32.
    发明专利
    未知

    公开(公告)号:DE19750238A1

    公开(公告)日:1999-05-27

    申请号:DE19750238

    申请日:1997-11-13

    Applicant: DEGUSSA

    Abstract: A pressed article (I) is based upon pyrogenically produced silicon dioxide having a pore volume of 0.5-1.8 ml/g. Independent claims are included for: (i) the production of (I) by mixing pyrogenically produced silicon dioxide with methylhydroxyethylcellulose, wax and polyethylene glycol and water followed by extrusion, optionally cutting the extrudate to a desired length, drying at 70-150 degrees C and heating at 400-1200 degrees C for up to 10 hours; (ii) a supported catalyst (II) comprising (I) for the production of vinylacetate monomer, that contains palladium (Pd) and/or Pd compounds and alkali compounds; gold (Au) and/or Au compound (Pd/alkali/Au system) or cadmium (Cd) and/or Cd compounds (Pd/alkali/Cd system) or barium (Ba) and/or Ba compounds (Pd/alkali/Ba system) or Pd, alkali compounds and mixture of Au and/or Cd and/or Ba; and (iii) the production of the catalyst support (II) by soaking, spraying, condensing, dipping or precipitating the Pd, Au, Cd and/or Ba compounds onto (I), optionally reducing the metal, washing to remove the resulting chloride content, impregnating with alkali acetate or alkali compound that is converted under reaction conditions at least partially to alkali acetate.

    40.
    发明专利
    未知

    公开(公告)号:ID26671A

    公开(公告)日:2001-01-25

    申请号:ID990868

    申请日:1999-09-17

    Applicant: DEGUSSA

    Abstract: Moldings are disclosed for use as a catalyst or catalyst support for hydrating olefin, such as ethylene and propylene. The moldings are based on a pyrogenically produced mixed oxide having the following physicochemical parameters:The moldings are produced by homogenizing pyrogenically produced mixed oxide as desired with water and one or more compounds selected from the group of methylcellulose, methylhydroxyethylcellulose, wax, polyethylene glycol, magnesium stearate or aluminium stearate; drying the product at a temperature of 70-150° C.; optionally comminuting to yield a powder; optionally compression molding the powder to yield moldings; and performing heat treatment for a period of 0.5 to 10 hours at a temperature of 400 to 1200° C. Prior to drying, the mixture may also be subjected to kneading and/or shaping processes and extruded.

Patent Agency Ranking