화학 증착법에 의한 PbTiO₃박막의 제조방법
    41.
    发明授权
    화학 증착법에 의한 PbTiO₃박막의 제조방법 失效
    通过化学蒸气沉积法制备PBTIO3薄膜的制备方法

    公开(公告)号:KR1019910005405B1

    公开(公告)日:1991-07-29

    申请号:KR1019880013032

    申请日:1988-10-06

    Inventor: 김호기 윤순길

    Abstract: PbTiO3 thin film is produced by chemical depositing Ti plate with Pb powder (99.9%), metal organic cpd. of Ti(C2H5O)4 and O2 (99.99%) in the reaction tube having a multite tube of 47mm inner diameter and 1m length in the two bands of horizontal resistance furnace. The chemical vapour deposition process is carried out at 600-750 deg.C, 0.02-0.23 fraction of Ti(C2H5O)4 and 0.06-0.33 atm of O2 partial pressure. The thin film has a good ferroelectricity.

    Abstract translation: PbTiO3薄膜通过化学沉积具有Pb粉末(99.9%),金属有机cpd的Ti板来生产。 在具有47mm内径和1m长度的多管的反应管中的Ti(C 2 H 5 O)4和O 2(99.99%)在水平电阻炉的两个带中。 化学气相沉积工艺在600-750℃,Ti(C 2 H 5 O)4的0.02-0.23分数和O 2分压的0.06-0.33atm下进行。 该薄膜具有良好的铁电性。

    마이크로파 가열을 이용한 리튬이차전지용 양극 분말의제조방법
    42.
    发明授权
    마이크로파 가열을 이용한 리튬이차전지용 양극 분말의제조방법 有权
    通过微波加热锂二次电池阴极粉末的合成方法

    公开(公告)号:KR100500699B1

    公开(公告)日:2005-07-12

    申请号:KR1020030005622

    申请日:2003-01-28

    Inventor: 김호기 박규성

    Abstract: 본 발명은 휴대전원으로서 각광받고 있는 리튬이차전지용 양극 분말의 제조방법에 관한 것으로, 양극 분말의 열처리과정은 양극 분말을 탄소와 함께 마이크로파에 노출시켜 탄소의 가열을 유도하여 환원성 분위기를 조성하면서 수행됨을 특징으로 하는 리튬이차전지용 양극 분말의 제조방법을 개시한다.
    본 발명에 의하면 기존의 고상반응법, 졸겔법 등에서 불활성 기체를 흘려주면서 환원분위기를 조절하는 방법과는 달리 간단하게 환원성 분위기를 제어할 수 있다.

    Abstract translation: 目的:提供一种制备用于锂二次电池的正极粉末和使用正极粉末制备的锂二次电池的方法,以便简单地控制还原条件而不流动高纯度的惰性或还原性气体 处理。 方案:该方法包括将微波施加到含有铁的正极粉末与碳一起以诱导碳的加热并进行还原的步骤。 正极粉末的组成由LiFe(1-x)MxPO4表示,其中0 <= x <1,M是过渡金属。 优选地,正极粉末的组成由LiFePO 4表示。 优选地,正电极粉末用导电性改进剂表面涂覆。

    마이크로파 유전체 자기조성물 및 그의 제조방법
    43.
    发明授权
    마이크로파 유전체 자기조성물 및 그의 제조방법 失效
    微波介电瓷组合物及其制造方法

    公开(公告)号:KR100299098B1

    公开(公告)日:2002-03-15

    申请号:KR1019980053745

    申请日:1998-12-08

    Abstract: 본 발명은 마이크로파 유전체 자기조성물 및 그 제조방법에 관한 것이다.
    본 발명의 마이크로파 유전체 자기조성물은 산화칼슘, 산화사마리움, 산화티타늄, 산화리튬을 원료로 조성한 일반식 (1-y)Ca
    0.4 Sm
    0.4 TiO
    3 - yLi
    0.5 Sm
    0.5 TiO
    3 의 조성물에 상기의 원료무게를 100으로 할 때 산화망간을 질산망간 수화물 형태로 산화물 무게비로 환산해서 3 wt % 미만으로 첨가하여 혼합 한 후, 1,000℃ ∼ 1,200℃에서 하소하고, 다시 분쇄하여 성형한 다음 1,200℃ ∼ 1,550℃의 산소분위기에서 소성한다.
    본 발명의 마이크로파 유전체 자기조성물은 산화망간을 질산망간 수화물 형태로 첨가하기 때문에 미량 첨가시에도 정확한 공정제어가 가능할 뿐만 아니라 유전율이 80 이상, 공진주파수(f)와 품질계수(Q)의 곱이 8,000 이상, 공진주파수의 온도의존계수가 ± 3 ppm/℃ 이하의 값을 가지는 우수한 유전특성을 가진다.

    리튬이차전지용 정극재료의 제조방법
    44.
    发明公开
    리튬이차전지용 정극재료의 제조방법 失效
    生产锂二次电池阴极材料的方法

    公开(公告)号:KR1020010077415A

    公开(公告)日:2001-08-17

    申请号:KR1020000005210

    申请日:2000-02-02

    Inventor: 한이섭 김호기

    Abstract: PURPOSE: Provided is a process for producing lithium manganese oxide(LiMn2O4) powder as a cathode material for a lithium secondary cell, which can synthesize the powder having excellent crystalline for a short drying and heating time. CONSTITUTION: The process comprises the steps of: dissolving manganese salts in nitric acid solvent; dissolving lithium salts in the manganese salts dissolved solution to produce a metal salts solution, wherein the ratio of 2Li/Mn is 0.95-2.00; adding a mixture solution of citric acid/ethylene glycol to the metal salts solution, wherein the molar ratio of the citric acid/ethylene glycol is 0-5; drying at 150deg.C or higher and performing spontaneous combustion; calcining the spontaneous combustion products.

    Abstract translation: 目的:提供一种生产锂锰氧化物(LiMn2O4)粉末作为锂二次电池的阴极材料的方法,其可以在短时间和加热时间内合成具有优异结晶性的粉末。 构成:该方法包括以下步骤:将锰盐溶解在硝酸溶剂中; 将锂盐溶解在锰盐溶解溶液中以产生金属盐溶液,其中2Li / Mn的比例为0.95-2.00; 向金属盐溶液中加入柠檬酸/乙二醇的混合溶液,其中柠檬酸/乙二醇的摩尔比为0-5; 干燥150℃以上,进行自燃; 煅烧自燃产物。

    관통형 콘덴서의 전극 부착방법
    45.
    发明授权
    관통형 콘덴서의 전극 부착방법 失效
    空值

    公开(公告)号:KR100270511B1

    公开(公告)日:2000-11-01

    申请号:KR1019980019746

    申请日:1998-05-29

    Abstract: PURPOSE: A method for attaching an electrode of a through type condenser is provided to improve the electric characteristic and to reduce the processing steps and manufacturing cost by attaching an external terminal and a through terminal using a spot welding. CONSTITUTION: An annular silver plated electrode is formed on both sides of a magnetic substrate of a ceramic material(5). Then, a through terminal(2) is connected to an upper external electrode(4) by means of a spot welding. A cream solder(7) is printed on a lower external electrode(6) so as to attach the through terminal(2), the upper external electrode(4), the ceramic material(5), and the lower external electrode(6) to each other. An arc welding method is used as the spot welding. The through type condenser is manufactured in a state that the solvent component of the cream solder(7) is completely dried.

    Abstract translation: 目的:提供一种连接通过型冷凝器的电极的方法,以通过使用点焊附接外部端子和贯通端子来改善电特性并减少加工步骤和制造成本。 构成:在陶瓷材料(5)的磁性基板的两侧形成环状镀银电极。 然后,通过点焊将贯通端子(2)与上部外部电极(4)连接。 将膏状焊料(7)印刷在下部外部电极(6)上,以便安装通孔(2),上部外部电极(4),陶瓷材料(5)和下部外部电极(6) 对彼此。 使用电弧焊法作为点焊。 直通式冷凝器是在奶油焊膏(7)的溶剂成分完全干燥的状态下制造的。

    고체전해질을 이용한 다층박형 2차 전지
    46.
    发明公开
    고체전해질을 이용한 다층박형 2차 전지 无效
    二次电池

    公开(公告)号:KR1020000040454A

    公开(公告)日:2000-07-05

    申请号:KR1019980056107

    申请日:1998-12-18

    Inventor: 김호기 박용준

    Abstract: PURPOSE: A second battery is provided to reduce the size of the battery by using a solid electrolyte. CONSTITUTION: An anode material(2) is evaporated on one side surface of a solid electrolyte(1). A cathode material(3) is evaporated on the other side surface of the solid electrolyte(1). A wire material(4) is engaged with the outside of the solid electrolyte(1). A unit battery(5) is manufactured by engaging the wire material with the outside of the solid electrolyte(1). The unit battery(5) is stacked to manufacture a secondary battery(6). According to the secondary battery, the size of the battery is reduced by using a solid electrolyte(1).

    Abstract translation: 目的:提供第二个电池以通过使用固体电解质来减小电池的尺寸。 构成:在固体电解质(1)的一个侧表面上蒸发阳极材料(2)。 阴极材料(3)在固体电解质(1)的另一侧表面蒸发。 线材(4)与固体电解质(1)的外部接合。 单体电池(5)通过将线材与固体电解质(1)的外部接合来制造。 单体电池(5)被堆叠以制造二次电池(6)。 根据二次电池,通过使用固体电解质(1)来减小电池的尺寸。

    유전체 하부전극용 백금박막 및 증착방법
    47.
    发明公开
    유전체 하부전극용 백금박막 및 증착방법 失效
    铂电介质下电极和沉积方法

    公开(公告)号:KR1019990069791A

    公开(公告)日:1999-09-06

    申请号:KR1019980004253

    申请日:1998-02-13

    Abstract: 본 발명은 유전체 하부전극용 백금(Pt)박막의 화학증착 방법에 관한 것으로, 백금(Pt)의 전구체로 메틸사이클로펜타디에닐 트리메틸 백금:(CH
    3 )
    3 (CH
    3 C
    5 H
    4 )Pt를 사용하여 증착한 결과 기존의 증착방법보다 우수한 특성을 갖는 Pt박막을 제조할 수 있다.
    본 발명의 화학증착법으로 제조된 백금박막은 스텝 커버리지(층 덮힘도)도 우수하고 700℃의 고온에서도 폴리실리콘(polysilicon)과 반응이 거의 없는 우수한 경계 특성을 나타내므로 비휘발성 기억소자, 초고집적 기억소자등의 유전체와 폴리실리콘 플러그(polysilicon plug)의 접속층에 활용이 가능한 백금 박막의 제조방법에 관한 것이다.

    온돌 난방용 패널
    48.
    发明公开
    온돌 난방용 패널 失效
    暖炕加热板

    公开(公告)号:KR1019990004463A

    公开(公告)日:1999-01-15

    申请号:KR1019970028580

    申请日:1997-06-28

    Inventor: 김호기 박융

    Abstract: 보온성과 정온성을 향상시킨 온돌난방용 패널에 관한 것이다.
    종래의 온수배관 온돌에 대체할 수 있는 전열식 온돌 난방용 패널이다.
    저면으로부터 목재패널과 금속패널을 교호로 적층하되 목재패널에는 PCT히터와 PCT 퓨즈를 안착시켜 합체한 구조이다.
    가볍고 보온성이 우수하며 전력소모량이 적어 실용성이 높고 목재가 가지는 적정한 정도의 충격흡수성이 가미되어 기존의 온돌용 패널과 다른 물성을 가진다.

    고주파 유전체용 자기조성물 및 그의 제조방법

    公开(公告)号:KR100164290B1

    公开(公告)日:1998-12-15

    申请号:KR1019960033523

    申请日:1996-08-13

    Inventor: 김호기 박융

    CPC classification number: H01L28/55 C04B35/49

    Abstract: 본 발명은 주성분으로 산화지르코늄(ZrO
    2 ), 산화주석(SnO
    2 ) 및 산화티타늄(TiO
    2 )을 (ZrO
    2 )
    1-x (SnO
    2 )x(TiO
    2 )
    1+Y (X는 0.1몰 X 0.4몰이고, Y는 0몰 Y 0.1몰이다)의 몰비로 혼합하여 1900℃ 이상에서 용융 분쇄하고, 부성분으로 질산망간(Mn(NO
    3 )
    2 4H
    2 O)을 산화망간(MnO)의 무게비(wt%)로 1 중량% 이하 첨가하여 제조된 고주파 유전체용 자기조성물 및 그의 제조방법에 관한 것이다. 본 발명의 제조방법은 비산화물 형태의 질산망간(Mn(NO
    3 )
    2 4H
    2 O)을 부성분으로 이용하므로, 정확한 공정제어를 가능케 하여 균일한 고주파 유전체용 자기조성물을 제공케 하고, 이렇게 제조된 고주파 유전체용 자기조성물은 유전율(k)이 40이상이며, 품질계수(Q) 값이 7000 이상이고, 공진주파수의 온도의존계수(τ
    f )가 10 이하의 매우 낮은 수치를 나타내었다. 따라서, 본 발명의 고주파 유전체용 자기조성물은 고주파에서 뿐만 아니라 마이크로웨이브에서의 집적회로 또는 유전체 공진기용으로 사용될 수 있다.