41.
    发明专利
    未知

    公开(公告)号:DE102004013408A1

    公开(公告)日:2005-10-06

    申请号:DE102004013408

    申请日:2004-03-18

    Applicant: BASF AG

    Abstract: The invention relates to polyether alcohols, to a process for preparing polyether alcohols by reacting alkylene oxides in the presence of a double metal cyanide (DMC) catalyst with at least one saturated OH component which may, if appropriate, have previously been reacted with an alkylene oxide, wherein an antioxidant is added before or during the reaction, and also to the further processing of the polyether alcohols to form polyurethanes.

    42.
    发明专利
    未知

    公开(公告)号:DE10240186A1

    公开(公告)日:2004-03-11

    申请号:DE10240186

    申请日:2002-08-28

    Applicant: BASF AG

    Abstract: The present invention provides a process for producing low-emission flexible polyurethane foams having a reduced odor and reduced fogging by reacting a) polyisocyanates with b) compounds having at least two hydrogen atoms which are reactive toward isocyanate groups, c) blowing agents wherein polyether alcohols which have been prepared by addition of alkylene oxides onto compounds derived from renewable raw materials using DMC catalysts are used as compounds b) having at least two hydrogen atoms which are reactive toward isocyanate groups.

    43.
    发明专利
    未知

    公开(公告)号:DE10226415A1

    公开(公告)日:2003-12-24

    申请号:DE10226415

    申请日:2002-06-13

    Applicant: BASF AG

    Abstract: The invention relates to a method for producing polyether alcohols, comprising the following steps: a) reacting a low-molecular alcohol with alkylene oxide in the presence of a basic catalyst in order to form an alkylene oxide addition product having a molecular weight ranging from 200 to 900 g/mol; b) separating the basic catalyst from the product obtained in step a), and; c) reacting the product obtained in step b) with another alkylene oxide in order to produce the desired final product while using at least one DMC catalyst. The inventive method is characterized in that sodium hydroxide is used as the basic catalyst in step a).

    METODO PARA PRODUCIR MATERIALES DE ESPUMA SUAVE DE POLIURETANO.

    公开(公告)号:MX2007002766A

    公开(公告)日:2008-03-05

    申请号:MX2007002766

    申请日:2005-09-20

    Applicant: BASF AG

    Abstract: La invencion se refiere al metodo para producir materiales de espuma de poliuretano suave, en particular materiales de espuma de poliuretano suave de poliuretano, haciendo reaccionar a) poli-isocianatos con b) compuestos que tienen por lo menos dos atomos de hidrogeno reactivos con grupos isocianato. La invencion se caracteriza porque b) por lo menos un alcohol de polieter, que puede producirse por medio de un catalizador de DMC bi) que tiene un numero de hidroxilos en la region de 15 a 35 mg KOH/g, un contenido de oxido de etileno en la region de 5 a 18 % en peso, en relacion con el peso total del alcohol de polieter, y un bloque extremo hecho de oxido de etileno de entre 25 a 75 % en peso, en relacion con la cantidad de oxido de alquileno en el bloque extremo, se usa como compuestos que tienen por lo menos dos atomos de hidrogeno que son reactivos con los grupos isocianato.

    PROCEDIMIENTO PARA LA OBTENCION DE ESPUMAS BLANDAS DE POLIURETANO QUE GENERAN POCAS EMISIONES.

    公开(公告)号:ES2290545T3

    公开(公告)日:2008-02-16

    申请号:ES03790810

    申请日:2003-07-24

    Applicant: BASF AG

    Abstract: Recipiente flexible (1) con un puerto de acceso (4), en el que una lámina flexible y una segunda pieza limitadora de tipo superficial están unidas entre sí a lo largo de una costura de unión (2), y en donde la costura de unión (2) recubre un puerto de acceso (4), que está dispuesto entre la lámina y la pieza limitadora y representa un acceso del exterior del recipiente al interior del recipiente, en donde el puerto de acceso (4) presenta un segmento (4a) que sobresale de la costura de unión (2) en dirección al interior del recipiente, caracterizado porque la costura de unión (2), en el punto en la que une el puerto de acceso (4) a la lámina, prosigue en la dirección del segmento sobresaliente (4a) del puerto de acceso (4), para unir igualmente una parte (5) de este segmento (4a) del puerto de acceso (4) a la lámina.

    47.
    发明专利
    未知

    公开(公告)号:AT384753T

    公开(公告)日:2008-02-15

    申请号:AT05744275

    申请日:2005-04-21

    Applicant: BASF AG

    Abstract: Process for preparing polyether polyols having an end block of ethylene oxide by addition of alkylene oxides onto H-functional starter substances, in which A) a polyether polyol precursor is prepared by means of double metal cyanide (DMC) catalysis in a semicontinuous mode of operation in which previously prepared polyether polyol together with the DMC catalyst are placed in a reactor and H-functional starter substance and propylene oxide are added continuously, B) the polyether polyol precursor from stage A) is reacted with propylene oxide or an ethylene oxide/propylene oxide mixture in the presence of the DMC catalyst in a continuously operating reactor to give a polyether polyol intermediate, C) the intermediate from stage B) is mixed with an alkali metal hydroxide as catalyst and D) reacted with ethylene oxide in a continuously operating reactor to give the final product, E) the catalyst is separated off from the final product obtained in stage D).

    48.
    发明专利
    未知

    公开(公告)号:DE102005011581A1

    公开(公告)日:2006-09-14

    申请号:DE102005011581

    申请日:2005-03-10

    Applicant: BASF AG

    Abstract: The invention relates to a process for preparing DMC catalysts by reacting cyanometalate compounds, preferably cyanometalate salts, in particular alkali metal or alkaline earth metal salts, with metal salts, wherein the reaction is carried out in the presence of a Brönsted acid.

    49.
    发明专利
    未知

    公开(公告)号:DE102004047406A1

    公开(公告)日:2006-03-30

    申请号:DE102004047406

    申请日:2004-09-28

    Applicant: BASF AG

    Abstract: The invention relates to a process for producing flexible polyurethane foams, in particular molded flexible polyurethane foams, by reacting a) polyisocyanates with b) compounds having at least two hydrogen atoms which are reactive toward isocyanate groups, wherein at least one polyether alcohol bi) which has been prepared by means of a DMC catalyst and has a hydroxyl number in the range from 15 to 35 mg KOH/g, and ethylene oxide content in the range from 5 to 18% by weight, based on the total weight of the polyether alcohol and an end block of ethylene oxide and propylene oxide having an ethylene oxide content of from 25 to 75% by weight, based on the amount of alkylene oxide in the end block, is used as compound b) having at least two hydrogen atoms which are reactive toward isocyanate groups.

    PROCEDIMIENTO PARA LA PREPARACION DE POLIETEROLES.

    公开(公告)号:MXPA05002616A

    公开(公告)日:2005-05-05

    申请号:MXPA05002616

    申请日:2003-09-11

    Applicant: BASF AG

    Inventor: RUPPEL RAIMUND

    Abstract: La presente invencion se refiere a un proceso para preparar un polieterol el cual comprende reaccionar por lo menos un oxido de alquileno con por lo menos un compuesto de inicio en la presencia de un catalizador de la formula I: y a los polieteroles preparados mediante un proceso tal y a su uso para la sintesis de poliuretanos, como aditivo de combustibles o como surfactante.