태양전지 폐 셀에서의 실리콘 회수 방법
    62.
    发明公开
    태양전지 폐 셀에서의 실리콘 회수 방법 失效
    从废物太阳能电池回收硅的方法

    公开(公告)号:KR1020110069962A

    公开(公告)日:2011-06-24

    申请号:KR1020090126570

    申请日:2009-12-18

    Inventor: 류호진 강석민

    CPC classification number: Y02E10/50 Y02W30/827 H01L31/04 H01L21/02

    Abstract: PURPOSE: A method for recycling silicon from a used solar cell is provided to immerse a used solar cell in a mixed acid solvent for proper time to eliminate a non-reflection coat film and an electrode material, thereby recycling the used solar cell as a silicon wafer. CONSTITUTION: The composition of a mixed acid solvent and the immersion time of a used solar battery cell(11) are determined to obtain an optimum silicon collecting rate from the used solar battery cell. The mixed acid solvent melts a non-reflection coat film and an electrode material in the used solar battery cell according to the composition of the mixed acid solvent. The composition of the used solar battery cell is cut by a fixed weight. The cut solar battery cell is immersed in the mixed acid solvent during the determined immersion time. When the non-reflection coat film and the electrode material of the used solar battery cell are melted in the mixed acid solvent, pure silicon is obtained.

    Abstract translation: 目的:提供一种从二手太阳能电池回收硅的方法,将二氧化硅太阳能电池浸入混合酸性溶剂中适当的时间以消除非反射涂膜和电极材料,从而将二氧化硅太阳能电池作为硅 晶圆。 构成:确定混合酸溶剂的组成和使用的太阳能电池单元(11)的浸渍时间,以从所使用的太阳能电池单元获得最佳的硅收集率。 混合酸溶剂根据混合酸溶剂的组成,在使用的太阳能电池单元中熔融非反射涂膜和电极材料。 所使用的太阳能电池单元的组成被固定重量切割。 在确定的浸渍时间内将切割的太阳能电池单元浸入混合的酸溶剂中。 当使用太阳能电池单元的非反射涂膜和电极材料在混合酸溶剂中熔化时,获得纯硅。

    광촉매로 유용한 축광체-이산화티타늄 복합 나노입자 및 이의 제조방법
    63.
    发明公开
    광촉매로 유용한 축광체-이산화티타늄 복합 나노입자 및 이의 제조방법 无效
    磷光体 - 二氧化钛纳米复合材料的制备及其制备方法

    公开(公告)号:KR1020110064130A

    公开(公告)日:2011-06-15

    申请号:KR1020090120592

    申请日:2009-12-07

    Abstract: PURPOSE: A phosphorescent material-titanium dioxide nanocomposite particle and a producing method thereof are provided to secure the optical activity of the nanocomposite particle on the non-irradiation condition of light. CONSTITUTION: A phosphorescent material-titanium dioxide nanocomposite particle contains CaAl2O4:Eu2+, a Nd3+ phosphorescent, and a titanium dioxide. The nanocomposite particle is plasticized at 400~600deg C, and exists in an anatase crystal phase. The nanocomposite particle has the photo-degradable activity from the ultraviolet ray to visible light wavelength area.

    Abstract translation: 目的:提供一种磷光材料 - 二氧化钛纳米复合材料颗粒及其制备方法,以确保纳米复合材料颗粒在非光照条件下的光学活性。 构成:磷光材料 - 二氧化钛纳米复合材料颗粒含有CaAl2O4:Eu2 +,Nd3 +磷光体和二氧化钛。 纳米复合材料颗粒在400〜600℃下塑化,呈锐钛矿晶相。 纳米复合颗粒具有从紫外线到可见光波长区域的光可降解活性。

    메카노케미컬 처리된 촉매를 이용한 탄소나노섬유의제조방법
    64.
    发明授权
    메카노케미컬 처리된 촉매를 이용한 탄소나노섬유의제조방법 失效
    具有受控尺寸和形态的碳纳米纤维使用用机械化学过程处理的催化剂合成

    公开(公告)号:KR100627352B1

    公开(公告)日:2006-09-25

    申请号:KR1020040066853

    申请日:2004-08-24

    Abstract: 본 발명은 메카노케미컬 처리된 촉매를 이용한 탄소나노섬유의 제조방법에 관한 것으로서, 더욱 상세하게는 촉매인 니켈과 담체인 마그네슘을 혼합시켜 특정의 반응 조건에서 메카노케미컬 처리한 담지촉매에, 탄소소재로 아세틸렌을 사용하여 합성하는 화학기상증착법으로 탄소나노섬유를 제조하면, 입경의 크기가 10 ∼ 100 ㎚으로 미세하고, 불순물을 적게하여 고품위를 가지고, 열 및 화학적으로 매우 안정하며 환경친화적이여서 연료전지용 전극지지체, 전계방출 디스플레이의 에미터용 소재로 적용 가능성이 높은 메카노케미컬 처리된 촉매를 이용한 탄소나노섬유의 제조방법에 관한 것이다.
    니켈, 마그네슘, 메카노케미컬, 탄소나노섬유

    변형된 유도결합형 플라즈마 화학기상증착법에 의한탄소나노튜브의 합성방법
    65.
    发明授权
    변형된 유도결합형 플라즈마 화학기상증착법에 의한탄소나노튜브의 합성방법 失效
    通过改性电感耦合等离子体化学气相沉积合成碳纳米管的方法

    公开(公告)号:KR100480663B1

    公开(公告)日:2005-04-06

    申请号:KR1020010082658

    申请日:2001-12-21

    Inventor: 류호진 김광식

    CPC classification number: C03C17/36 B82Y30/00 C01B32/15

    Abstract: 본 발명은 변형된 유도결합형 플라즈마 화학기상증착법에 의한 탄소나노튜브의 합성방법에 관한 것으로, 본 발명에 따라 유리기판상에 전도성 금속층 및 전이금속 촉매층을 형성시키고 식각 가스를 이용한 유도결합형 플라즈마로 상기 전이금속 촉매층을 식각한 후, 기판상에 탄소원료가스와 촉매가스를 주입하고, 주입된 원료가스를 전기저항 열선으로 분해시키면서, 기판에 직류 바이어스를 인가하고 촉매가스의 RF(radio frequency) 플라즈마를 생성시켜 탄소나노튜브를 수직 배향으로 성장시키는 방법에 의하면 성장된 탄소나노튜브의 수직 배향성이 개선되어 전기적 특성이 향상되기 때문에, 전자소자, 나노소자 및 FED(Field Emission Display) 에미터(emitter)용 소재로 사용할 수 있다.

    플라즈마 화학 기상 증착장치 및 이를 이용한 박막 형성방법
    66.
    发明授权
    플라즈마 화학 기상 증착장치 및 이를 이용한 박막 형성방법 失效
    等离子体化学气相沉积装置及其使用薄膜的方法

    公开(公告)号:KR100478404B1

    公开(公告)日:2005-03-23

    申请号:KR1020020016273

    申请日:2002-03-26

    Inventor: 류호진 김광식

    Abstract: 플라즈마 화학 기상 증착장치 및 이를 이용한 박막 형성 방법이 개시되어 있다. 상기 장치에는 기판 상에 박막을 형성하기 위한 공간을 제공하기 위한 챔버가 구비된다. 상기 챔버로 제공되는 분위기가스 및 소스가스를 플라즈마 상태로 형성하기 위한 플라즈마 발생부가 구비된다. 상기 플라즈마 발생부 하방에 배치되고, 기판 상에 소스가스를 제공하기 위한 소스가스 제공부가 구비된다. 상기 소스가스를 열 분해하기 위한 저항 가열부가 구비된다. 그리고, 상기 기판을 가열함과 동시에 상기 열 분해된 소스가스를 플라즈마 상태로 조성하도록 네가티브 바이어스 전력이 인가되는 블록 바디가 구비된다. 또한 상기와 같은 구성요소를 포함하는 장치를 이용하여 박막을 형성하는 단계를 갖음으로서 전개방출 능력이 우수하고, 수직 배향성이 우수한 박막을 형성할 수 있다.

    헥사플루오로프로필렌옥사이드의 제조방법
    67.
    发明公开
    헥사플루오로프로필렌옥사이드의 제조방법 失效
    制备十六烷基氧化亚铁的方法

    公开(公告)号:KR1020040063606A

    公开(公告)日:2004-07-14

    申请号:KR1020030001083

    申请日:2003-01-08

    Abstract: PURPOSE: A process for preparing hexafluoropropylene oxide is provided, thereby significantly improving conversion rate of hexafluoropropylene oxide by increasing the reaction area in the interface between the organic phase and water-soluble phase, and reducing the temperature increase at an early stage of the reaction to maintain the constant reaction temperature. CONSTITUTION: The process for preparing hexafluoropropylene oxide comprises the steps of: liquid-liquid interface reacting the organic phase containing hexafluoropropylene(HFP) with the water-soluble phase containing an oxidizing agent in the presence of phase transition catalyst and 0.001 to 0.01 mole% of fluorine surfactant of formula (I), CnF2n=1C2H4O(C2H4O)mH, wherein m is mole number of ethylene oxide, 6 and 12; and n is an integer of 4 to 12; and the mole ratio of organic phase and water-soluble phase is 1:2 to 1:7.

    Abstract translation: 目的:提供一种制备六氟环氧丙烷的方法,从而通过增加有机相和水溶性相界面的反应面积,显着提高六氟环氧丙烷的转化率,并将反应初期的温度升高降低至 保持反应温度恒定。 构成:制备六氟环氧丙烷的方法包括以下步骤:在相变催化剂存在下使含有六氟丙烯(HFP)的有机相与含有氧化剂的水溶性相反应的液 - 液界面和0.001至0.01摩尔% 式(I)的氟表面活性剂,CnF2n = 1C2H4O(C2H4O)mH,其中m为环氧乙烷的摩尔数,6和12; n为4〜12的整数。 有机相和水溶性相的摩尔比为1:2至1:7。

    폐삼파장형광램프에서 란탄과 유로피움을 분리하는 방법
    68.
    发明授权
    폐삼파장형광램프에서 란탄과 유로피움을 분리하는 방법 失效
    如何从废弃的3波长荧光灯中分离镧和铕

    公开(公告)号:KR100412397B1

    公开(公告)日:2003-12-24

    申请号:KR1020010068594

    申请日:2001-11-05

    Abstract: 본 발명은 폐삼파장형광램프의 형광체 성분 중에서 La과 Eu을 효율적으로 분리하는 방법에 관한 것이다.
    본 발명에 따르면, Mg, La, Eu, Y, Tb, Ce 등의 금속이 포함된 형광체가 도포된 폐삼파장형광램프의 파쇄물을 아세트산에 침지시켜 Mg를 선택적으로 용해시켜 분리한 다음, 잔여 고형분을 말레익산에 침지시켜 La, Eu을 용해시켜 분리하는 과정을 포함하여 이루어진 유가금속분리방법에 있어서, 상기 La, Eu이 용해된 말레익산에 추출제로 D2EHPA 또는 TBP를 혼합하고, 이와 함께 희석제로 Kerosene 또는 Hexane을 혼합하여 La과 Eu를 분리하는 것을 특징으로 하는 폐삼파장형광램프에서 La과 Eu을 분리하는 방법이 제공된다.

    폐삼파장형광램프의 유가금속분리방법
    69.
    发明授权
    폐삼파장형광램프의 유가금속분리방법 失效
    폐삼파장형광램프의유가금속분리방법

    公开(公告)号:KR100392518B1

    公开(公告)日:2003-07-28

    申请号:KR1020000063130

    申请日:2000-10-26

    Abstract: PURPOSE: A method is provided, for separating precious metals such as Mg, La, Eu, Y, Tb and Ce from a waste three-wave fluorescent lamp more effectively. CONSTITUTION: The method comprises the steps of crashing waste three-wave fluorescent lamps where fluorescent material containing metals such as Mg, La, Eu, Y, Tb and Ce is coated; dipping the crashed one into various acid solutions which have the selectivity to specific metals, to dissolve the specific metals and to obtain the acid solutions containing specific metal; precipitating the specific metal in the form of a metal salt; separating the metal salt from the solution; and calcining the separated metal salt to form metal oxide.

    Abstract translation: 目的:提供一种更有效地从废三波荧光灯中分离贵金属如Mg,La,Eu,Y,Tb和Ce的方法。 本发明的方法包括以下步骤:将包含Mg,La,Eu,Y,Tb和Ce等金属的荧光材料涂覆在废弃的三波荧光灯上; 将撞击的试样浸入具有对特定金属的选择性的各种酸溶液中,溶解特定金属并获得含特定金属的酸溶液; 沉淀金属盐形式的特定金属; 从溶液中分离金属盐; 并煅烧分离的金属盐以形成金属氧化物。

    툴리움을 포함하는 백색 발광다이오드용 알루미늄산이트륨황색 형광체 및 그 제조방법
    70.
    发明授权
    툴리움을 포함하는 백색 발광다이오드용 알루미늄산이트륨황색 형광체 및 그 제조방법 有权
    툴리움을포함하는백색발광다이오이용알루미늄산이트륨황색황색체및그제조방툴

    公开(公告)号:KR100367854B1

    公开(公告)日:2003-01-10

    申请号:KR1020000084132

    申请日:2000-12-28

    CPC classification number: Y02B20/181

    Abstract: PURPOSE: Provided is an yttrium aluminate yellow phosphor, containing thulium, for a white light emitting diode, which is excellent in light emitting brightness under the excitation of blue light source generated from a blue light emitting diode. CONSTITUTION: The yttrium aluminate yellow phosphor represented by the formula: (Y1-a-bCeaTmb)3Al5O12 is produced by a process comprising the steps of: mixing yttrium aluminate with cerium oxide and thulium oxide; drying the mixture and pre-sintering at 1,200deg.C under the atmosphere; cooling the pre-sintered mixture and heat-treating at 1,650deg.C or higher; post-treating such as grinding. In the formula, 0.005

    Abstract translation: 本发明提供一种白色发光二极管用含有th的铝酸钇黄色荧光体,其在由蓝色发光二极管产生的蓝色光源的激发下发光亮度优异。 构成:由式(Y 1-a-b Ce a T b)3 Al 5 O 12表示的铝酸钇黄色磷光体通过包括以下步骤的方法生产:将铝酸钇与氧化铈和氧化mixing混合; 干燥混合物并在大气中于1200℃预烧; 冷却预烧结的混合物并在1650℃或更高温度下进行热处理; 后处理如研磨。 在该式中,0.005≤α≤0.03和0≤b≤0.025。