公开(公告)号:CA1196486A
公开(公告)日:1985-11-12
申请号:CA410157
申请日:1982-08-26
Applicant: UNITED TECHNOLOGIES CORP
Inventor: NEAL JAMES W , LOERSCH JOSEPH F
IPC: C21D7/06
Abstract: Method for Simultaneous Peening and Smoothing A method for simultaneously shot peening and smoothing includes use of relatively large, smooth, hard, spherical steel shot having a substantially uniform diameter in the range 1-2.5 mm. Titanium workpieces are provided in one step with a compressive stress layer of the order of 0.13 mm. and a surface finish of better than 15 x 10 6 inch AA, compared to conventional peened finishes of the order of 40 x 10-6 inch AA. Surface finish and peening intensity are interrelated and dependent on shot diameter, mass, velocity, and energy within relatively small limits. The shot diameter is uniform within ? 0.05 mm; the shot impact velocity is uniform within ? 4 percent or less, in the range 1.4-12 m/s. The method is also applied to the simultaneous densification and smoothing of overlay coatings on workpieces, such as those deposited by physical vapor deposition and plasma spraying. Usually heat treatment follows the peening step.
-
公开(公告)号:CA1191672A
公开(公告)日:1985-08-13
申请号:CA409436
申请日:1982-08-13
Applicant: UNITED TECHNOLOGIES CORP
Inventor: LOERSCH JOSEPH F , NEAL JAMES W
Abstract: Shot Peening Apparatus In apparatus for shot peening, gravity is used to accelerate uniform sized steel shot, and thereby impart a combination of good surface finish and uniform compressive stresses to workpieces. It is especially useful for finishing gas turbine airfoils. Shot is introduced into the peening enclosure (28) through a gate (40) at near zero velocity. It is then accelerated along a streamline (31) toward the workpiece (18) with uniform velocity. The workpiece, positioned along the streamline, can be manipulated in three rotational modes: oscillatory rotation to uniformly peen contoured surfaces of a workpiece, periodic incremental rotation to peen different sides of a workpiece; and, tilting motion to enable peening of shoulders (22). The apparatus is especially suited to peening fragile workpieces such as gas turbine airfoils (18). A diverter plate (44) intercepts the shot stream at times when repositioning of a fragile workpiece is undertaken. Thus, possibly damaging impacts are avoided and steady state operation is able to be promptly resumed.
-
公开(公告)号:SG11201500286RA
公开(公告)日:2015-02-27
申请号:SG11201500286R
申请日:2013-07-31
Applicant: UNITED TECHNOLOGIES CORP
Inventor: NEAL JAMES W , LITTON DAVID A , BEERS RUSSELL A , ZIMMERMAN BENJAMIN JOSEPH , MALONEY MICHAEL J
Abstract: A coating system for coating a part (10), such as a turbine blade or vane, has a mask (14) positioned adjacent to a first portion (16) of the part (10) to be coated and a mechanism (30) for moving the mask (14) relative to the part (10). The mechanism (30) may be a gear mechanism or a magnetic mechanism.
-
公开(公告)号:SG165296A1
公开(公告)日:2010-10-28
申请号:SG2010022168
申请日:2010-03-30
Applicant: UNITED TECHNOLOGIES CORP
Inventor: LATOUR ROBERT F , NEAL JAMES W
Abstract: A method of processing an article includes heating the article in an atmosphere substantially free of oxygen to an oxidation temperature within a predetermined temperature range. The article includes a substrate and a bond coat disposed on the substrate. A partial pressure of oxygen is then established within the atmosphere after heating to the oxidation temperature. At least a portion of the bond coat oxidizes in the partial pressure of oxygen at the oxidation temperature to form a desired type of oxide to the substantial exclusion of forming other types of oxides. A ceramic coating is then deposited on the oxide.
-
公开(公告)号:SG165295A1
公开(公告)日:2010-10-28
申请号:SG2010022150
申请日:2010-03-30
Applicant: UNITED TECHNOLOGIES CORP
Inventor: NEAL JAMES W
Abstract: A physical vapor deposition apparatus includes first and second chambers. A first directed vapor deposition crucible is at least partially within the first chamber for presenting a first source material to be deposited on a work piece. A second directed vapor deposition crucible is at least partially within the second chamber for presenting a second, different source material to be deposited as a second coating on the work piece. At least one of the materials may be deposited as a coating.
-
公开(公告)号:AT410530T
公开(公告)日:2008-10-15
申请号:AT04254725
申请日:2004-08-05
Applicant: UNITED TECHNOLOGIES CORP
Inventor: MEMMEN ROBERT L , NEAL JAMES W
IPC: C23C14/32 , F01D5/28 , B23P6/00 , C22C14/00 , C23C14/02 , C23C14/04 , C23C14/14 , C23C14/16 , C23C14/30 , C23C14/58 , F01D5/00 , F01D5/12 , F01D5/30 , F01D25/00 , F02C7/00 , F04D29/34 , F04D29/38
Abstract: Physical vapor deposition is utilized to deposit repair material on Ti alloy turbine components. In a preferred embodiment, a damaged area (30) of an airfoil leading edge is machined to produce a base surface (50), and a backing element (52) is attached to the airfoil (26) to receive the repair material which can subsequently be machined to the appropriate profile.
-
公开(公告)号:CA1192387A
公开(公告)日:1985-08-27
申请号:CA409536
申请日:1982-08-16
Applicant: UNITED TECHNOLOGIES CORP
Inventor: NEAL JAMES W , LOERSCH JOSEPH F
Abstract: Shot peening of thin edges of workpieces which are subject to deformation damage by direct impacts is accomplished by rotating the workpiece edge near centerline through a particular angle measured from the nor mal to the shot streamline. The angle is sufficient to cause oblique blows on the centerline of the edge, but insufficient to cause direct impacts. Compressive stresses by the oblique blows provide residual compressive stresses along the centerline to the desired depth. The angle is calcuable from the edge radius, the depth of stressing desired at the centerline, and the depth of stressing produced by shot at a reference location. Oscillatory rotation is preferably used to obtain even peening.
-
公开(公告)号:EP2880195A4
公开(公告)日:2015-07-22
申请号:EP13825631
申请日:2013-07-31
Applicant: UNITED TECHNOLOGIES CORP
Inventor: NEAL JAMES W , LITTON DAVID A , BEERS RUSSELL A , ZIMMERMAN BENJAMIN JOSEPH , MALONEY MICHAEL J
CPC classification number: C23C14/042 , C23C14/044 , C23C14/30 , F05D2230/313
Abstract: A coating system for coating a part (10), such as a turbine blade or vane, has a mask (14) positioned adjacent to a first portion (16) of the part (10) to be coated and a mechanism (30) for moving the mask (14) relative to the part (10). The mechanism (30) may be a gear mechanism or a magnetic mechanism.
Abstract translation: 用于涂覆诸如涡轮叶片或叶片的部分(10)的涂覆系统具有邻近待涂覆的部分(10)的第一部分(16)定位的掩模(14)和用于 使面罩(14)相对于部件(10)移动。 机构(30)可以是齿轮机构或磁性机构。
-
19.
公开(公告)号:EP2236642B1
公开(公告)日:2017-06-21
申请号:EP10250669
申请日:2010-03-31
Applicant: UNITED TECHNOLOGIES CORP
Inventor: LATOUR ROBERT F , NEAL JAMES W
CPC classification number: C23C14/024 , C23C8/02 , C23C8/12 , C23C8/80 , C23C14/083 , C23C14/568 , C23C28/3215 , C23C28/345 , C23C28/3455 , Y10T428/12549
-
20.
公开(公告)号:EP2971222A4
公开(公告)日:2017-05-10
申请号:EP14765262
申请日:2014-03-14
Applicant: UNITED TECHNOLOGIES CORP
Inventor: HAZEL BRIAN T , MALONEY MICHAEL J , NEAL JAMES W , LITTON DAVID A
CPC classification number: C23C14/30 , C23C14/228 , C23C14/243 , C23C14/246 , C23C14/505
Abstract: A deposition apparatus (20) comprising: a chamber (22); a process gas source (62) coupled to the chamber; a vacuum pump (52) coupled to the chamber; at least two electron guns (26); one or more power supplies (30) coupled to the electron guns; a plurality of crucibles (32,33,34) positioned or positionable in an operative position within a field of view of at least one said electron gun; and a part holder (170) having at least one operative position for holding parts spaced above the crucibles by a standoff height H. The standoff height H is adjustable in a range including at least 22 inches.
Abstract translation: 一种沉积装置(20),包括:腔室(22); 耦合到所述室的处理气体源(62); 联接到腔室的真空泵(52) 至少两个电子枪(26); 耦合到电子枪的一个或多个电源(30) 多个坩埚(32,33,34),位于或可定位在至少一个所述电子枪的视场内的操作位置; 以及具有至少一个操作位置的零件保持器(170),该操作位置用于保持在坩埚上方与隔离高度H隔开的部分。隔离高度H可在包括至少22英寸的范围内调节。
-
-
-
-
-
-
-
-
-