公开(公告)号:DE69230509T2
公开(公告)日:2000-05-04
申请号:DE69230509
申请日:1992-05-13
Applicant: KAO CORP
Inventor: UEMURA TOMOHIRO , TANAHASHI MASANORI , MUROI YOSHIYUKI , KONO YOSHINAO
-
公开(公告)号:DE69230509D1
公开(公告)日:2000-02-03
申请号:DE69230509
申请日:1992-05-13
Applicant: KAO CORP
Inventor: UEMURA TOMOHIRO , TANAHASHI MASANORI , MUROI YOSHIYUKI , KONO YOSHINAO
-
公开(公告)号:DE69219201T2
公开(公告)日:1997-08-14
申请号:DE69219201
申请日:1992-05-13
Applicant: KAO CORP
Inventor: UEMURA TOMOHIRO , TANAHASHI MASANORI , MUROI YOSHIYUKI , KONO YOSHINAO
-
公开(公告)号:ES2064200B1
公开(公告)日:1995-09-01
申请号:ES9201112
申请日:1992-05-29
Applicant: KAO CORP
Inventor: TAKAHASHI HIROMICHI , ISHIBASHI YOICHI , MIYAUCHI YOSHITAKA , SHIROISHI TAKANOBU , KONO YOSHINAO
Abstract: A deinking composition which shows a good deinking performance, a good defoaming property and excellent operation characteristics whereby a deinked pulp having a high whiteness and little contamination with the total remaining ink can be obtained in the reclamation of waste papers by flotation, washing or a combination procedure thereof and wherein the deinking composition comprises a reaction mixture (II), as a deinking agent, obtained by the addition reaction of alkylene oxide (D) with a mixture (I) comprising a fat and oil (A) which is constituted with a mixture of higher fatty acids (a) comprising fatty acids having 8 to 24 carbon atoms; having an average carbon atom number of from 12.7 to 22.5; containing from 9.6 to 70.6% by weight of higher fatty acids having 20 to 24 carbon atoms and having an iodine value (IV) of 70 or less and glycerol (b-1), and/or, a transesterification reaction mixture (B) obtained by reacting the fat and oil (A) with glycerol (b-2), and at least one mono- to tetradecahydric alcohol (C).
-
公开(公告)号:HK33991A
公开(公告)日:1991-05-10
申请号:HK33991
申请日:1990-05-02
Applicant: KAO CORP
Inventor: TAKEMA YOSHINORI , TSUSHIMA RIKIO , YASUDA YUTAKA , KONO YOSHINAO
IPC: C08F16/00 , A61K8/00 , A61K8/02 , A61K8/04 , A61K8/72 , A61K8/81 , A61Q3/02 , A61Q19/00 , C08F16/02 , C08F216/06 , A61K7/00
Abstract: A film-forming cosmetic composition useful as a facial pack, nail enamel, eye liner etc., which comprises a copolymer of vinyl alcohol and alkyl vinyl ether, being referred to simply as PVA/AVE, consisting of 98 to 80 mole% of vinyl alcohol monomer units and 2 to 20 mole% of linear or branched alkyl vinyl monomer units having from 1 to 6 carbon atoms.The molar ratio of the vinyl alcohol monomer units to the alkyl vinyl ether monomer units is in the range of from 95/5 to 85/15.The PVA/AVE according to the invention has no acetic groups with ester bonds in a molecule. Instead, there are alkyl or alkenyl groups having ether bonds which serve for steric hindrance for preventing gelation of an aqueous solution of such copolymer. From this reason, the PVA/AVE does not undergo any hydrolysis as time passes and is thus excellent in storage stability.
-
公开(公告)号:DE2712871A1
公开(公告)日:1977-10-27
申请号:DE2712871
申请日:1977-03-24
Applicant: KAO CORP
Inventor: TAKAMORI SHIGERU , YAMASHITA KAZUTAKA , KONO YOSHINAO
IPC: C09D5/03 , C08G59/00 , C08G65/332 , C08L63/00 , C08L67/00 , C09D163/00 , C09D3/58 , C09D5/40
-
公开(公告)号:DE2557073A1
公开(公告)日:1976-07-08
申请号:DE2557073
申请日:1975-12-18
Applicant: KAO CORP
Inventor: FURUKAWA JUN-ICHI , KONO YOSHINAO , SAKAGUCHI KAHEI
IPC: D06M13/325 , C03C25/32 , C08J3/03 , D06M13/02 , D06M13/328 , D06M15/507 , D06M15/53 , D06M101/00 , C03C25/02
Abstract: A sizing agent for glass fibers comprises a lubricant for glass fibers, a coupling agent, an antistatic agent and a film-forming substance composed of an oil-in-water type emulsion of an unsaturated polyester obtained by reacting a dibasic acid, an adduct of bisphenol A and alkylene oxide, an adduct of caster oil and an alkylene oxide or polyethylene glycol and an amino-glycol or its derivative.
-
38.
公开(公告)号:JP2009001479A
公开(公告)日:2009-01-08
申请号:JP2008132878
申请日:2008-05-21
Inventor: HAMADA DAISUKE , YABE KENICHIRO , SAGAWA KEIICHIRO , SHIMODA MASARO , YADOKORO YOSHIAKI , KONO YOSHINAO , HAMAI TOSHIMASA
IPC: C04B24/26 , C04B28/02 , C04B103/40 , C08F290/06
CPC classification number: C08F290/06 , C04B24/2647 , C04B28/02 , C04B2103/308 , C04B2103/408 , C08F220/06 , C08F220/14 , C08F220/28 , C08F290/00 , C08F290/061 , C08F290/062 , C08F2220/285
Abstract: PROBLEM TO BE SOLVED: To provide a dispersion maintaining agent for hydraulic composition that excels in both fluidity retention and viscosity retention, especially a dispersion maintaining agent that not influenced by the type of hydraulic powder, exhibits excellent fluidity retention and viscosity retention.
SOLUTION: The dispersion maintaining agent for hydraulic composition comprises a copolymer obtained by polymerization of specified monomers 1 of the general formula (1) together with specified monomers 2 of the general formula (2) whose corresponding alcohol compound satisfies a specified property requirement. In the constituent monomers of the above copolymer, the ratio of the monomers 1 is within a specified range, and a specified monomer is used as at least some of the monomers 2, and the ratio of monomer having an acid group or a group resulting from neutralization thereof is ≤5 wt.%.
COPYRIGHT: (C)2009,JPO&INPITAbstract translation: 要解决的问题为了提供流动性保持性和粘度保持性优异的水硬性组合物用分散维持剂,特别是不受液压粉末的影响的分散维持剂,显示出优异的流动性保持性和粘度保持性。 解决方案:用于水硬性组合物的分散维持剂包括通过将通式(1)的特定单体1与指定的通式(2)的单体2聚合得到的共聚物,其相应的醇化合物满足规定的性能要求 。 在上述共聚物的构成单体中,单体1的比例在规定范围内,特定单体用作至少一种单体2,并且具有酸性基团或由 其中和度≤5重量%。 版权所有(C)2009,JPO&INPIT
-
公开(公告)号:JP2008127221A
公开(公告)日:2008-06-05
申请号:JP2006311146
申请日:2006-11-17
Inventor: HAMADA DAISUKE , SHIMODA MASARO , KONO YOSHINAO , KOYANAGI KOJI
IPC: C04B24/26 , C04B28/02 , C08F220/06 , C08F220/28
CPC classification number: C04B24/2641 , C04B20/023
Abstract: PROBLEM TO BE SOLVED: To provide an additive which can be added to a concrete composition with a small amount of paste per unit volume and gives the composition an excellent feeling to workers.
SOLUTION: The additive for concrete comprises: a monomer having a specific oxyalkylene group; and a polymer of a specific polycarboxylic acid base which is obtained by polymerizing with the monomer and has the weight average molecular weight of 15,000-30,000 and the ratio (Mw/Mn) of the weight average molecular weight (Mw) to the number average molecular weight (Mn) of 1.0-1.6.
COPYRIGHT: (C)2008,JPO&INPITAbstract translation: 待解决的问题:为了提供可以添加到每单位体积少量糊料的混凝土组合物中的添加剂,并且给予组合物对工人的良好感觉。 解决方案:混凝土添加剂包括:具有特定氧化烯基团的单体; 以及通过与单体聚合并且具有15,000-30,000的重均分子量和重均分子量(Mw)与数均分子量(Mw)的比(Mw / Mn)而获得的特定聚羧酸碱的聚合物 重量(Mn)为1.0-1.6。 版权所有(C)2008,JPO&INPIT
-
公开(公告)号:JP2007092062A
公开(公告)日:2007-04-12
申请号:JP2006240673
申请日:2006-09-05
Inventor: SHIMODA MASARO , KONO YOSHINAO , MORII YOSHIKAZU , NAKA YOSHIHITO
IPC: C08F220/26 , C04B24/26 , C08F2/38 , C08F230/02 , C08F290/06
Abstract: PROBLEM TO BE SOLVED: To provide a method for producing a dispersing agent for hydraulic composition imparting an excellent dispersing effect and viscosity reducing effect to a hydraulic composition and stably storing without corruption, in a practical industrial level.
SOLUTION: The method for producing the phosphate polymer comprises copolymerization of a specific monomer 1 having a polyoxyalkylene group and a phosphate based monomer 2 in the presence of a chain transfer agent by a solution polymerization method, wherein 50-3000mg of hydrogen peroxide per 1kg of the reaction liquid is added to the reaction liquid after copolymerization reaction.
COPYRIGHT: (C)2007,JPO&INPITAbstract translation: 解决问题的方案:提供一种水硬性组合物的分散剂的制造方法,其在实用的工业水平上赋予液压组合物优异的分散效果和粘度降低效果,并且在不发生腐蚀的情况下稳定地储存。 解决方案:磷酸酯聚合物的制造方法包括在链转移剂的存在下通过溶液聚合法共聚具有聚氧化烯基的特定单体1和磷酸酯类单体2,其中50-3000mg过氧化氢 共聚反应后每1kg反应液加入反应液中。 版权所有(C)2007,JPO&INPIT
-
-
-
-
-
-
-
-
-