binder has a property of drying at 50 DEG C. in 72 hours to a film from 0.3 to 1 mm in thickness and, following a subsequent 15 minute cure at 130 DEG C. in air, has a gel content of above 50% by weight, wherein the binder includes less than 0.1% by weight, based on A)+B), of a phosphorus-containing reaction accelerant with fibers or chips.
-
-
-
-
-
-
-
-
-