公开(公告)号:TR9801201T2
公开(公告)日:1998-10-21
申请号:TR9801201
申请日:1996-12-16
Applicant: BASF AG
Inventor: KRECH RUDIGER , ROTERMUND UDO , BOLLMANN HEINZ , HEMPEL RENATE , SCHOLZ WOLFGANG , GENZ MANFRED
IPC: C08J9/36 , C08G18/08 , C08G18/40 , C08G18/76 , C08G101/00
CPC classification number: C08G18/089 , C08G18/7664 , C08G2101/0066 , C08G2101/0083 , C08G2350/00
-
公开(公告)号:TR199801194T2
公开(公告)日:1998-10-21
申请号:TR9801194
申请日:1996-12-16
Applicant: BASF AG
Inventor: KRECH RUDIGER , ROTERMUND UDO , BOLLMANN HEINZ , HEMPEL RENATE , SCHOLZ WOLFGANG , GENZ MANFRED
Abstract: PCT No. PCT/EP96/05640 Sec. 371 Date Oct. 7, 1998 Sec. 102(e) Date Oct. 7, 1998 PCT Filed Dec. 16, 1996 PCT Pub. No. WO97/23535 PCT Pub. Date Jul. 3, 1997A microcellular PU elastomer having improved dynamic mechanical properties and based on an isocyanate component consisting essentially of 4,4'-MDI and further customary constituents has a physicochemical structure which, in the gel permeation chromatograph (GPC) of a solution of the microcellular polyurethane elastomer prepared at 90 DEG C. in N,N-dimethylformamide containing 1 percent of di-n-butylamine measured against polymethyl methacrylate (PMMA) as standard, displays a signal occurring in addition to low molecular weight main signal and comprising one or more peaks at an (apparent) molar mass of greater than 250,000 g/mol which becomes smaller or disappears on addition of lithium chloride to this solution, and a urea content of from 14 to 18% by weight. A process is also provided for preparing such a microcellular PU elastomer having improved dynamic mechanical properties. The microcellular PU elastomers can be used for producing damping elements.
-
公开(公告)号:CZ9801769A3
公开(公告)日:1998-10-14
申请号:CZ176998
申请日:1996-12-16
Applicant: BASF AG
Inventor: KRECH RUDIGER , ROTERMUND UDO , BOLLMANN HEINZ , HEMPEL RENATE , SCHOLZ WOLFGANG , GENZ MANFRED
IPC: C08J9/36 , C08G18/08 , C08G18/40 , C08G18/76 , C08G101/00
CPC classification number: C08G18/089 , C08G18/7664 , C08G2101/0066 , C08G2101/0083 , C08G2350/00
-
54.
公开(公告)号:AU5317998A
公开(公告)日:1998-06-10
申请号:AU5317998
申请日:1997-11-05
Applicant: BASF AG
Inventor: REICHELT MICHAEL , HEINZ MARION , ROTERMUND UDO , HEMPEL RENATE , HENSIEK RAINER , SEIFERT HOLGER
IPC: C07C263/18 , C08G18/24 , C08G18/70
Abstract: The invention relates to polyisocyanates containing tin in the form of compounds of quadrivalent and/or bivalent tin in a quantity ranging from 0.1 to 20 ppm tin with respect to the mass of the polyisocyanate, the polyurethane and/or the polyisocyanurate. The invention further relates to the method for preparing said polyisocyanates and their use.
-
公开(公告)号:AU1372597A
公开(公告)日:1997-07-17
申请号:AU1372597
申请日:1996-12-16
Applicant: BASF AG
Inventor: KRECH RUDIGER , ROTERMUND UDO , BOLLMANN HEINZ , HEMPEL RENATE , SCHOLZ WOLFGANG , GENZ MANFRED
IPC: C08J9/36 , C08G18/08 , C08G18/40 , C08G18/76 , C08G101/00
Abstract: PCT No. PCT/EP96/05639 Sec. 371 Date Nov. 18, 1998 Sec. 102(e) Date Nov. 18, 1998 PCT Filed Dec. 16, 1996 PCT Pub. No. WO97/23534 PCT Pub. Date Jul. 3, 1997A microcellular PU elastomer having improved dynamic-mechanical properties and based on an isocyanate component consisting essentially of 4,4'-MDI and also further customary constituents has, after heating at from 100 to 120 DEG C. for from 8 to 24 hours, a melting range of from 130 DEG C. as the minimum lower limit to 230 DEG C. as a minimum upper limit, measured by differential scanning calorimetry (DSC) at a heating rate of 20 DEG C./min, and a urea content of from 14 to 18% by weight. A process is also provided for preparing such a microcellular PU elastomer having improved dynamic mechanical properties. The microcellular PU elastomers can be used for producing damping elements.
-
公开(公告)号:DE19548771A1
公开(公告)日:1997-06-26
申请号:DE19548771
申请日:1995-12-23
Applicant: BASF AG
Inventor: KRECH RUEDIGER , ROTERMUND UDO DR , BOLLMANN HEINZ , HEMPEL RENATE , SCHOLZ WOLFGANG , GENZ MANFRED DR
IPC: C08J9/36 , C08G18/08 , C08G18/40 , C08G18/76 , C08G101/00 , C08G18/78 , C08G18/38 , C08G18/10 , C08G18/65 , C08L75/00 , B29C67/20 , B29C45/03
Abstract: The invention relates to a microcellular PU elastomer with improved dynamic-mechanical characteristics, based on an isocyanate component consisting essentially of 4,4'-MDI and on other standard components. The proposed elastomer following tempering at temperatures of 100-120 DEG C for 8-24 hours has a melting range of between 130 DEG C as minimum lower limit and 230 DEG C as minimum upper limit, as measured by differential scanning calorimetry (DSC) at a heating rate of 20 DEG C/min and a urea content of 14-18 wt.%. Also disclosed are a process for producing such a microcellular PU elastomer with improved dynamic-mechanical characteristics and the use of said elastomers in the production of damping elements.
-
公开(公告)号:DE19816526B4
公开(公告)日:2006-12-21
申请号:DE19816526
申请日:1998-04-15
Applicant: BASF AG
Inventor: DINSCH STEFAN , ROTERMUND UDO , FALKE PETER , HEMPEL RENATE , SCHROETER HORST
IPC: C07B63/04 , C07C217/08 , C08G18/50 , C08G18/66 , C08K5/16 , C09K15/20 , C10M133/04 , C10M133/08 , C10M133/14 , C10M149/12
-
公开(公告)号:ES2238742T3
公开(公告)日:2005-09-01
申请号:ES98117895
申请日:1998-09-22
Applicant: BASF AG
Inventor: ROTERMUND UDO DR , BIEDERMANN ANJA , HEMPEL RENATE , WIEGMANN WERNER , HEINZ MARION
IPC: C08J3/02 , C08G18/40 , C08G18/42 , C08G18/48 , C08G18/50 , C08G18/66 , C08G101/00 , C08J9/12 , C08J9/14 , C08L75/04
Abstract: EL OBJETO DE LA INVENCION SON EMULSIONES SIN HALOGENOS QUE CONTIENEN AGENTES POROGENOS QUE SON ESTABLES EN ALMACENAMIENTO PARA LA FABRICACION DE ESPUMAS DURAS A BASE DE ISOCIANATO QUE CONTIENEN A) COMPUESTOS QUE CONTIENEN ATOMOS DE HIDROGENO QUE SON REACTIVOS CON LOS GRUPOS ISOCIANATO, B) AGUA, C) AGENTES POROGENOS SIN HALOGENOS QUE ACTUAN FISICAMENTE, ASI COMO OPCIONALMENTE D) ADYUVANTES Y/O ADITIVOS USUALES EN LA QUIMICA DEL POLIURETANO, CARACTERIZADO PORQUE COMO COMPONENTE A) SE UTILIZAN POLIETERALCOHOLES CON UNA FUNCIONALIDAD MAYOR DE 1,5, UN INDICE DE HIDROXILO DE 10 A 100 MG DE KOH/G EN UNA CANTIDAD DE 0,2 % HASTA 80 % EN MASA, CON RELACION A LA MASA DEL COMPONENTE A), Y COMO ESPUMANTES QUE ACTUAN DE MANERA FISICA Y SIN HALOGENOS SE PUEDEN UTILIZAR C) HIDROCARBUROS CON 3 A 10 ATOMOS DE CARBONO.
-
公开(公告)号:DE59812630D1
公开(公告)日:2005-04-14
申请号:DE59812630
申请日:1998-09-22
Applicant: BASF AG
Inventor: ROTERMUND DR , BIEDERMANN ANJA , HEMPEL RENATE , WIEGMANN WERNER , HEINZ MARION
IPC: C08J3/02 , C08G18/40 , C08G18/42 , C08G18/48 , C08G18/50 , C08G18/66 , C08G101/00 , C08J9/12 , C08J9/14 , C08L75/04
Abstract: Emulsions containing polyether alcohols are used in the production of hard foams based on isocyanates to improve the temperature stability of the foams. Storage-stable halogen-free emulsions used in the production of hard foams based on isocyanates contain: (a) compounds containing hydrogen atoms reactive towards isocyanate groups; (b) water; (c) halogen-free propellants; and optionally (d) usual auxiliary aids and/or additives. (a) is used in an amount of 0.2-80 wt.% and has a functionality of more than 1.5, and an OH number of 10-100 mg KOH/g. (c) consists of 3-10 C hydrocarbons. Independent claims are also included for: (1) the production of the hard foams described; (2) the foams, and (3) the use of the polyether alcohols described.
-
公开(公告)号:DE10309798A1
公开(公告)日:2004-09-16
申请号:DE10309798
申请日:2003-03-05
Applicant: BASF AG
Inventor: ROTERMUND UDO , HEMPEL RENATE , RUDLOFF JAN , HENNIG INGOLF , MOEHWALD HELMUT , RAHNER DIETMAR , TROMMER KRISTIN
-
-
-
-
-
-
-
-
-